Silopren® LSR 3486/20是一种双组分液体硅橡胶注射成型工艺。这种材料是制造需要自润滑特性的弹性体制品的最佳候选材料。自润滑效果是通过长时间从硫化胶中渗出的液体来实现的。通常在硫化后的几小时到一天之间开始。Silopren® LSR 3486/20液体硅橡胶在硫化后未经后固化,压缩永久变形较低。由Silopren® LSR 3486/20液态硅橡胶组成的硫化胶的主要特点和优点通常具有以下特性:低压缩永久变形,无后固化自润滑特性,低粘度,快速固化,高热稳定性,优异的耐老化性,易于着色,因其突出的应用潜力G属性,Silopren® LSR 3486/20液体硅橡胶是以下弹性材料线束应用的理想选择:电缆密封垫,密封垫圈,密封塞密封 Silopren LSR 3486/20 is a two-component liquid silicone rubber for injection molding processes. This material is an excellent candidate to consider for the manufacture of elastomeric articles requiring self-lubricating properties. The self-lubricating effect is achieved by a fluid which exudes out of the vulcanizate over an extended period of time. It typically starts between a few hours and one day after vulcanization. Silopren LSR 3486/20 liquid silicone rubber shows a low compression set after vulcanization without post-curing. Key Features and Benefits Vulcanizates consisting of Silopren LSR 3486/20 liquid silicone rubber are typically distinguished by the following properties: low compression set without post-cure self-lubricating properties low viscosity fast cure high thermal stability outstanding resistance to aging easy to color Potential Applications Because of the outstanding properties, Silopren LSR 3486/20 liquid silicone rubber is an excellent candidate to consider for use in wire harness applications for the following elastomeric articles: cable seals mat seals grommets gaskets plug seals |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.10 | g/cm³ | DIN 53479 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
|||
邵氏 A Shaw's A |
20 | DIN 53505 | |
弹性体 elastic body |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength |
6.80 | MPa | DIN 53504 |
拉伸应变 Tensile strain |
|||
断裂 fracture |
760 | % | DIN 53504 |
撕裂强度 tear strength 2 |
12.0 | kN/m | ASTM D624 |
压缩形变 Compression deformation |
|||
175℃,22 hr 175℃,22 hr |
% | ISO 815 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热固组件 Thermosetting components |
|||
部件 A Component A |
|||
部件 B Component B |
|||
贮藏期限 Storage period |
|||
< 27℃ < 27℃ |
wk | ||
后固化时间 Post curing time |
|||
200℃ 200℃ |
hr | ||
补充信息 Supplementary information |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
Vulcanization(175℃) Vulcanization(175℃) |
min | ||
Uncured Properties Uncured Properties |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
颜色 colour |
|||
-- -- 3 |
|||
-- -- 4 |
|||
粘度 viscosity |
DIN 53018 | ||
20℃ 20℃ 4 |
Pa·s | DIN 53018 | |
20℃ 20℃ 3 |
Pa·s | DIN 53018 | |
储存稳定性 storage stability |
|||
20 ℃ 20 ℃ |
min | ||
Cured Properties Cured Properties |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
Fluid Content Fluid Content |
|||
-- -- 3 |
% | ||
-- -- 4 |
% |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 B 模具 |
3 Part B |
4 Part A |
【新闻资讯】查看全部
助剂企业大幅涨价 上调幅度达10%
2017-03-07 重要链接:今年还是中国的峰会大年,实体行业需要接连面对3月份开“两会”,5月份要开“一带一路”峰会,9月份的金砖国家峰会,以及近几年约定俗成的第四季度雾霾大会。这也导致国内环保压力急剧增大,并且影响到各种原料的上涨! 据悉,第十二届全国人民代表大会第五次会议和政协第十二届全国委员会第五次会议,将分别于2017年3月5日和3月3日在北京召开。为确保“两会”在此期间能够拥有蓝天白云,防止高污染,京津冀相关政府紧急布局,有多家媒体报道当地部分化工企业已经收到2月下旬至3月上旬的环 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |