技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.40 | g/cm³ | ASTM D792 |
特定体积 Specific volume |
0.710 | cm³/g | ASTM D792 |
密度 Density |
1.40 | g/cm³ | ISO 1183 |
熔体质量流动速率 Melt Flow Rate |
|||
250℃,2.16kg 250℃,2.16kg |
8.6 | g/10min | ASTM D1238 |
熔体体积流动速率 Melt Volume Rate |
|||
250℃,2.16 kg 250℃,2.16 kg |
8.00 | cm³/10min | ISO 1133 |
收缩率 Shrinkage rate |
Internal Method | ||
MD MD 2 |
% | 内部方法 | |
MD MD 3 |
% | 内部方法 | |
MD MD 4 |
% | 内部方法 | |
MD:3.2 mm MD:3.2 mm |
% | 内部方法 | |
吸水率 Water absorption rate |
|||
饱和,23℃ Saturation, 23 ℃ |
% | ISO 62 | |
平衡,23℃,50% RH Equilibrium, 23 ℃, 50% RH |
% | ISO 62 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength |
|||
-30℃ -30℃ 10 |
kJ/m² | ISO 179/1eA | |
23℃ 23℃ 10 |
kJ/m² | ISO 179/1eA | |
23℃ 23℃ |
kJ/m² | ISO 179/2C | |
简支梁无缺口冲击强度 Charpy Unnotch Impact strength 10 |
ISO 179/1eU | ||
-30℃ -30℃ |
ISO 179/1eU | ||
23℃ 23℃ |
ISO 179/1eU | ||
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
ASTM D256 | ||
-30℃ -30℃ |
J/m | ASTM D256 | |
23℃ 23℃ |
J/m | ASTM D256 | |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch 11 |
ISO 180/1A | ||
23℃ 23℃ |
J/m | ASTM D4812 | |
-30℃ -30℃ |
kJ/m² | ISO 180-1A | |
23℃ 23℃ |
kJ/m² | ISO 180-1A | |
悬臂梁无缺口冲击强度 Notched impact strength of cantilever beam 11 |
ISO 180/1U | ||
-30℃ -30℃ |
ISO 180/1U | ||
23℃ 23℃ |
ISO 180/1U | ||
装有测量仪表的落镖冲击 Dart impact equipped with measuring instruments |
|||
23℃,Total Energy 23℃,Total Energy |
J | ASTM D3763 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
ASTM D648 | ||
0.45 MPa,未退火,6.4 mm 0.45 MPa, unannealed, 6.4 mm |
℃ | ASTM D648 | |
0.45 MPa,未退火,100 mm跨距 0.45 MPa, unannealed, 100 mm span 12 |
℃ | ISO 75-2/Be | |
1.8 MPa,未退火,3.2 mm 1.8 MPa, unannealed, 3.2 mm |
℃ | ASTM D648 | |
1.8 MPa,未退火,6.4 mm 1.8 MPa, unannealed, 6.4 mm |
℃ | ASTM D648 | |
热变形温度 Hot deformation temperature |
|||
1.8 MPa,未退火,100 mm跨距 1.8 MPa, unannealed, 100 mm span 12 |
℃ | ISO 75-2/Ae | |
1.8 MPa,未退火,64 mm跨距 1.8 MPa, unannealed, 64 mm span 13 |
℃ | ISO 75-2/Af | |
维卡软化温度 Vicat Softening Temp |
℃ | ASTM D1525 14 | |
维卡软化温度 Vicat Softening Temp |
|||
A50 A50 |
℃ | ISO 306/A50 | |
B50 B50 |
℃ | ISO 306 | |
B120 B120 |
℃ | ISO 306/B120 | |
球压测试 Ball pressure test |
|||
125℃ 125℃ |
IEC 60695-10-2 | ||
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
TD:-40~40℃ TD:-40~40℃ |
1/℃ | ASTM E831 | |
TD TD |
ISO 11359-2 | ||
-40 到 40℃ -40 to 40 ℃ |
cm/cm/℃ | ISO 11359-2 | |
MD MD |
ASTM E831 | ||
-40 到 40℃ -40 to 40 ℃ |
cm/cm/℃ | ASTM E831 | |
60 到 138℃ 60 to 138 ℃ |
cm/cm/℃ | ASTM E831 | |
MD MD |
ISO 11359-2 | ||
-40 到 40℃ -40 to 40 ℃ |
cm/cm/℃ | ISO 11359-2 | |
23 到 60℃ 23 to 60 ℃ |
cm/cm/℃ | ISO 11359-2 | |
导热系数 Thermal conductivity coefficient |
W/m/K | ISO 8302 | |
相对温度指数 Relative temperature index |
|||
电气性能 Electrical performance |
℃ | UL 746 | |
强度机械性能 Strength mechanical performance |
℃ | UL 746 | |
冲击机械性能 Impact mechanical performance |
℃ | UL 746 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表面电阻率 Surface resistivity |
ohms | IEC 60093 | |
体积电阻率 Volume resistivity |
ohms·cm | IEC 60093 | |
介电强度 Dielectric strength |
ASTM D149 | ||
1.6 mm,在油中 1.6 mm in oil |
kV/mm | ASTM D149 | |
3.2 mm,在空气中 3.2 mm in air |
kV/mm | ASTM D149 | |
介电强度 Dielectric strength |
IEC 60243-1 | ||
0.8 mm,在油中 0.8 mm in oil |
kV/mm | IEC 60243-1 | |
1 mm 1 mm 15 |
kV/mm | IEC 60243-1 | |
1.6 mm,在油中 1.6 mm in oil |
kV/mm | IEC 60243-1 | |
3.2 mm,在油中 3.2 mm in oil |
kV/mm | IEC 60243-1 | |
相对电容率 Relative permittivity |
IEC 60250 | ||
50 Hz 50 Hz |
IEC 60250 | ||
60 Hz 60 Hz |
IEC 60250 | ||
100 Hz 100 Hz |
IEC 60250 | ||
1 MHz 1 MHz |
IEC 60250 | ||
耗散因数 Dissipation factor |
IEC 60250 | ||
50 Hz 50 Hz |
IEC 60250 | ||
60 Hz 60 Hz |
IEC 60250 | ||
100 Hz 100 Hz |
IEC 60250 | ||
1 MHz 1 MHz |
IEC 60250 | ||
耐电弧性 Arc resistance 16 |
ASTM D495 | ||
相比漏电起痕指数 Compared to the leakage tracing index |
UL 746 | ||
相比漏电起痕指数 Compared to the leakage tracing index |
IEC 60112 | ||
CTI CTI |
V | IEC 60112 | |
解决方案 B Solution B |
V | IEC 60112 | |
高电弧燃烧指数(HAI) High Arc Burning Index (HAI) |
UL 746 | ||
高压电弧抗点燃指数(HVAR)(PLC) High voltage arc ignition resistance index (HVAR) (PLC) |
UL 746 | ||
高电压电弧起痕速率 High voltage arc marking rate |
|||
HVTR HVTR |
UL 746 | ||
热丝引燃 Hot wire ignition |
|||
HWI HWI |
UL 746 | ||
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame retardant level |
UL 94 | ||
0.71 mm 0.71 mm |
UL 94 | ||
3.00 mm 3.00 mm |
UL 94 | ||
灼热丝可燃性指数 Glowing wire flammability index |
|||
1.0 mm 1.0 mm |
℃ | IEC 60695-2-12 | |
极限氧指数 Extreme oxygen index |
% | ISO 4589-2 | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus 5 |
MPa | ASTM D638 | |
拉伸模量 Tensile modulus |
MPa | ISO 527-1-2 | |
拉伸强度 tensile strength |
|||
断裂 fracture |
MPa | ISO 527-2/50 | |
断裂 fracture 6 |
MPa | ASTM D638 | |
屈服 yield 6 |
MPa | ASTM D638 | |
屈服 yield |
MPa | ISO 527-2/50 | |
拉伸应变 Tensile strain |
|||
断裂 fracture 6 |
% | ASTM D638 | |
断裂 fracture |
% | ISO 527-2/50 | |
屈服 yield 6 |
% | ASTM D638 | |
屈服 yield |
% | ISO 527-2/50 | |
弯曲模量 Bending modulus 8 |
MPa | ISO 178 | |
50 mm跨距 50 mm span 7 |
MPa | ASTM D790 | |
弯曲强度 bending strength 8 , 9 |
MPa | ISO 178 | |
弯曲强度 bending strength 7 |
|||
屈服,50 mm跨度 Yield, 50 mm span 7 |
MPa | ASTM D790 | |
泰伯耐磨性 Taber abraser |
|||
1000 周期,1000 g,CS-17 转轮 1000 cycles, 1000 g, CS-17 wheels |
mg | 内部方法 | |
洛氏硬度 Rockwell hardness |
|||
R 级 R-level |
ISO 2039-2 | ||
球压硬度 Ball hardness |
|||
H358/30 H358/30 |
MPa | ISO 2039-1 | |
特殊值 Special value |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
TD TD 2 |
% | 内部方法 | |
TD TD 4 |
% | 内部方法 | |
TD TD 3 |
% | 内部方法 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 Tensile Bar |
3 0.75 to 2.3 mm |
4 2.3 to 4.6 mm |
5 0.20 in/min |
6 类型 1, 2.0 in/min |
7 0.051 in/min |
8 0.079 in/min |
9 Yield |
10 80*10*4 sp=62mm |
11 80*10*4 |
12 120*10*4 mm |
13 80*10*4 mm |
14 标准 B (120°C/h), 载荷2 (50N) |
15 速率 A (50°C/h), 载荷2 (50N) |
16 Short-Time |
17 钨电极 |
【新闻资讯】查看全部
亚洲化学品出口欧美市场活跃
2021-08-01 搜料网资讯: 在新冠肺炎疫情限制措施继续施压亚洲市场需求的背景下,亚洲一些主要的石化市场看到了向活跃的欧洲和美国市场出口的新机会。 在脂肪酸市场,欧盟对C18油酸的需求依 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |