Kynar Flex 2850 PC粉末涂料是偏氟乙烯和六氟丙烯的半结晶共聚物。KYNA Flex 2850 PC有一个特殊的粒度,使其理想的喷涂金属粉末的耐磨损性和耐腐蚀性。 Kynar Flex® resins are fluorinated thermoplastic copolymers. Kynar Flex® 2850 PC resin powder coating is a semi-crystalline copolymer of vinylidene fluoride and hexafluoropropylene. It has a special particle size making it ideal for spray applied powder coating on metal substrates for abrasion and corrosion protection |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.78 | g/cm³ | ISO 1183 |
熔体体积流动速率 Melt Volume Rate |
|||
230℃,3.8 kg 230℃,3.8 kg |
7.50 | cm³/10min | ISO 1133 |
吸水率 Water absorption rate |
|||
饱和,23℃ Saturation, 23 ℃ |
0.030 | % | ISO 62 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength |
|||
屈服 yield |
35.0 | MPa | ISO 527-2 |
拉伸应变 Tensile strain |
|||
屈服 yield |
10 | % | ISO 527-2 |
标称拉伸断裂应变 Nominal tensile fracture strain |
% | ISO 527-2 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ISO 75-2/A | |
熔融温度 Melting temperature 2 |
℃ | ISO 11357-3 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
体积电阻率 Volume resistivity |
ohms·cm | IEC 60093 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
极限氧指数 Extreme oxygen index |
% | ISO 4589-2 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 65% R.H. |
【新闻资讯】查看全部
再生塑料:进口废料再次推上风口 环保彻查仍在继续
2017-07-06 进口再生塑料在经历过2013年绿篱专项行动、2017年初的国门利剑行动之后,7月1日环保部开展为期1个月的打击进口废物加工利用企业环境违法行为专项行动。环保部有关负责人称,近年来破坏自然保护区违法违规行为频繁发生,习近平 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |