牌号简介 About |
---|
Lexan ML7667树脂Lexan ML7667专用聚碳酸酯(PC)树脂是一种9%玻璃纤维增强,紫外线稳定,阻燃注射成型等级。该中流量专用PC树脂将UL94V0@1.5mm、5VB@3.0mm阻燃剂与无氯、无溴阻燃剂相结合,具有优良的加工性能、改善的释放性能和良好的冲击性能。本产品仅提供有限的不透明颜色,可能是广泛应用的理想选择,即电气和电子外壳应用。 LEXAN ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.0mm flame retardancy based on non-chlorine, non-bromine FR agents with excellent processability, improved release performance and good impact performance. This product is available in limited opaque colors only and may be an excellent candidate for a broad range of applications, i.e. electrical and electronic enclosure applications. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.26 | g/cm³ | ASTM D792 |
密度 Density |
1.26 | g/cm³ | ISO 1183 |
熔体质量流动速率 Melt Flow Rate |
|||
300℃,1.20kg 300℃,1.20kg |
9.0 | g/10min | ASTM D1238 |
熔体体积流动速率 Melt Volume Rate |
|||
300℃,1.2 kg 300℃,1.2 kg |
8.00 | cm³/10min | ISO 1133 |
收缩率 Shrinkage rate |
|||
MD:3.2 mm MD:3.2 mm |
0.20 to 0.60 | % | 内部方法 |
吸水率 Water absorption rate |
|||
饱和,23℃ Saturation, 23 ℃ |
% | ISO 62 | |
平衡,23℃,50% RH Equilibrium, 23 ℃, 50% RH |
% | ISO 62 | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus 2 |
MPa | ASTM D638 | |
拉伸模量 Tensile modulus |
MPa | ISO 527-1-2 | |
拉伸强度 tensile strength 3 |
|||
断裂 fracture 3 |
MPa | ASTM D638 | |
断裂 fracture |
MPa | ISO 527-2/5 | |
屈服 yield |
MPa | ISO 527-2/5 | |
屈服 yield 3 |
MPa | ASTM D638 | |
拉伸应变 Tensile strain |
|||
断裂 fracture |
% | ISO 527-2/5 | |
断裂 fracture 4 |
% | ASTM D638 | |
屈服 yield 3 |
% | ASTM D638 | |
屈服 yield |
% | ISO 527-2/5 | |
弯曲模量 Bending modulus 5 |
MPa | ISO 178 | |
50 mm跨距 50 mm span 4 |
MPa | ASTM D790 | |
弯曲强度 bending strength 5 , 6 |
MPa | ISO 178 | |
弯曲强度 bending strength 4 |
|||
屈服,50 mm跨度 Yield, 50 mm span 4 |
MPa | ASTM D790 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength 7 |
ISO 179/1eA | ||
-30℃ -30℃ |
kJ/m² | ISO 179/1eA | |
23℃ 23℃ |
kJ/m² | ISO 179/1eA | |
简支梁无缺口冲击强度 Charpy Unnotch Impact strength 7 |
ISO 179/1eU | ||
-30℃ -30℃ |
ISO 179/1eU | ||
23℃ 23℃ |
ISO 179/1eU | ||
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
ASTM D256 | ||
-30℃ -30℃ |
J/m | ASTM D256 | |
23℃ 23℃ |
J/m | ASTM D256 | |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch 8 |
ISO 180/1A | ||
-30℃ -30℃ |
kJ/m² | ISO 180-1A | |
23℃ 23℃ |
kJ/m² | ISO 180-1A | |
悬臂梁无缺口冲击强度 Notched impact strength of cantilever beam 8 |
ISO 180/1U | ||
-30℃ -30℃ |
ISO 180/1U | ||
23℃ 23℃ |
ISO 180/1U | ||
装有测量仪表的落镖冲击 Dart impact equipped with measuring instruments |
|||
23℃,Total Energy 23℃,Total Energy |
J | ASTM D3763 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature 9 |
|||
1.8 MPa,未退火,3.2 mm 1.8 MPa, unannealed, 3.2 mm |
℃ | ASTM D648 | |
1.8 MPa,未退火,100 mm跨距 1.8 MPa, unannealed, 100 mm span 9 |
℃ | ISO 75-2/Ae | |
维卡软化温度 Vicat Softening Temp |
℃ | ASTM D1525 10 | |
维卡软化温度 Vicat Softening Temp |
|||
B50 B50 |
℃ | ISO 306 | |
B120 B120 |
℃ | ISO 306/B120 | |
球压测试 Ball pressure test |
|||
125℃ 125℃ |
IEC 60695-10-2 | ||
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
TD:-40~40℃ TD:-40~40℃ |
1/℃ | ASTM E831 | |
TD:-40~40℃ TD:-40~40℃ |
1/℃ | ISO 11359-2 | |
MD:-40~40℃ MD:-40~40℃ |
1/℃ | ISO 11359-2 | |
MD:-40~40℃ MD:-40~40℃ |
1/℃ | ASTM E831 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
相比漏电起痕指数 Compared to the leakage tracing index |
UL 746 | ||
相比漏电起痕指数 Compared to the leakage tracing index |
V | IEC 60112 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame retardant level |
UL 94 | ||
0.75 mm 0.75 mm |
UL 94 | ||
1.50 mm 1.50 mm |
UL 94 | ||
3.00 mm 3.00 mm |
UL 94 | ||
灼热丝可燃性指数 Glowing wire flammability index |
|||
1.1 mm 1.1 mm |
℃ | IEC 60695-2-12 | |
灼热丝起燃温度 Igniting temperature of the hot wire |
IEC 60695-2-13 | ||
1 mm 1 mm |
℃ | IEC 60695-2-13 | |
2 mm 2 mm |
℃ | IEC 60695-2-13 | |
2.5 mm 2.5 mm |
℃ | IEC 60695-2-13 | |
3 mm 3 mm |
℃ | IEC 60695-2-13 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 0.20 in/min |
3 类型 1, 0.20 in/min |
4 0.051 in/min |
5 0.079 in/min |
6 Yield |
7 80*10*3 sp=62mm |
8 80*10*3 |
9 120*10*4 mm |
10 标准 B (120°C/h), 载荷2 (50N) |
【新闻资讯】查看全部
学生采用PLA和TPU材料,通过3D打印技术重新设计伦敦火车站
2021-04-12 搜料网资讯: 来自UCL巴特莱特建筑学院的四名硕士生组成的小组,设计并3D打印了一种新颖的多材料建筑面板。 该项目被称为Metaplas,利用刚性和柔性可回收聚合物的组合,通过3D打印创 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |