牌号简介 About |
---|
型号:Estane® 58863 TPU是85A聚醚型热塑性聚氨酯。特点:具有良好的弹性-高熔体流动性,便于加工使用:挤出-电线和电缆,一般挤出 Type: Estane® 58863 TPU is an 85A Polyether-Type Thermoplastic Polyurethane. Features: Good Elasticity - High melt flow for easy processing Uses: Extrusion - Wire and cable, general extrusion |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.12 | g/cm³ | ASTM D792 |
弹性体 elastic body |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength |
ASTM D412 | ||
断裂,0.762 mm Fracture, 0.762 mm |
40.7 | MPa | ASTM D412 |
100% 应变,0.762 mm 100% strain, 0.762 mm |
6.90 | MPa | ASTM D412 |
300% 应变,0.762 mm 300% strain, 0.762 mm |
11.0 | MPa | ASTM D412 |
拉伸应变 Tensile strain |
|||
断裂,0.762 mm Fracture, 0.762 mm |
600 | % | ASTM D412 |
撕裂强度 tear strength |
|||
0.762 mm 0.762 mm 1 |
kN/m | ASTM D624 | |
开裂 cracking |
kN/m | ASTM D470 | |
压缩形变 Compression deformation |
ASTM D395 | ||
23℃,22 hr 23℃,22 hr |
% | ASTM D395 | |
70℃,22 hr 70℃,22 hr |
% | ASTM D395 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
玻璃化转变温度 Glass transition temperature |
℃ | DSC | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
|||
邵氏 A,5 秒 Shore A, 5 seconds |
ASTM D2240 | ||
弯曲模量 Bending modulus |
|||
23℃ 23℃ |
MPa | ASTM D790 | |
泰伯耐磨性 Taber abraser |
|||
1000 周期,1000 g,CS-17 转轮 1000 cycles, 1000 g, CS-17 wheels |
mg | ASTM D3389 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 C 模具 |
【新闻资讯】查看全部
印度阿克苏诺贝尔任命Amit Jain为新董事长
2017-06-21 印度阿克苏诺贝尔宣布任命Amit Jain为新董事长,该决定自8月15日起生效。 公司在一份声明中表示Amit Jain自2009至2013出任总经理一职,他将从Nihal Kaviratne CBE手里接任董事长一职。 声明中还表示,由于还有其他事情要处理,Kaviratne将不会寻求连任,该公司的董事会年度股东大会定于2017年8月14日举行。 Amit Jain有着超过30年的管理经验,横跨亚洲和欧洲。他曾经与与可口可乐公司和维亚康姆公 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |