ACRYLITE® LED White 0V200是专门设计用于均匀的光分布时背光与强大的LED光源。结合高透光性,扩散级还能够消除干扰热点(LED光源产生的光斑)。这些特性使得减少灯罩和光源之间所需的间距成为可能,从而优化组件的壁厚。ACRYLITE® LED White 0V200比其对应物(0V606)的透光率稍高,但仍保持等级的光扩散性质。ACRYLITE® LED White 0V200的特点是光的漫散射,并提供以下丙烯酸聚合物:丙烯酸盐8N,丙烯酸盐H12,丙烯酸盐H15,和丙烯酸盐抗ZKX。丙烯酸酯类聚合物的典型性能有:优良的耐候性、高机械强度、高表面硬度和耐损伤性、各种熔体流动速率。 ACRYLITE® LED White 0V200 is specifically engineered for uniform light distribution when backlit with strong LED light sources. Combined with high light transmission, the diffusion grade also has the ability to eliminate disturbing hotspots (spots of light created by the LED source). These properties make it possible to reduce the spacing required between the cover and the light source, optimizing the wall thickness of the component. ACRYLITE® LED White 0V200 has slightly higher light transmission than its counterpart (0V606), while still retaining the light diffusing nature of the grade. ACRYLITE® LED White 0V200 is characterized by diffuse scattering of light, and is offered in the following ACRYLITE® polymers: ACRYLITE® 8N, ACRYLITE® H12, ACRYLITE® H15, and ACRYLITE® Resist zkX. Typical properties of ACRYLITE® acrylic polymers are: excellent weather resistance high mechanical strength high surface hardness and mar resistance various melt flow rate |
技术参数 Technical Data | |||
---|---|---|---|
光学性能 optical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
透光率 Transmittance 2 |
|||
1000 µm 1000 µm |
73.0 | % | |
2000 µm 2000 µm |
55.0 | % | |
3000 µm 3000 µm |
45.0 | % | |
4000 µm 4000 µm |
38.0 | % | |
Luminance Luminance |
|||
1.00 mm 1.00 mm |
< 114 | cd/m² | |
2.00 mm 2.00 mm |
cd/m² | ||
3.00 mm 3.00 mm |
cd/m² | ||
4.00 mm 4.00 mm |
cd/m² | ||
补充信息 Supplementary information |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
Half-Value Angle Half-Value Angle |
|||
1.00 mm 1.00 mm |
° | ||
2.00 mm 2.00 mm |
° | ||
3.00 mm 3.00 mm |
° | ||
4.00 mm 4.00 mm |
° | ||
散射功率 Scattering power |
|||
1.00 mm 1.00 mm |
|||
2.00 mm 2.00 mm |
|||
3.00 mm 3.00 mm |
|||
4.00 mm 4.00 mm |
备注 |
---|
2、D65 |
【新闻资讯】查看全部
【干货】注塑产品脱模不良怎么办?
2020-12-30 搜料网资讯: 脱模不良,又称黏模流道,是由于注射口与喷嘴圆弧接触面不良,浇口料未同制品一起脱模以及不正常的填料。通常,主流道直径要足够大,使制作脱模时浇口料仍未全部 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |