PP4821是一种基于聚丙烯共聚物的热塑性无卤绝缘化合物。PP4821的成分基于碳和氢元素。因此,基于这些元素的化合物将是该产品燃烧产生的烟气的唯一重要成分。其他元素的浓度可能低于0.1%应用PP4821设计用于:70°C额定绝缘,用于建筑电线(安装电缆)、软线、电力电缆。它可用于对烟雾或腐蚀性和有毒燃烧产物敏感的区域。PP4821稳定用于接触铜。 PP4821 is a thermoplastic, non-halogen containing, insulation compound based on a polypropylene copolymer. The composition of PP4821 is based on the elements Carbon and Hydrogen. Compounds based on these elements will therefore be the only significant constituents of the fumes due to the combustion of this product. Other elements may be present in concentrations less than 0.1% Applications PP4821 is designed for: 70°C rated insulation for building wires (installation cables), flexible cords, power cables It can be used in areas sensitive to smoke or corrosive and toxic combustion products. PP4821 is stabilised for use in contact with copper. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
0.915 | g/cm³ | ISO 1183 |
熔体质量流动速率 Melt Flow Rate |
|||
230℃,2.16kg 230℃,2.16kg |
2.8 | g/10min | ISO 1133 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
|||
15 秒 15 seconds |
48 | ISO 868 | |
拉伸强度 tensile strength 2 |
18.0 | MPa | IEC 60811-1-1 |
拉伸应变 Tensile strain |
|||
断裂 fracture |
600 | % | IEC 60811-1-1 |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
低温弯曲 Low temperature bending |
|||
-20℃ -20℃ |
IEC 60811-1-4 | ||
老化性能 Aging performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
Change in Tensile Stress(120℃,336 hr) Change in Tensile Stress(120℃,336 hr) |
% | IEC 60754-1 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
体积电阻率 Volume resistivity |
ohms·cm | IEC 60093 | |
介电强度 Dielectric strength |
kV/mm | IEC 60243-1 | |
介电常数 Dielectric constant |
|||
50 Hz 50 Hz |
IEC 60250 | ||
补充信息 Supplementary information |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
Bottle Mean Failure Height Bottle Mean Failure Height |
IEC 60227-2/2.3 | ||
击穿电压 breakdown voltage |
V | ISO 6722 | |
锥形量热试验 Cone calorimetry test |
ISO 5660 | ||
平均热释放速率 Average heat release rate 3 |
kW/m² | ISO 5660 | |
CO CO 3 |
g/cm³ | ISO 5660 | |
CO2 CO2 |
g/cm³ | ISO 5660 | |
燃烧热 Combustion heat 4 |
ISO 5660 | ||
点燃时间 Ignition time 3 |
min | ISO 5660 | |
最大热释放速率 Maximum heat release rate 3 |
kW/m² | ISO 5660 | |
Smoke Obscuration Smoke Obscuration 5 |
ISO 5660 | ||
热压测试 Hot pressing test 6 |
|||
120℃ 120℃ 6 |
% | IEC 60811-3-1 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 2.0 in/min |
3 Heat flus 35 kW/m², 3 mm plaque |
4 Heat flus 35 kW/m², 3 mm plaque, Mj/dm3 |
5 Heat flus 35 kW/m², 3 mm plaque, m2/dm3 |
6 at High Temperatureat 4 hours. Cable (0.5 mm insulation over 1.5 mm² solid Cu) |
【新闻资讯】查看全部
浙江首个出口模具质量平安示范区经过考核验收
2017-12-25 近日,宁波市宁海县出口模具质量安全示范区顺利通过宁波检验检疫局专家组的考核验收,成为浙江省首个出口模具质量安全示范区。这是继2016年成功创建省级出口文具示范区后,又一省级出口示范区落户宁海。 宁海县是全国综合实力百强县,模具产业高度集聚,享有“中国模具产业基地”称号,现拥有模具企业500多家,规模以上企业44家,出现了如方正、震裕、双林等较大规模的龙头企业,其中双林集团荣获“中国驰名商标”,从业人员5万多人,生产的大型塑料模、冲压模、橡胶模和压铸模等综合水平国内领先,部分 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |