牌号简介 About |
---|
Noryl NH7112树脂是一种10%的玻璃增强改性PPE-PS混合物。该材料提供了一个特殊的强度和尺寸稳定性平衡,同时使用非卤化阻燃剂,以达到UL94的火焰等级。这一等级可以通过挤压或注射成型加工。诺丽尔NH7112可定制颜色,可能是一个优秀的材料候选人在电气和电子市场使用。 NORYL NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to achieve UL94 flame ratings. This grade can be processed via extrusion or injection molding. NORYL NH7112 is available in custom colors and may be an excellent material candidate for use in electrical and electronics markets. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
|||
-- -- |
1.16 | g/cm³ | ASTM D792 |
-- -- |
1.17 | g/cm³ | ISO 1183 |
熔体质量流动速率 Melt Flow Rate |
|||
280℃,5.0kg 280℃,5.0kg |
6.5 | g/10min | ASTM D1238 |
熔体体积流动速率 Melt Volume Rate |
|||
300℃,5 kg 300℃,5 kg |
14.0 | cm³/10min | ISO 1133 |
收缩率 Shrinkage rate |
|||
MD:3.2 mm MD:3.2 mm |
0.20 到 0.40 | % | 内部方法 |
吸水率 Water absorption rate |
|||
饱和,23℃ Saturation, 23 ℃ |
% | ||
平衡,23℃,50% RH Equilibrium, 23 ℃, 50% RH |
% | ||
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
|||
-- -- 3 |
MPa | ASTM D638 | |
-- -- |
MPa | ISO 527-1-2 | |
拉伸强度 tensile strength |
|||
屈服 yield 4 |
MPa | ASTM D638 | |
屈服 yield |
MPa | ISO 527-2/5 | |
断裂 fracture 4 |
MPa | ASTM D638 | |
断裂 fracture |
MPa | ISO 527-2/5 | |
拉伸应变 Tensile strain |
|||
屈服 yield 4 |
% | ASTM D638 | |
屈服 yield |
% | ISO 527-2/5 | |
断裂 fracture 4 |
% | ASTM D638 | |
断裂 fracture |
% | ISO 527-2/5 | |
弯曲模量 Bending modulus |
|||
50 mm跨距 50 mm span 5 |
MPa | ASTM D790 | |
-- -- 6 |
MPa | ISO 178 | |
弯曲强度 bending strength |
|||
-- -- 6 , 7 |
MPa | ISO 178 | |
-- -- 6 , 8 |
MPa | ISO 178 | |
屈服,50 mm跨度 Yield, 50 mm span 5 |
MPa | ASTM D790 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength 9 |
|||
-30℃ -30℃ |
kJ/m² | ISO 179/1eA | |
23℃ 23℃ |
kJ/m² | ISO 179/1eA | |
简支梁无缺口冲击强度 Charpy Unnotch Impact strength 9 |
|||
-30℃ -30℃ |
kJ/m² | ||
23℃ 23℃ |
kJ/m² | ||
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
|||
-30℃ -30℃ |
J/m | ASTM D256 | |
23℃ 23℃ |
J/m | ASTM D256 | |
-30℃ -30℃ 10 |
kJ/m² | ISO 180-1A | |
23℃ 23℃ 10 |
kJ/m² | ISO 180-1A | |
悬臂梁无缺口冲击强度 Notched impact strength of cantilever beam |
|||
-30℃ -30℃ 10 |
kJ/m² | ||
23℃ 23℃ 10 |
kJ/m² | ||
23℃ 23℃ 11 |
kJ/m² | ||
装有测量仪表的落镖冲击 Dart impact equipped with measuring instruments |
|||
23℃,Total Energy 23℃,Total Energy |
J | ASTM D3763 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
1.8 MPa,未退火,3.2 mm 1.8 MPa, unannealed, 3.2 mm |
℃ | ASTM D648 | |
1.8 MPa,未退火,4.0 mm,64 mm跨距 1.8 MPa, unannealed, 4.0 mm, 64 mm span 10 |
℃ | ISO 75-2/Af | |
维卡软化温度 Vicat Softening Temp |
|||
-- -- |
℃ | ASTM D1525 12 | |
B120 B120 |
℃ | ISO 306/B120 | |
球压测试 Ball pressure test |
|||
123~127℃ 123~127℃ |
IEC 60695-10-2 | ||
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
MD:-40~40℃ MD:-40~40℃ |
1/℃ | ASTM E831 | |
MD:-40~40℃ MD:-40~40℃ |
1/℃ | ISO 11359-2 | |
TD:-40~40℃ TD:-40~40℃ |
1/℃ | ASTM E831 | |
TD:-40℃ TD:-40℃ |
1/℃ | ISO 11359-2 | |
相对温度指数 Relative temperature index |
℃ | UL 746 | |
电气性能 Electrical performance |
℃ | UL 746 | |
冲击机械性能 Impact mechanical performance |
℃ | UL 746 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表面电阻率 Surface resistivity |
ohms | IEC 60093 | |
体积电阻率 Volume resistivity |
ohms·cm | IEC 60093 | |
介电强度 Dielectric strength |
|||
3.2 mm,在油中 3.2 mm in oil |
kV/mm | ASTM D149 | |
3.2 mm,在油中 3.2 mm in oil |
kV/mm | IEC 60243-1 | |
介电常数 Dielectric constant |
|||
1 MHz 1 MHz |
ASTM D150 | ||
1 MHz 1 MHz |
IEC 60250 | ||
耗散因数 Dissipation factor |
|||
1 MHz 1 MHz |
ASTM D150 | ||
相比漏电起痕指数 Compared to the leakage tracing index |
UL 746 | ||
高电弧燃烧指数(HAI) High Arc Burning Index (HAI) 13 |
UL 746 | ||
高电压电弧起痕速率 High voltage arc marking rate |
|||
HVTR HVTR |
UL 746 | ||
热丝引燃 Hot wire ignition |
|||
HWI HWI |
UL 746 | ||
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame retardant level |
|||
1.00 mm 1.00 mm |
|||
2.50 mm 2.50 mm |
|||
灼热丝可燃性指数 Glowing wire flammability index |
|||
1.0 mm 1.0 mm |
℃ | IEC 60695-2-12 | |
灼热丝起燃温度 Igniting temperature of the hot wire |
|||
1 mm 1 mm |
℃ | ||
2 mm 2 mm |
℃ | ||
3 mm 3 mm |
℃ |
备注 |
---|
3. 5.0 mm/min |
4. 类型 1, 5.0 mm/min |
5. 1.3 mm/min |
6. 2.0 mm/min |
7. at Yield |
8. at Break |
9. 80*10*4 sp=62mm |
10. 80*10*4 mm |
11. 80*10*3 mm |
12. 速率 A (50°C/h), 载荷2 (50N) |
13. Surface |
【新闻资讯】查看全部
印度阿克苏诺贝尔任命Amit Jain为新董事长
2017-06-21 印度阿克苏诺贝尔宣布任命Amit Jain为新董事长,该决定自8月15日起生效。 公司在一份声明中表示Amit Jain自2009至2013出任总经理一职,他将从Nihal Kaviratne CBE手里接任董事长一职。 声明中还表示,由于还有其他事情要处理,Kaviratne将不会寻求连任,该公司的董事会年度股东大会定于2017年8月14日举行。 Amit Jain有着超过30年的管理经验,横跨亚洲和欧洲。他曾经与与可口可乐公司和维亚康姆公 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |