公司信息及水印
牌号简介 About |
---|
SABIC® LLDPE 726NE是一种丁烯线性低密度聚乙烯树脂。该等级的设计旨在使吹塑薄膜具有较高的刚度,从而具有良好的可加工性和其他性能(如抗穿刺性、冲击强度和热密封性)的良好总体平衡性。SABIC® LLDPE 726NE的典型应用是运输袋、生产袋、罐衬和运输袋。SABIC® LLDPE 726NE与低密度聚乙烯(15-85%)混合时具有非常好的光学性能。本文所述产品尤其未经测试,因此未经验证可用于医药/医疗应用。 SABIC® LLDPE 726NE is a butene linear low density polyethylene resin. This grade is designed to give blown films a relatively high stiffness for good machinability and a good overall balance of other performance properties, such as puncture resistance, impact strength and heat sealability. Application Typical applications for SABIC® LLDPE 726NE are shipping sacks, produce bags, can liners and carrier bags. SABIC® LLDPE 726NE has very good optical properties when blended with a LDPE (15-85%). The product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/medical applications. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
0.925 | g/cm³ | ISO 1183/A |
熔体质量流动速率 Melt Flow Rate |
|||
190℃,2.16kg 190℃,2.16kg |
0.70 | g/10min | ISO 1133 |
薄膜 film |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
薄膜厚度 film thickness |
|||
测试 test |
50 | µm | |
拉伸模量 Tensile modulus |
ISO 527-3 | ||
MD,50 µm,吹塑薄膜 MD, 50 µ m, blow molded film |
220 | MPa | |
TD,50 µm,吹塑薄膜 TD, 50 µ m, blow molded film |
240 | MPa | |
拉伸强度 tensile strength |
ISO 527-3 | ||
MD,屈服,50 µm,吹塑薄膜 MD, yield, 50 µ m, blow molded film |
MPa | ||
TD,屈服,50 µm,吹塑薄膜 TD, yield, 50 µ m, blow molded film |
MPa | ||
MD,断裂,50 µm,吹塑薄膜 MD, fracture, 50 µ m, blow molded film |
MPa | ||
TD,断裂,50 µm,吹塑薄膜 TD, fracture, 50 µ m, blow molded film |
MPa | ||
拉伸应变 Tensile strain |
ISO 527-3 | ||
MD,断裂,50 µm,吹塑薄膜 MD, fracture, 50 µ m, blow molded film |
% | ||
TD,断裂,50 µm,吹塑薄膜 TD, fracture, 50 µ m, blow molded film |
% | ||
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
悬臂梁冲击强度 Izod notched impact strength |
|||
50µm,吹塑成型 50 µ m, blow molded |
J/cm | ASTM D4272 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
维卡软化温度 Vicat Softening Temp |
℃ | ISO 306/A | |
熔融温度 Melting temperature |
|||
DSC DSC |
℃ | 内部方法 | |
光学性能 optical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
光泽度 gloss |
|||
45°,50.0 µm,吹塑薄膜 45 °, 50.0 µ m, blow molded film |
ASTM D2457 | ||
雾度 Haze |
|||
50 µm,吹塑薄膜 50 µ m, blow molded film |
% | ASTM D1003 | |
补充信息 Supplementary information |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
抗穿刺性 Puncture resistance |
|||
吹塑薄膜,50.0 µm Blow molded film, 50.0 µ m |
J/m | 内部方法 | |
撕裂强度 tear strength 1 |
ISO 6383-2 | ||
MD,50 µm MD,50 µm |
kN/m | ||
TD,50 µm TD,50 µm |
kN/m | ||
memo_intro memo_intro |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 Blown Film |
【新闻资讯】查看全部
工程塑料注塑后发生模垢缘由及对策
2016-05-13 1、模垢的形成 几乎所有热塑性塑料注塑成型时都会发生模垢。当最终产品的功能要求必须混入相关的添加物时(例如改质剂、防火剂等),成型过程中,这些添加物非常可能残留在模穴表面,导致形成模垢。 模垢的形成还有其他方面的原因,最常见的原因如下: ▶原料的热分解产物; ▶注射成型时,熔体流动极端的剪切力; ▶不适当的排气; 如上造成的模垢时常是不同因素的组合产物,并且寻求发现这些模垢究竟是什么原因造成及如 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |