KetaSpire KT -820 CF30是低流量、30 %碳纤增强聚醚醚酮(PEEK) 。在温度接近300℃时,碳纤增强 KetaSpire PEEK 的机械性能达到行业最高水平,并且,具有KetaSpire 产品系列最低的线性热膨胀系数。KetaSpire PEEK按照行业最高标准加工,以兼具各种出色的性能为特征,包括优异的耐磨损性、一流的抗疲劳性、易于熔融加工、高纯度、优异的耐有机物、酸和碱等化学物质的性能。 这些特性使得它非常适合医疗保健、交通运输、电子、化学处理和其它工业用途。 KetaSpire® KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical properties at temperatures approaching 300°C, and the lowest coefficient of linear thermal expansion within the KetaSpire® product family. KetaSpire® PEEK is produced to the highest industry standards and is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, ease of melt processing, high purity, and excellent chemical resistance to organics, acids and bases. These properties make it well-suited for applications in healthcare, transportation, electronics, chemical processing and other industrial uses. |
技术参数 Technical Data | |||
---|---|---|---|
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
|||
-- -- |
69 | J/m | ASTM D256 |
-- -- |
10 | kJ/m² | ISO 180 |
悬臂梁无缺口冲击强度 Notched impact strength of cantilever beam |
|||
-- -- |
750 | J/m | ASTM D4812 |
-- -- |
44 | kJ/m² | ISO 180 |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
1.8 MPa,退火 1.8 MPa, annealed |
315 | ℃ | ASTM D648 |
玻璃化转变温度 Glass transition temperature |
℃ | ASTM D3418 | |
熔融峰值温度 Melting peak temperature |
℃ | ASTM D3418 | |
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
MD:-50~50℃ MD:-50~50℃ |
1/℃ | ASTM E831 | |
比热 specific heat |
DSC | ||
50℃ 50℃ |
J/kg/℃ | DSC | |
200℃ 200℃ |
J/kg/℃ | DSC | |
导热系数 Thermal conductivity coefficient |
W/m/K | ASTM E1530 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame retardant level |
UL 94 | ||
0.80 mm 0.80 mm |
UL 94 | ||
1.60 mm 1.60 mm |
UL 94 | ||
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
|||
邵氏 D,1 秒 Shore D, 1 second |
ASTM D2240 | ||
洛氏硬度 Rockwell hardness |
|||
M 级 M-level |
ASTM D785 | ||
拉伸模量 Tensile modulus |
|||
-- -- 4 |
MPa | ASTM D638 | |
-- -- |
MPa | ISO 527-2/1A/1 | |
拉伸强度 tensile strength |
|||
屈服 yield |
MPa | ISO 527-2/1A/5 | |
-- -- |
MPa | ASTM D638 | |
拉伸应变 Tensile strain |
|||
断裂 fracture 4 |
% | ASTM D638 | |
断裂 fracture |
% | ISO 527-2/1A/5 | |
弯曲模量 Bending modulus |
|||
-- -- |
MPa | ASTM D790 | |
-- -- |
MPa | ISO 178 | |
弯曲强度 bending strength |
|||
-- -- |
MPa | ASTM D790 | |
-- -- |
MPa | ISO 178 | |
压缩强度 compressive strength |
MPa | ASTM D695 | |
剪切强度 shear strength |
MPa | ASTM D732 | |
泊松比 Poisson's ratio |
ASTM E132 | ||
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
g/cm³ | ASTM D792 | |
熔体质量流动速率 Melt Flow Rate |
|||
400℃,2.16kg 400℃,2.16kg |
g/10min | ASTM D1238 | |
收缩率 Shrinkage rate 3 |
ASTM D955 | ||
MD:3.2 mm MD:3.2 mm |
% | ASTM D955 | |
TD:3.2 mm TD:3.2 mm |
% | ASTM D955 | |
吸水率 Water absorption rate |
|||
24hr 24hr |
% | ASTM D570 | |
熔体表观粘度 Apparent viscosity of melt |
|||
400℃,1000 sec^-1 400℃,1000 sec^-1 |
Pa·s | ASTM D3835 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 5" x 0.5" x 0.125" bars |
3 0.20 in/min |