公司信息及水印
牌号简介 About |
---|
Adsyl 5 C 39 F ST是一种高级聚烯烃,专门设计用于共挤和金属化薄膜应用中的密封层。该等级具有极低的密封启动温度和优良的光学性能。它在高速BOPP生产线上提供了增强的可加工性。它含有抗阻塞添加剂。 Adsyl 5 C 39 F ST is an advanced polyolefin, specially designed for use as a sealing layer in co-extruded and metallizable film applications. This grade features a very low seal initiation temperature and excellent optics. It provides enhanced processability on high speed BOPP lines. It contains anti-block additives. For regulatory information please refer to Adsyl 5 C 39 F ST Product Stewardship Bulletin (PSB). |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
0.900 | g/cm³ | ISO 1183/A |
熔体质量流动速率 Melt Flow Rate |
|||
230℃,2.16kg 230℃,2.16kg |
6.0 | g/10min | ISO 1133 |
薄膜 film |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
薄膜厚度 film thickness |
|||
测试 test |
50 | µm | |
拉伸模量 Tensile modulus |
ISO 527-3/25 | ||
MD,50 µm,铸造薄膜 MD, 50 µ m, cast thin film |
260 | MPa | ISO 527-3/25 |
TD,50 µm,铸造薄膜 TD, 50 µ m, cast thin film |
240 | MPa | ISO 527-3/25 |
拉伸强度 tensile strength |
ISO 527-3/500 | ||
MD,屈服,50 µm,吹塑薄膜 MD, yield, 50 µ m, blow molded film |
MPa | ISO 527-3/500 | |
TD,屈服,50 µm,吹塑薄膜 TD, yield, 50 µ m, blow molded film |
MPa | ISO 527-3/500 | |
拉伸强度 tensile strength |
ISO 527-3/500 | ||
MD,断裂,50 µm,吹塑薄膜 MD, fracture, 50 µ m, blow molded film |
MPa | ISO 527-3/500 | |
TD,断裂,50 µm,吹塑薄膜 TD, fracture, 50 µ m, blow molded film |
MPa | ISO 527-3/500 | |
拉伸应变 Tensile strain |
ISO 527-3/500 | ||
MD,断裂,50 µm,铸造薄膜 MD, fracture, 50 µ m, cast thin film |
% | ISO 527-3/500 | |
TD,断裂,50 µm,铸造薄膜 TD, fracture, 50 µ m, cast thin film |
% | ISO 527-3/500 | |
拉伸应变 Tensile strain |
ISO 527-3/500 | ||
MD,屈服,50 µm,铸造薄膜 MD, yield, 50 µ m, cast thin film |
% | ISO 527-3/500 | |
TD,屈服,50 µm,铸造薄膜 TD, yield, 50 µ m, cast thin film |
% | ISO 527-3/500 | |
始封温度 Initial sealing temperature |
℃ | ||
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
0.45 MPa,未退火 0.45 MPa, unannealed |
℃ | ISO 75-2/B | |
维卡软化温度 Vicat Softening Temp |
|||
A50 A50 |
℃ | ISO 306/A50 | |
熔融温度 Melting temperature |
℃ | ISO 11357-3 | |
光学性能 optical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
光泽度 gloss |
|||
45°,50.0 µm,铸造薄膜 45 °, 50.0 µ m, cast thin film |
ASTM D2457 | ||
雾度 Haze |
|||
50 µm,铸造薄膜 50 µ m, cast thin film |
% | ASTM D1003 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
【新闻资讯】查看全部
海南炼化乙烯项目年产20万吨气相法聚丙烯装置中交
2022-07-20 7月18日,由五建公司承建的海南炼化100万吨/年乙烯及炼油改扩建工程20万吨/年气相聚丙烯装置成功达标交付。 五建海南炼化乙烯项目部开工以来,从加强物资供应保障入手,每周组织 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |