公司信息及水印
牌号简介 About |
---|
EMERGE™ PC 8080-15高级树脂是一种不透明的阻燃PC树脂,不含氯化、溴化或磷基添加剂。这种树脂含有脱模剂,并且是紫外线稳定的。它结合了良好的机械和高热性能,并保持良好的加工性能。EMERGE™ PC 8080-15的UL 94 V-0额定值为0.7 mm。应用:电子电器 EMERGE™ PC 8080-15 advanced resin is an opaque, ignition resistant PC resin that contains no chlorinated or brominated or phosphorous based additives. This resin contains mould release and it is UV stabilized. It combines good mechanical and high heat properties and maintains excellent processability. EMERGE™ PC 8080-15 has a UL 94 V-0 rating at 0.7 mm. Applications: Electrical Electronics |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.20 | g/cm³ | ISO 1183/B |
熔体质量流动速率 Melt Flow Rate |
|||
300℃,1.20kg 300℃,1.20kg |
15 | g/10min | ISO 1133 |
收缩率 Shrinkage rate |
0.50 到 0.70 | % | ISO 294-4 |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength |
|||
23℃ 23℃ |
25 | kJ/m² | ISO 179/1eA |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
|||
23℃ 23℃ |
65 | kJ/m² | ISO 180-A |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
0.45 MPa,退火 0.45 MPa, annealed |
℃ | ISO 75-2/B | |
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ISO 75-2/A | |
1.8 MPa,退火 1.8 MPa, annealed |
℃ | ISO 75-2/A | |
维卡软化温度 Vicat Softening Temp |
|||
B50 B50 |
℃ | ISO 306 | |
球压温度 Ball pressure temperature |
℃ | IEC 60335-1 | |
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
MD MD |
1/℃ | ISO 11359-2 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表面电阻率 Surface resistivity |
ohms | IEC 60093 | |
体积电阻率 Volume resistivity |
ohms·cm | IEC 60093 | |
介电强度 Dielectric strength |
kV/mm | IEC 60243-1 | |
介电常数 Dielectric constant |
|||
1 Hz 1 Hz |
|||
50 Hz 50 Hz |
|||
耗散因数 Dissipation factor |
|||
1 Hz 1 Hz |
|||
50 Hz 50 Hz |
|||
相比漏电起痕指数 Compared to the leakage tracing index |
|||
解决方案 A Solution A |
V | IEC 60112 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame retardant level 4 |
|||
0.70 mm 0.70 mm |
|||
2.00 mm 2.00 mm |
|||
2.50 mm 2.50 mm |
|||
灼热丝可燃性指数 Glowing wire flammability index 4 |
|||
1.0 mm 1.0 mm |
℃ | ||
2.0 mm 2.0 mm |
℃ | ||
3.0 mm 3.0 mm |
℃ | ||
灼热丝起燃温度 Igniting temperature of the hot wire 4 |
|||
1 mm 1 mm |
℃ | ||
2 mm 2 mm |
℃ | ||
3 mm 3 mm |
℃ | ||
极限氧指数 Extreme oxygen index 4 |
% | ISO 4589-2 | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
洛氏硬度 Rockwell hardness |
|||
M 级 M-level |
|||
R 级 R-level |
|||
拉伸模量 Tensile modulus |
MPa | ISO 527-1-2 | |
拉伸强度 tensile strength |
|||
屈服 yield |
MPa | ||
断裂 fracture |
MPa | ||
拉伸应变 Tensile strain |
|||
断裂 fracture |
% | ISO 527-2/50 | |
弯曲模量 Bending modulus 3 |
MPa | ISO 178 | |
弯曲强度 bending strength 3 |
MPa | ISO 178 |
备注 |
---|
3. 2.0 mm/min |
4. This rating not intended to reflect hazards presented by this or any other material under actual fire conditions. |
【新闻资讯】查看全部
PBT资料的5大使用范围
2018-02-05 PBT是工程塑料中工业化最晚但发展最快的一个品种,它以其优良的综合性能,良好的成型加工性和性价比,优良的机械性能,机械强度高,耐疲劳性和尺寸稳定好,蠕变也小。这些性能在高温条件下也极少有变化,非常适合用于汽车、电子等领域,今天小编就一点点的老来了解PBT材料的应用。 一、发展史 1942德国科学家P.Schlack研制出成PBT树脂,之后美国Celanese公司(现为Ticona)进行工业开发,以Celanex商品名上市 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |