Pocan B 4235 Z 000000 PBT,30%玻璃纤维,注塑,阻燃,提高冲击强度 POCAN® B4235Z 000000 PBT, 30 % glass fibers, injection molding, flame retardant, improved impact strength POCAN® B4235Z 000000 PBT, 30 % glass fibers, injection molding, flame retardant, improved impact strength POCAN® B4235Z 000000 PBT, 30 % glass fibers, injection molding, flame retardant, improved impact strength |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.62 | g/cm³ | ISO 1183 |
表观密度 Apparent density |
0.80 | g/cm³ | ISO 60 |
熔体体积流动速率 Melt Volume Rate |
|||
260℃,5 kg 260℃,5 kg |
26.0 | cm³/10min | ISO 1133 |
收缩率 Shrinkage rate |
ISO 294-4 | ||
TD:250℃,2.0 mm TD:250℃,2.0 mm |
0.90 | % | ISO 294-4 |
TD:120℃,2.0 mm,2 hrs TD:120℃,2.0 mm,2 hrs |
0.10 | % | ISO 294-4 |
MD:250℃,2.0 mm MD:250℃,2.0 mm |
% | ISO 294-4 | |
MD:120℃,2.0 mm,2 hrs MD:120℃,2.0 mm,2 hrs |
% | ISO 294-4 | |
吸水率 Water absorption rate |
ISO 62 | ||
饱和,23℃ Saturation, 23 ℃ |
% | ISO 62 | |
平衡,23℃,50% RH Equilibrium, 23 ℃, 50% RH |
% | ISO 62 | |
粘度值 Viscosity value |
|||
降低的粘度 Reduced viscosity |
ml/g | ISO 1628 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength |
ISO 179/1eA | ||
-30℃ -30℃ |
kJ/m² | ISO 179/1eA | |
23℃ 23℃ |
kJ/m² | ISO 179/1eA | |
简支梁无缺口冲击强度 Charpy Unnotch Impact strength |
ISO 179/1eU | ||
-30℃ -30℃ |
kJ/m² | ISO 179/1eU | |
23℃ 23℃ |
kJ/m² | ISO 179/1eU | |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
ISO 180/1A | ||
-40℃ -40℃ |
kJ/m² | ISO 180-1A | |
-30℃ -30℃ |
kJ/m² | ISO 180-1A | |
23℃ 23℃ |
kJ/m² | ISO 180-1A | |
悬臂梁无缺口冲击强度 Notched impact strength of cantilever beam |
ISO 180/1U | ||
-30℃ -30℃ |
kJ/m² | ISO 180/1U | |
23℃ 23℃ |
kJ/m² | ISO 180/1U | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
0.45 MPa,未退火 0.45 MPa, unannealed |
℃ | ISO 75-2/B | |
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ISO 75-2/A | |
8.0 MPa,未退火 8.0 MPa, unannealed |
℃ | ISO 75-2/C | |
维卡软化温度 Vicat Softening Temp |
|||
B120 B120 |
℃ | ISO 306/B120 | |
球压测试 Ball pressure test |
|||
210℃ 210℃ |
IEC 60695-10-2 | ||
熔融温度 Melting temperature |
℃ | ISO 11357-3 | |
线性热膨胀系数 Linear coefficient of thermal expansion |
ISO 11359-2 | ||
MD:23~55℃ MD:23~55℃ |
1/℃ | ISO 11359-2 | |
TD:23~55℃ TD:23~55℃ |
1/℃ | ISO 11359-2 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
相比漏电起痕指数 Compared to the leakage tracing index |
|||
解决方案 A Solution A |
V | IEC 60112 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame retardant level |
UL 94 | ||
0.75 mm 0.75 mm |
UL 94 | ||
1.50 mm 1.50 mm |
UL 94 | ||
3.00 mm 3.00 mm |
UL 94 | ||
灼热丝可燃性指数 Glowing wire flammability index |
|||
2.0 mm 2.0 mm |
℃ | IEC 60695-2-12 | |
补充信息 Supplementary information |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
ISO Shortname ISO Shortname |
ISO 7792 | ||
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
球压硬度 Ball hardness |
MPa | ISO 2039-1 | |
拉伸模量 Tensile modulus |
|||
23℃ 23℃ |
MPa | ISO 527-1-2 | |
拉伸强度 tensile strength |
|||
断裂,23℃ Fracture, 23 ℃ |
MPa | ISO 527-2/5 | |
拉伸应变 Tensile strain |
|||
断裂,23℃ Fracture, 23 ℃ |
% | ISO 527-2/5 | |
弯曲模量 Bending modulus |
|||
23℃ 23℃ |
MPa | ISO 178-A | |
弯曲强度 bending strength |
|||
23℃ 23℃ |
MPa | ISO 178 | |
弯曲应变 Bending strain |
% |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 60x60x2mm, 80°C MT, 600 bar |
3 60x60x2; WZ 80°C; 600 Bar |
4 60x60x2 |
5 60x60x2mm |
6 0.079 in/min |
7 2 mm/min |
8 Pull Rate: 2 mm/min; 50% RH |
9 10°C/min |
【新闻资讯】查看全部
速度与力量兼备!拓斯达推出MBW-130Pro高速牛头机械手
2022-03-28 随着塑料加工行业在我国的迅速发展,注塑成型设备的自动化程度也越来越高。现代化的注塑机常配置有注塑机械手,以提高生产效率。注塑机械手是为注塑生产自动化专门配备的机械 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |