Sarlink TPV X6100系列是为消费者、汽车和工业应用而设计的工程材料,需要卓越的着色性和弹性性能。Sarlink® TPV X6190N是一种高硬度、低密度、多用途的热塑性硫化胶,不需要预干燥,可通过注射成型进行加工。 Sarlink® TPV X6100 series are engineered materials designed for consumer, automotive, and industrial applications requiring superior colorability and elastic performance. Sarlink® TPV X6190N is a higher hardness, low density, multi-purpose thermoplastic vulcanizate that does not require pre-drying and can be processed by injection molding.
Sarlink TPV 4100系列是专为要求苛刻的汽车和工业应用而设计的工程材料。sarlink 4190既有天然的也有黑色的,是一种低密度、高硬度的热塑性硫化胶,具有优异的抗弯曲疲劳性、热老化性、增强的弹性和弹性。sarlink 4190可用于注塑件、板材和型材挤压件,如挡风雨条和伸缩缝,也可吹塑成护套和管道。 SARLINK® TPV 4100 series are engineered materials designed primarily for demanding automotive and industrial applications. Available in both natural and black, SARLINK® 4190 is a low density, higher hardness thermoplastic vulcanizates with excellent flex fatigue resistance, heat aging, improved elasticity and resilience. SARLINK® 4190 can be used in injection molded parts, sheet and profile extrusions such as weather-stripping and expansion joints, and can also be blow molded into boots and ducts.
产品描述
厂家:
美国特诺尔爱佩斯 Teknor Apex
美国特诺尔爱佩斯 Teknor Apex
类别:
TPV TPV
TPV TPV
填料:
用途:
柔软触感应用,橡胶取代,消费品应用领域,汽车领域的应用,工业应用
橡胶取代,片材,家电部件,汽车内部零件,吹塑成型应用,汽车的发动机罩下的零件,管道密封,汽车外部零件,垫圈,农业应用,汽车领域的应用,耐候性密封条,工业应用,型材,大型家用电器和小型家用电器
性能特点:
易加工,韧性好,易流动,硬度高,粘结性好,有弹性,低密度,耐化学性,着色性好 Excellent Processability,Good flexibility,Good liquidity,Good Hardness,Good bond,Elastic,Low density,Solvent resistance,Good coloring
易加工,耐老化,韧性好,表面光泽度好,弯曲性能好,硬度高,粘结性好,耐疲劳性好,熔体强度好,有弹性,耐低温柔性,低密度,耐热性好,耐化学性,熔体稳定性高,防火阻燃等级HB Excellent Processability,Good heat aging resistance,Good flexibility,Good surface appearance,High elastic,Good Hardness,Good bond,Fatigue resistance,Good melt strength,Elastic,Low temperature toughness,Low density,Heat Resistance, Good,Solvent resistance,Higher melt stability,HB
加工条件:
注射成型 Injection Molding
吹塑成型
技术参数
物理性能 PHYSICAL
Sarlink® TPV X6190N
Sarlink® TPV 4190
单位 UNIT
测试方法 TEST METHOD
密度
Density
g/cm³
ASTM D792
密度
Density
g/cm³
ISO 1183
密度(--)
Density
g/cm³
ASTM D792
密度(--)
Density
g/cm³
ISO 1183
机械性能 MECHANICAL
Sarlink® TPV X6190N
Sarlink® TPV 4190
单位 UNIT
测试方法 TEST METHOD
邵氏硬度(邵氏 A,5 秒,挤出成型)
Shore hardness
邵氏硬度(邵氏 A,5 秒,挤出成型)
Shore hardness
ASTM D2240
邵氏硬度(邵氏 A,5 秒,挤出成型)
Shore hardness
ISO 868
邵氏硬度(邵氏 A,5 秒,注塑成型)
Shore hardness
邵氏硬度(邵氏 A,5 秒,注塑成型)
Shore hardness
ASTM D2240
邵氏硬度(邵氏 A,5 秒,注塑成型)
Shore hardness
ISO 868
弹性体 ELASTOMER
Sarlink® TPV X6190N
Sarlink® TPV 4190
单位 UNIT
测试方法 TEST METHOD
压缩形变(125℃,70 hr)
Compression deformation
%
压缩形变(125℃,70 hr)
Compression deformation
%
ASTM D395
压缩形变(125℃,70 hr)
Compression deformation
%
ISO 815
压缩形变(23℃,22 hr)
Compression deformation
%
压缩形变(23℃,22 hr)
Compression deformation
%
ASTM D395
压缩形变(23℃,22 hr)
Compression deformation
%
ISO 815
压缩形变(70℃,22 hr)
Compression deformation
%
压缩形变(70℃,22 hr)
Compression deformation
%
ASTM D395
压缩形变(70℃,22 hr)
Compression deformation
%
ISO 815
拉伸应变(TD,断裂)
Tensile strain
%
拉伸应变(断裂)
Tensile strain
%
ASTM D412
拉伸应变(断裂)
Tensile strain
%
ISO 37
拉伸应变(流量,断裂)
Tensile strain
%
拉伸应变(流量,断裂)
Tensile strain
%
ASTM D412
拉伸应变(流量,断裂)
Tensile strain
%
ISO 37
拉伸强度(MD,100% 应变)
tensile strength
MPa
ASTM D412
拉伸强度(MD,100% 应变)
tensile strength
MPa
ISO 37
拉伸强度(MD,断裂)
tensile strength
MPa
ASTM D412
拉伸强度(MD,断裂)
tensile strength
MPa
ISO 37
拉伸强度(TD,100% 应变)
tensile strength
MPa
ASTM D412
拉伸强度(TD,100% 应变)
tensile strength
MPa
ASTM D412, ISO 37
拉伸强度(TD,100% 应变)
tensile strength
MPa
ISO 37
拉伸强度(TD,断裂)
tensile strength
MPa
ASTM D412, ISO 37
拉伸强度(断裂)
tensile strength
MPa
ASTM D412
拉伸强度(断裂)
tensile strength
MPa
ISO 37
撕裂强度(--)
tear strength
kN/m
ISO 34-1
撕裂强度(TD)
tear strength
kN/m
ASTM D624
撕裂强度(TD)
tear strength
kN/m
ISO 34-1
补充信息
Sarlink® TPV X6190N
Sarlink® TPV 4190
单位 UNIT
测试方法 TEST METHOD
熔体表观粘度 - Capillary @ 206/s(200℃)
Apparent viscosity of melt - Capillary @ 206/s
Pa·s
ASTM D3835
熔体表观粘度 - Capillary @ 206/s(200℃)
Apparent viscosity of melt - Capillary @ 206/s
Pa·s
ISO 11443
熔体表观粘度(200℃)
Apparent viscosity of melt
Pa·s
ISO 11443
熔体表观粘度(Capillary:200℃)
Apparent viscosity of melt
Pa·s
ASTM D3835
热性能 THERMAL
Sarlink® TPV X6190N
Sarlink® TPV 4190
单位 UNIT
测试方法 TEST METHOD
相对温度指数(冲击机械性能)
Relative temperature index
℃
UL 746
相对温度指数(强度机械性能)
Relative temperature index
℃
UL 746
相对温度指数(电气性能)
Relative temperature index
℃
UL 746
老化性能 AGING
Sarlink® TPV X6190N
Sarlink® TPV 4190
单位 UNIT
测试方法 TEST METHOD
体积变化(125℃,70 hr,在IRM 903油中)
Volume change
%
ASTM D471
体积变化(125℃,70 hr,在IRM 903油中)
Volume change
%
ISO 1817
在空气中断裂时拉伸应力变化 - TD(135℃,1000 hr)
Changes in tensile stress when fractured in air - TD
%
ISO 188
在空气中断裂时拉伸应力变化 - TD(150℃,168 hr)
Changes in tensile stress when fractured in air - TD
%
ISO 188
空气中拉伸强度的变化率 - TD(100% 应变 135℃,1000 hr)
Change rate of tensile strength in air - TD
%
ISO 188
空气中拉伸强度的变化率 - TD(100% 应变 150℃,168 hr)
Change rate of tensile strength in air - TD
%
ISO 188
空气中拉伸强度的变化率 - TD(100% 应变,135℃,1000 hr)
Change rate of tensile strength in air - TD
%
ASTM D573
空气中拉伸强度的变化率 - TD(100% 应变,150℃,168 hr)
Change rate of tensile strength in air - TD
%
ASTM D573
空气中拉伸强度的变化率 - TD(135℃,1000 hr)
Change rate of tensile strength in air - TD
%
ASTM D573
空气中拉伸强度的变化率 - TD(135℃,1000 hr)
Change rate of tensile strength in air - TD
%
ISO 188
空气中拉伸强度的变化率 - TD(150℃,168 hr)
Change rate of tensile strength in air - TD
%
ASTM D573
空气中拉伸强度的变化率 - TD(150℃,168 hr)
Change rate of tensile strength in air - TD
%
ISO 188
空气中极限伸长率的变化率 - TD(135℃,1000 hr)
Change rate of ultimate elongation in air - TD
%
ASTM D573
空气中极限伸长率的变化率 - TD(150℃,168 hr)
Change rate of ultimate elongation in air - TD
%
ASTM D573
空气中硬度计硬度的变化率(邵氏 A,135℃,1000 hr)
The rate of change in hardness of a hardness tester in the air
ASTM D573
空气中硬度计硬度的变化率(邵氏 A,150℃,168 hr)
The rate of change in hardness of a hardness tester in the air
ASTM D573
空气中邵氏硬度的变化率(邵氏 A,135℃,1000 hr)
The rate of change of Shore hardness in air
ISO 188
空气中邵氏硬度的变化率(邵氏 A,150℃,168 hr)
The rate of change of Shore hardness in air
ISO 188
阻燃性能 FLAMMABILITY
Sarlink® TPV X6190N
Sarlink® TPV 4190
单位 UNIT
测试方法 TEST METHOD
1.00 mm,所有颜色
1.00 mm, all colors
UL 94