牌号简介 About |
---|
55邵尔D高性能聚酯弹性体 55 Shore D High Performance Polyester Elastomer |
技术参数 Technical Data | |||
---|---|---|---|
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
ISO 868 | ||
邵氏 D Shaw's D |
55 | ISO 868 | |
邵氏 D,15 秒 Shore D, 15 seconds |
51 | ISO 868 | |
拉伸模量 Tensile modulus |
180 | MPa | ISO 527-2 |
拉伸强度 tensile strength |
ISO 527-2 | ||
断裂 fracture |
40.0 | MPa | ISO 527-2 |
屈服 yield |
15.0 | MPa | ISO 527-2 |
5% 应变 5% strain |
MPa | ISO 527-2 | |
10% 应变 10% strain |
MPa | ISO 527-2 | |
50% 应变 50% strain |
MPa | ISO 527-2 | |
100% 应变 100% strain |
MPa | ISO 527-2 | |
拉伸应变 Tensile strain |
|||
断裂 fracture |
% | ISO 527-2 | |
屈服 yield |
% | ISO 527-2 | |
标称拉伸断裂应变 Nominal tensile fracture strain |
% | ISO 527-2 | |
Tensile Creep Modulus(1 hr) Tensile Creep Modulus(1 hr) |
MPa | ISO 899-1 | |
拉伸蠕变模量 Tensile creep modulus |
|||
1000 hr 1000 hr |
MPa | ISO 899-1 | |
弯曲模量 Bending modulus |
MPa | ISO 178 | |
抗磨损性 abrasion resistance |
mm³ | ISO 4649 | |
薄膜 film |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
水气透过率 Water vapor transmittance |
|||
23℃,85% RH 23℃,85% RH |
g/m²/24 hr | DIS 15106-1/-2 | |
氧气传输速率 Oxygen transfer rate 2 |
|||
23℃,25.0 µm 23℃,25.0 µm 2 |
cm³/m²/bar/24 hr | DIS 15105-1/-2 | |
弹性体 elastic body |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
撕裂强度 tear strength |
ISO 34-1 | ||
TD TD |
kN/m | ISO 34-1 | |
MD MD |
kN/m | ISO 34-1 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength |
ISO 179/1eA | ||
-40℃,局部断裂 -40 ℃, localized fracture |
kJ/m² | ISO 179/1eA | |
-30℃,局部断裂 -30 ℃, localized fracture |
kJ/m² | ISO 179/1eA | |
23℃ 23℃ |
ISO 179/1eA | ||
简支梁无缺口冲击强度 Charpy Unnotch Impact strength |
ISO 179/1eU | ||
-30℃ -30℃ |
ISO 179/1eU | ||
23℃ 23℃ |
ISO 179/1eU | ||
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
ISO 180/1A | ||
-40℃ -40℃ |
ISO 180/1A | ||
23℃ 23℃ |
ISO 180/1A | ||
拉伸冲击强度 Tensile impact strength |
|||
23℃ 23℃ |
kJ/m² | ISO 8256/1 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ISO 75-2/A | |
0.45 MPa,未退火 0.45 MPa, unannealed |
℃ | ISO 75-2/B | |
脆化温度 Embrittlement temperature |
℃ | ISO 974 | |
玻璃化转变温度 Glass transition temperature 3 |
℃ | ISO 11357-2 | |
维卡软化温度 Vicat Softening Temp |
|||
A50 A50 |
℃ | ISO 306/A50 | |
B50 B50 |
℃ | ISO 306 | |
熔融温度 Melting temperature 5 |
℃ | ISO 11357-3 | |
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
TD TD |
ISO 11359-2 | ||
-40 到 23℃ -40 to 23 ℃ |
cm/cm/℃ | ISO 11359-2 | |
MD MD |
ISO 11359-2 | ||
-- -- |
cm/cm/℃ | ISO 11359-2 | |
-40 到 23℃ -40 to 23 ℃ |
cm/cm/℃ | ISO 11359-2 | |
Effective Thermal Diffusivity Effective Thermal Diffusivity |
m²/s | ||
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表面电阻率 Surface resistivity |
ohms | IEC 60093 | |
体积电阻率 Volume resistivity |
ohms·cm | IEC 60093 | |
介电强度 Dielectric strength |
kV/mm | IEC 60243-1 | |
相对电容率 Relative permittivity |
IEC 60250 | ||
100 Hz 100 Hz |
IEC 60250 | ||
1 MHz 1 MHz |
IEC 60250 | ||
耗散因数 Dissipation factor |
IEC 60250 | ||
100 Hz 100 Hz |
IEC 60250 | ||
1 MHz 1 MHz |
IEC 60250 | ||
相比漏电起痕指数 Compared to the leakage tracing index |
V | IEC 60112 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame retardant level |
UL 94 | ||
1.50 mm 1.50 mm |
UL 94 | ||
3.00 mm 3.00 mm |
UL 94 | ||
可燃性等级 Flammability level |
IEC 60695-11-10, -20 | ||
1.5 mm 1.5 mm |
IEC 60695-11-10, -20 | ||
3.0 mm 3.0 mm |
IEC 60695-11-10, -20 | ||
极限氧指数 Extreme oxygen index |
% | ISO 4589-2 | |
FMVSS 阻燃等级 FMVSS flame retardant rating |
FMVSS 302 | ||
Fogging(Gvalue,condensate) Fogging(Gvalue,condensate) |
g | ISO 6452 | |
补充信息 Supplementary information |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
有机化合物的排放 Emissions of organic compounds |
µgC/g | VDA 277 | |
Odor Odor |
VDA 270 | ||
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
g/cm³ | ISO 1183 | |
熔体质量流动速率 Melt Flow Rate |
|||
220℃,2.16kg 220℃,2.16kg |
g/10min | ISO 1133 | |
熔体体积流动速率 Melt Volume Rate |
|||
220℃,2.16 kg 220℃,2.16 kg |
cm³/10min | ISO 1133 | |
收缩率 Shrinkage rate |
ISO 294-4 | ||
TD TD |
% | ISO 294-4 | |
MD MD |
% | ISO 294-4 | |
吸水率 Water absorption rate |
|||
饱和,23℃,2.00 mm Saturation, 23 ℃, 2.00 mm |
% | ISO 62 | |
平衡,23℃,50% RH,2.00 mm Equilibrium, 23 ℃, 50% RH, 2.00 mm |
% | ISO 62 | |
23℃,24hr 23℃,24hr |
% | ISO 62 | |
熔体密度 Melt density |
g/cm³ | ||
Specific Heat Capacity of Melt Specific Heat Capacity of Melt |
J/kg/℃ | ||
Thermal Conductivity of Melt Thermal Conductivity of Melt |
W/m/K |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 10°C/min |
3 FMVSS 302 |
【新闻资讯】查看全部
注塑机螺杆异响打滑,怎样办?
2018-01-29 注塑螺杆在加料口产生压料困难时,或沿着机筒长度不能形成足够的粘着力以输送物料,那么螺杆就发生了打滑现象。在螺杆预塑阶段,螺杆在机筒内旋转沿着螺杆方向输送物料并后退积累物料准备下一次注塑时,螺杆也会发生打滑。 如果螺杆在预塑阶段开始打滑,那么在螺杆继续旋转时,螺杆的轴向运动会停止。通常螺杆打滑会导致物料在注塑之前发生降解,还会出现短射、加工循环周期延长等制品质量问题。 螺杆出现打滑的原因包括背压太高、机筒后半段过热或过冷、机筒或螺杆磨损、螺杆加料段螺槽太浅、料 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |