Technyl One J 60x1 V30灰色7035是一种基于非卤化阻燃系统的高温聚酰胺,用30%的玻璃纤维增强,具有一流的防火性能,热稳定,用于注塑成型。一张完整的黄色卡片具有0.4 mm的UL94 V0额定值、不匹配的热老化性能(150°C电气RTI-相对热指数)和出色的电气性能,包括较高的比较跟踪指数(600伏及以上的CTI 0)。与传统的高性能塑料相比,该产品具有优越的电气性能。低腐蚀性确保了加工工具的使用寿命。该产品基于高流动性矩阵,在生产率和设计自由度方面具有很强的优势。 TECHNYL® ONE J 60X1 V30 Grey 7035 is a high temperature polyamide based on a non-halogenated flame retardant system, reinforced with 30% of glass fiber with best-in-class fire protection behavior, heat stabilized, for injection molding. A full yellow card is available with a UL94 V0 rating at 0.4 mm, unmatched thermal ageing properties (150°C electrical RTI - Relative Thermal Index), and outstanding electrical properties, including a high comparative tracking index (CTI 0 for 600 volts and higher). This product has superior electrical performance compared to traditional high-performance plastics. Its low corrosion ensures processing tools longevity. This product, based on a high fluidity matrix, offers strong benefits in term of productivity and design freedom. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.44 | g/cm³ | |
吸水率 Water absorption rate |
|||
23℃,24hr 23℃,24hr |
0.55 | % | |
平衡,23℃,50% RH Equilibrium, 23 ℃, 50% RH |
1.3 | % | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
|||
23℃ 23℃ |
11000 | MPa | |
拉伸强度 tensile strength |
|||
断裂,23℃ Fracture, 23 ℃ |
130 | MPa | |
拉伸应变 Tensile strain |
|||
断裂,23℃ Fracture, 23 ℃ |
% | ||
弯曲模量 Bending modulus |
|||
23℃ 23℃ |
MPa | ||
弯曲强度 bending strength |
|||
23℃ 23℃ |
MPa | ||
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength |
|||
-30℃ -30℃ |
kJ/m² | ||
23℃ 23℃ |
kJ/m² | ||
简支梁无缺口冲击强度 Charpy Unnotch Impact strength |
|||
-30℃ -30℃ |
kJ/m² | ||
23℃ 23℃ |
kJ/m² | ||
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
|||
23℃ 23℃ |
kJ/m² | ||
悬臂梁无缺口冲击强度 Notched impact strength of cantilever beam |
|||
23℃ 23℃ |
kJ/m² | ||
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
0.45 MPa,未退火 0.45 MPa, unannealed |
℃ | ||
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ||
熔融温度 Melting temperature |
℃ | ||
相对温度指数 Relative temperature index |
|||
电气性能,0.40 mm Electrical performance, 0.40 mm |
℃ | ||
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表面电阻率 Surface resistivity |
ohms | ||
体积电阻率 Volume resistivity |
ohms·cm | ||
介电强度 Dielectric strength |
|||
0.8 mm 0.8 mm |
kV/mm | ||
相比漏电起痕指数 Compared to the leakage tracing index |
|||
解决方案 A Solution A |
V | ||
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame retardant level |
|||
0.40 mm 0.40 mm |
|||
灼热丝可燃性指数 Glowing wire flammability index |
|||
0.80 mm 0.80 mm |
℃ | ||
1.6 mm 1.6 mm |
℃ | ||
3.2 mm 3.2 mm |
℃ | ||
灼热丝起燃温度 Igniting temperature of the hot wire |
|||
0.8 mm 0.8 mm |
℃ | ||
1.6 mm 1.6 mm |
℃ | ||
极限氧指数 Extreme oxygen index |
% | ||
补充信息 Supplementary information |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
欧洲铁路认证 European Railway Certification |
|||
R22 R22 |
|||
R23 R23 |
备注 | |||
---|---|---|---|
暂无数据 |
【新闻资讯】查看全部
飞鹿股份新型高端水性涂料项目进入批量试生产阶段
2022-05-12 近日,飞鹿新型高端水性涂料项目,已进入批量试生产阶段,该项目全面达产后,预计可实现年产值6亿元以上,将进一步助力望城新材料产业发展。 我们这个基地建设有三个生产车间 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |