牌号简介 About |
---|
Torlon 4275是耐磨等级的聚酰胺 - 酰亚胺(PAI) 。该牌号树脂的机械性能和耐磨损性取得了极好的平衡。具有高挠曲强度和抗压强度,在高流速和高压条件下,摩擦系数低,耐磨损性优异。 在所有能耐受275 ℃( 525°F )高温的热塑性树脂中,Torlon PAI具有最高的强度和刚度 。并具有优异的耐磨损性、抗蠕变性和耐化学性。 Torlon 4275 聚酰胺 - 酰亚胺树脂可用于止推垫圈、花键衬、阀座、衬套、轴承、耐磨环、凸轮和其它需要在高温条件下保持强度和耐磨损的产品中。 Torlon® 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with a low coefficient of friction and outstanding wear resistance at both high velocity and high pressure conditions. Torlon® PAI has the highest strength and stiffness of any thermoplastic up to 275°C (525°F). It has outstanding resistance to wear, creep and chemicals. Potential applications for Torlon® 4275 polyamide-imide include thrust washers, spline liners, valve seats, bushings, bearings, wear rings, cams and other applications requiring strength at high temperature and resistance to wear. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.51 | g/cm³ | ASTM D792 |
收缩率 Shrinkage rate |
|||
MD MD |
0.25 到 0.45 | % | ASTM D955 |
吸水率 Water absorption rate |
|||
24hr 24hr |
0.33 | % | ASTM D570 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
|||
-- -- |
8830 | MPa | ASTM D638 |
-- -- 2 |
7790 | MPa | ASTM D1708 |
拉伸强度 tensile strength |
MPa | ASTM D638 | |
拉伸强度 tensile strength 3 |
MPa | ASTM D1708 | |
拉伸应变 Tensile strain |
|||
断裂 fracture |
% | ASTM D638 | |
断裂 fracture 2 |
% | ASTM D1708 | |
弯曲模量 Bending modulus |
ASTM D790 | ||
23℃ 23℃ |
MPa | ASTM D790 | |
232℃ 232℃ |
MPa | ASTM D790 | |
弯曲强度 bending strength |
ASTM D790 | ||
23℃ 23℃ |
MPa | ASTM D790 | |
232℃ 232℃ |
MPa | ASTM D790 | |
压缩模量 Compression modulus |
MPa | ASTM D695 | |
压缩强度 compressive strength |
MPa | ASTM D695 | |
摩擦系数 friction coefficient |
|||
-- -- 4 |
ASTM D3702 | ||
-- -- 5 |
ASTM D3702 | ||
-- -- 6 |
ASTM D1894 | ||
-- -- 7 |
ASTM D1894 | ||
磨损因数 Wear factor |
ASTM D3702 | ||
5.2 MPa,0.38 m/sec 5.2 MPa,0.38 m/sec 8 |
10^-8 mm³/N·m | ASTM D3702 | |
6.9 MPa,0.38 m/sec 6.9 MPa,0.38 m/sec 8 |
10^-8 mm³/N·m | ASTM D3702 | |
3.4 MPa,0.25 m/sec 3.4 MPa,0.25 m/sec 9 |
10^-8 mm³/N·m | ASTM D3702 | |
0.22 MPa,4.1 m/sec 0.22 MPa,4.1 m/sec 9 |
10^-8 mm³/N·m | ASTM D3702 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
J/m | ASTM D256 | |
悬臂梁无缺口冲击强度 Notched impact strength of cantilever beam |
J/m | ASTM D256 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ASTM D648 | |
导热系数 Thermal conductivity coefficient |
W/m/K | ASTM C177 | |
线性热膨胀系数 Linear coefficient of thermal expansion |
cm/cm/℃ | ASTM D696 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表面电阻率 Surface resistivity |
ohms | ASTM D257 | |
体积电阻率 Volume resistivity |
ohms·cm | ASTM D257 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 以前,ASTM标准试验方法D1708用于测量PAI和类似材料的拉伸性能,因为小试样能节约材料。现在使用最广泛的是ASTM D638 1 Bar 试样 。所含D1708数值仅用作历史参考,不与D638值作对照用。 |
3 以前,ASTM标准试验方法D1708用于测量PAI和类似材料的拉伸性能,因为小试样能节省材料。现在使用最广泛的是ASTM D638 1 Bar 试样 。所含D1708数值仅用作历史参考,不与D638值作对照用。 |
4 润滑: 0.25 m/s, 6.9 MPa (75 fpm, 1000 psi) |
5 润滑: 4 m/s, 5.2 MPa (800 fpm, 750 psi) |
6 干燥:0.25 m/s, 3.4 MPa (50 fpm, 500 psi) |
7 干燥:4 m/s, 0.2 MPa (800 fpm, 31.25 psi) |
8 润滑 |
9 干燥 |
【新闻资讯】查看全部
巴斯夫与CHINAPLAS携手设计师与品牌商
2017-02-13 在CHINAPLAS 2017国际橡塑展"设计x创新"同期活动中,巴斯夫将携手CHINAPLAS展出包括机械手、免充气自行车胎、别具一格的儿童玩具和混合动力电子设备等在内的一系列旨在提高智能生活的优秀设计品原型。这些展品均由顶级设计师和品牌商联合开发,由巴斯夫支持,并采用了巴斯夫的先进材料制造而成。 这些以"塑"三角(TRIO)命名的共创项目体现了巴斯夫与设计师和品牌商之间的合作。巴斯夫为设计品原型提供制作材料,而产品理念则由设计师和品牌商共同构思。凭借强大的研发、技术、工 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |