牌号信息
搜索
搜索
牌号简介
Vydyne® 47H BG0693是一种通用的冲击改性PA66树脂。米色可选,热稳定,提高耐高温性能。Vydyne® 47H BG0693的热稳定包装是为了在预期持续或延长高温暴露的应用中使用时提供热耐久性而制定的。Vydyne® 47H BG0693是公认的所有加工和性能优势固有的PA66与提高冲击强度。该树脂具有高熔点、良好的表面润滑性、耐磨性和对许多化学品、机器和汽车油、溶剂和汽油的抵抗力等工程性能的良好平衡组合。Vydyne® 47H BG0693的设计是为了满足许多汽车技术规格中提出的关键低温冲击要求。 Vydyne 47H BG0693 is a general-purpose, impact-modified PA66 resin. Available in beige, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 47H BG0693 was formulated to provide thermal endurance when used in applications in which continuous or extended high-temperature exposure is anticipated. Vydyne 47H BG0693 is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact strength. This resin offers a well balanced combination of engineering properties characterized by high melt point, good surface lubricity, abrasion resistance and resistance to many chemicals, machine and motor oils, solvents and gasoline. Vydyne 47H BG0693 is designed to meet the critical low-temperature impact requirements called out in many automotive specifications.
47H BK0668是一种高性能、中冲击改性、热稳定的PA66树脂。 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.
产品描述
厂家:
美国奥升德 Ascend
美国奥升德 Ascend
类别:
PA66 PA66
PA66 PA66
填料:
用途:
汽车领域的应用,齿轮,紧固件,消费品应用领域,电气/电子应用领域,工业应用,连接器
电气/电子应用领域,消费品应用领域,齿轮,紧固件,工业应用,汽车领域的应用,连接器
性能特点:
易加工,韧性好,冲击性能好,耐磨,耐油,耐化学性,耐低温韧性,耐低温冲击,耐汽油,热稳定性好,防火阻燃等级HB Excellent Processability,Good flexibility,High impact resistance,Good wear resistance,Grease resistance,Solvent resistance,Low temperature toughness,low-temperature impact resistance,Gasoline resistance,Heat Stabilized,HB
易加工,韧性好,冲击性能好,耐磨,耐油,耐化学性,耐低温韧性,耐低温冲击,耐汽油,防火阻燃等级HB Excellent Processability,Good flexibility,High impact resistance,Good wear resistance,Grease resistance,Solvent resistance,Low temperature toughness,low-temperature impact resistance,Gasoline resistance,HB
加工条件:
注射成型 Injection Molding
注射成型 Injection Molding
技术参数
物理性能 PHYSICAL
Vydyne® 47H BG0693
Vydyne® 47H BK0668
单位 UNIT
测试方法 TEST METHOD
吸水率(23℃,24hr)
Water absorption rate
%
ISO 62
吸水率(平衡,23℃,50% RH)
Water absorption rate
%
ISO 62
密度
Density
g/cm³
ISO 1183
收缩率(MD:23℃,2.0 mm)
Shrinkage rate
%
ISO 294-4
收缩率(TD:23℃,2.0 mm)
Shrinkage rate
%
ISO 294-4
机械性能 MECHANICAL
Vydyne® 47H BG0693
Vydyne® 47H BK0668
单位 UNIT
测试方法 TEST METHOD
弯曲强度(23℃)
bending strength
MPa
ISO 178
弯曲模量(23℃)
Bending modulus
MPa
ISO 178
拉伸应变(断裂,23℃)
Tensile strain
%
ISO 527-2
拉伸强度(屈服,23℃)
tensile strength
MPa
ISO 527-2
拉伸强度(断裂,23℃)
tensile strength
MPa
ISO 527-2
拉伸模量(23℃)
Tensile modulus
MPa
ISO 527-2
冲击性能 IMPACT
Vydyne® 47H BG0693
Vydyne® 47H BK0668
单位 UNIT
测试方法 TEST METHOD
悬臂梁缺口冲击强度(-30℃)
Impact strength of cantilever beam notch
kJ/m²
ISO 180
悬臂梁缺口冲击强度(-40℃)
Impact strength of cantilever beam notch
kJ/m²
ISO 180
悬臂梁缺口冲击强度(23℃)
Impact strength of cantilever beam notch
kJ/m²
ISO 180
简支梁无缺口冲击强度(-30℃)
Charpy Unnotch Impact strength
ISO 179
简支梁无缺口冲击强度(-30℃)
Charpy Unnotch Impact strength
ISO 179/1eU
简支梁无缺口冲击强度(23℃)
Charpy Unnotch Impact strength
ISO 179
简支梁无缺口冲击强度(23℃)
Charpy Unnotch Impact strength
ISO 179/1eU
简支梁缺口冲击强度(-30℃)
Charpy Notched Impact Strength
kJ/m²
ISO 179
简支梁缺口冲击强度(-30℃)
Charpy Notched Impact Strength
kJ/m²
ISO 179/1eA
简支梁缺口冲击强度(-40℃)
Charpy Notched Impact Strength
kJ/m²
ISO 179
简支梁缺口冲击强度(-40℃)
Charpy Notched Impact Strength
kJ/m²
ISO 179/1eA
简支梁缺口冲击强度(23℃)
Charpy Notched Impact Strength
kJ/m²
ISO 179
简支梁缺口冲击强度(23℃)
Charpy Notched Impact Strength
kJ/m²
ISO 179/1eA
热性能 THERMAL
Vydyne® 47H BG0693
Vydyne® 47H BK0668
单位 UNIT
测试方法 TEST METHOD
热变形温度(0.45 MPa,未退火)
Hot deformation temperature
℃
ISO 75-2/B
热变形温度(1.8 MPa,未退火)
Hot deformation temperature
℃
ISO 75-2/A
熔融温度
Melting temperature
℃
ISO 11357-3
相对温度指数(0.75 mm)
Relative temperature index
℃
UL 746
相对温度指数(1.5 mm)
Relative temperature index
℃
UL 746
相对温度指数(3.0 mm)
Relative temperature index
℃
UL 746
相对温度指数(冲击机械性能)
Relative temperature index
UL 746
相对温度指数(强度机械性能)
Relative temperature index
UL 746
相对温度指数(电气性能)
Relative temperature index
UL 746
线性热膨胀系数(MD:23~55℃,2 mm)
Linear coefficient of thermal expansion
1/℃
ISO 11359-2
线性热膨胀系数(TD:23~55℃,2 mm)
Linear coefficient of thermal expansion
1/℃
ISO 11359-2
电气性能 ELECTRICAL
Vydyne® 47H BG0693
Vydyne® 47H BK0668
单位 UNIT
测试方法 TEST METHOD
介电强度(1 mm)
Dielectric strength
kV/mm
IEC 60243
体积电阻率(0.75 mm)
Volume resistivity
ohms·cm
IEC 60093
热丝引燃(0.75 mm)
Hot wire ignition
UL 746
热丝引燃(1.5 mm)
Hot wire ignition
UL 746
热丝引燃(3.0 mm)
Hot wire ignition
UL 746
热丝引燃(HWI)
Hot wire ignition
UL 746
相比漏电起痕指数(3.00 mm)
Compared to the leakage tracing index
V
IEC 60112
耐电弧性
Arc resistance
ASTM D495
高电压电弧起痕速率(HVTR)
High voltage arc marking rate
UL 746
高电弧燃烧指数(HAI) (0.75 mm)
High Arc Burning Index (HAI)
UL 746
高电弧燃烧指数(HAI) (1.5 mm)
High Arc Burning Index (HAI)
UL 746
高电弧燃烧指数(HAI) (3.0 mm)
High Arc Burning Index (HAI)
UL 746
阻燃性能 FLAMMABILITY
Vydyne® 47H BG0693
Vydyne® 47H BK0668
单位 UNIT
测试方法 TEST METHOD
灼热丝可燃性指数(0.75 mm)
Glowing wire flammability index
℃
IEC 60695-2-12
灼热丝可燃性指数(1.5 mm)
Glowing wire flammability index
℃
IEC 60695-2-12
灼热丝可燃性指数(3.0 mm)
Glowing wire flammability index
℃
IEC 60695-2-12
灼热丝起燃温度(0.75 mm)
Igniting temperature of the hot wire
℃
IEC 60695-2-13
灼热丝起燃温度(1.5 mm)
Igniting temperature of the hot wire
℃
IEC 60695-2-13
灼热丝起燃温度(3 mm)
Igniting temperature of the hot wire
℃
IEC 60695-2-13
阻燃等级(0.75 mm)
Flame retardant level
UL 94
阻燃等级(1.50 mm)
Flame retardant level
UL 94
阻燃等级(3.00 mm)
Flame retardant level
UL 94
补充信息
Vydyne® 47H BG0693
Vydyne® 47H BK0668
单位 UNIT
测试方法 TEST METHOD
汽车材料(thickness d = 1 mm)
Automotive materials
FMVSS 302