LIM™ 6040液体硅橡胶是一种双组分产品,用于高性能弹性体零件的液体注射成型。它是清晰的,但容易色素与现代性能材料色母粒的颜色。主要特点和优点:高清晰度、高可见度、优异的撕裂强度、方便与自动设备配合使用的1:1配合比、快速固化时间:10到40秒,取决于零件尺寸、配置和成型温度、各种成型温度:1500摄氏度(3020华氏度)到2050摄氏度(4000华氏度)从金属模具良好释放幕式应用-结合出色的清晰度,撕裂强度和非常高的拉伸强度,使本产品适合各种应用。婴儿奶嘴接头插入密封件柔性安装阀运动护目镜口罩保健设备摄像头零件涂层金属辊 LIM 6040 liquid silicone rubber is a 2-component product formulated for use in liquid injection molding to high performance elastomeric parts. It is clear, but easily pigmentable with Momentive Performance Materials masterbatch colors. Key Features and Benefits High clarity for excellent visibility Excellent tear strength Convenient 1:1 mix ratio for use with automatic equipment Rapid cure time: 10 to 40 seconds depending upon part size, configuration, and molding temperature Wide range of molding temperatures: 1500C (3020F) to 2050C (4000F) Excellent release from metal molds Potential Applications The combination of excellent clarity, tear strength and very high tensile strength makes this product suitable for a wide variety of applications. Baby bottle nipples Connector inserts Seals Flexible mounts Valves Sports goggles Masks Health care equipment Camera parts Coating metal rolls |
技术参数 Technical Data | |||
---|---|---|---|
弹性体 elastic body |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
巴肖氏弹性 Basho's elasticity |
|||
-- -- 1 |
54 | % | |
-- -- 2 |
58 | % | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame retardant level |
HB | UL 94 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热固组件 Thermosetting components |
|||
部件 A Component A |
按重量计算的混合比: 1.0 | ||
部件 B Component B |
按重量计算的混合比: 1.0 | ||
Uncured Properties Uncured Properties |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
颜色 colour |
|||
-- -- 3 |
|||
-- -- 4 |
|||
密度 Density |
|||
-- -- 5 |
g/cm³ | ||
-- -- 6 |
g/cm³ | ||
Cured Properties Cured Properties |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
|||
邵氏 A Shaw's A 7 |
|||
邵氏 A Shaw's A 8 |
|||
拉伸模量 Tensile modulus |
|||
100% 正割 100% secant 9 |
MPa | ||
100% 正割 100% secant 10 |
MPa | ||
拉伸强度 tensile strength |
|||
-- -- 11 |
MPa | ||
-- -- 12 |
MPa | ||
拉伸应变 Tensile strain |
|||
断裂 fracture 13 |
% | ||
断裂 fracture 14 |
% | ||
压缩形变 Compression deformation |
|||
177℃,22 hr 177℃,22 hr 15 |
% | ||
177℃,22 hr 177℃,22 hr 16 |
% | ||
撕裂强度 tear strength |
|||
Die B Die B 17 |
kN/m | ||
Die B Die B 18 |
kN/m | ||
耐电强度 Electrical strength 19 |
kV/mm | ||
相对电容率 Relative permittivity 20 |
|||
1 kHz 1 kHz 20 |
|||
体积电阻率 Volume resistivity |
|||
-- -- |
ohms·cm | ||
耗散因数 Dissipation factor 22 |
|||
1 kHz 1 kHz 22 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 Postbaked 1 hr @ 204°C (400°F) |
3 As Molded 30 sec @ 177°C (350°F) |
4 Part B |
5 Part A |
【新闻资讯】查看全部
发改委再强调遏制“两高”项目盲目发展 9省份上半年能耗强度不降反升
2021-09-07 搜料网资讯: 节能和坚决遏制两高项目盲目发展,正成为中央和地方环境资源工作的重中之重。 8月17日,国家发改委新闻发言人孟玮在8月份例行新闻发布会上介绍,近日发改委印发《 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |