公司信息及水印
牌号简介 About |
---|
MEP52 0074混合工程聚合物颗粒Axplas® MEP52 0074级是一种干净的、洗涤过的、富含聚丙烯的颗粒碎片的混合物,颗粒大小规则。也存在少量的木材和橡胶。请注意,组成图是一个典型的结果,所有材料分数可能会在饼图上显示的数字周围变化百分之几。该产品由100%回收成分制成,具有一系列用户利益,包括:低碳输入可以减少碳足迹。从资源效率中获得环境收益节省原材料应用成本:分离PS和ABS塑料的原料木材制造混合剂或混合塑料的填料。板、片、板产品制造 MEP52 0074 Mixed engineering polymers granules Axplas® MEP52 0074 grade is a mix of clean, washed granular chips rich in PP with regular particle size. Minor quantities of wood and rubber are also present. Please note the composition chart is a typical result and that all material fractions may vary by a few percent around the numbers shown on the pie chart. Produced from 100% recycled content, this product offers a range of user benefits, including: Low carbon input can reduce your carbon footprint Environmental gains from resource efficiency Cost savings on raw material Applications: Feedstock material for separation of PS and ABS Plastics wood manufacture Blending agent or filler for mixed plastics products Manufacture of panels, sheets and boards |
技术参数 Technical Data | |||
---|---|---|---|
暂无数据 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
【新闻资讯】查看全部
注塑机温升过高怎样办?
2017-03-27 注塑机温升过高的原因 1、油箱容积太小,散热面积不够,冷却装置但其容量过小。 2、按快进速度选择油泵容量的定量泵供油系统,在工作时会有大部分多余的流量在高压下从溢流阀溢回而发热。 3、系统中卸荷回路出现故障或因未设置卸荷回路,停止工作时油泵不能卸荷,泵的全部流量在高压下溢流,产生溢流损失而发热,导致温升。 4、系统管路过细过长,弯曲过多,局部压力损失和沿程压力损失大。 5、元件 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |