Valox 310SE0树脂Valox 310SE0是一种无增强、阻燃的PBT注塑树脂。应用:电器行业、线轴、键盘、开关元件及电器外壳。 VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.40 | g/cm³ | ASTM D792 |
特定体积 Specific volume |
0.710 | cm³/g | ASTM D792 |
密度 Density |
1.40 | g/cm³ | ISO 1183 |
熔体质量流动速率 Melt Flow Rate |
|||
250℃,2.16kg 250℃,2.16kg |
8.6 | g/10min | ASTM D1238 |
熔体体积流动速率 Melt Volume Rate |
|||
250℃,2.16 kg 250℃,2.16 kg |
8.00 | cm³/10min | ISO 1133 |
收缩率 Shrinkage rate |
Internal Method | ||
MD MD 2 |
% | 内部方法 | |
MD MD 3 |
% | 内部方法 | |
MD MD 4 |
% | 内部方法 | |
MD:3.2 mm MD:3.2 mm |
% | 内部方法 | |
吸水率 Water absorption rate |
|||
饱和,23℃ Saturation, 23 ℃ |
% | ISO 62 | |
平衡,23℃,50% RH Equilibrium, 23 ℃, 50% RH |
% | ISO 62 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength |
|||
-30℃ -30℃ 10 |
kJ/m² | ISO 179/1eA | |
23℃ 23℃ 10 |
kJ/m² | ISO 179/1eA | |
23℃ 23℃ |
kJ/m² | ISO 179/2C | |
简支梁无缺口冲击强度 Charpy Unnotch Impact strength 10 |
ISO 179/1eU | ||
-30℃ -30℃ |
ISO 179/1eU | ||
23℃ 23℃ |
ISO 179/1eU | ||
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
ASTM D256 | ||
-30℃ -30℃ |
J/m | ASTM D256 | |
23℃ 23℃ |
J/m | ASTM D256 | |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch 11 |
ISO 180/1A | ||
23℃ 23℃ |
J/m | ASTM D4812 | |
-30℃ -30℃ |
kJ/m² | ISO 180-1A | |
23℃ 23℃ |
kJ/m² | ISO 180-1A | |
悬臂梁无缺口冲击强度 Notched impact strength of cantilever beam 11 |
ISO 180/1U | ||
-30℃ -30℃ |
ISO 180/1U | ||
23℃ 23℃ |
ISO 180/1U | ||
装有测量仪表的落镖冲击 Dart impact equipped with measuring instruments |
|||
23℃,Total Energy 23℃,Total Energy |
J | ASTM D3763 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
ASTM D648 | ||
0.45 MPa,未退火,6.4 mm 0.45 MPa, unannealed, 6.4 mm |
℃ | ASTM D648 | |
0.45 MPa,未退火,100 mm跨距 0.45 MPa, unannealed, 100 mm span 12 |
℃ | ISO 75-2/Be | |
1.8 MPa,未退火,3.2 mm 1.8 MPa, unannealed, 3.2 mm |
℃ | ASTM D648 | |
1.8 MPa,未退火,6.4 mm 1.8 MPa, unannealed, 6.4 mm |
℃ | ASTM D648 | |
热变形温度 Hot deformation temperature |
|||
1.8 MPa,未退火,100 mm跨距 1.8 MPa, unannealed, 100 mm span 12 |
℃ | ISO 75-2/Ae | |
1.8 MPa,未退火,64 mm跨距 1.8 MPa, unannealed, 64 mm span 13 |
℃ | ISO 75-2/Af | |
维卡软化温度 Vicat Softening Temp |
℃ | ASTM D1525 14 | |
维卡软化温度 Vicat Softening Temp |
|||
A50 A50 |
℃ | ISO 306/A50 | |
B50 B50 |
℃ | ISO 306 | |
B120 B120 |
℃ | ISO 306/B120 | |
球压测试 Ball pressure test |
|||
125℃ 125℃ |
IEC 60695-10-2 | ||
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
TD:-40~40℃ TD:-40~40℃ |
1/℃ | ASTM E831 | |
TD TD |
ISO 11359-2 | ||
-40 到 40℃ -40 to 40 ℃ |
cm/cm/℃ | ISO 11359-2 | |
MD MD |
ASTM E831 | ||
-40 到 40℃ -40 to 40 ℃ |
cm/cm/℃ | ASTM E831 | |
60 到 138℃ 60 to 138 ℃ |
cm/cm/℃ | ASTM E831 | |
MD MD |
ISO 11359-2 | ||
-40 到 40℃ -40 to 40 ℃ |
cm/cm/℃ | ISO 11359-2 | |
23 到 60℃ 23 to 60 ℃ |
cm/cm/℃ | ISO 11359-2 | |
导热系数 Thermal conductivity coefficient |
W/m/K | ISO 8302 | |
相对温度指数 Relative temperature index |
|||
电气性能 Electrical performance |
℃ | UL 746 | |
强度机械性能 Strength mechanical performance |
℃ | UL 746 | |
冲击机械性能 Impact mechanical performance |
℃ | UL 746 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表面电阻率 Surface resistivity |
ohms | IEC 60093 | |
体积电阻率 Volume resistivity |
ohms·cm | IEC 60093 | |
介电强度 Dielectric strength |
ASTM D149 | ||
1.6 mm,在油中 1.6 mm in oil |
kV/mm | ASTM D149 | |
3.2 mm,在空气中 3.2 mm in air |
kV/mm | ASTM D149 | |
介电强度 Dielectric strength |
IEC 60243-1 | ||
0.8 mm,在油中 0.8 mm in oil |
kV/mm | IEC 60243-1 | |
1 mm 1 mm 15 |
kV/mm | IEC 60243-1 | |
1.6 mm,在油中 1.6 mm in oil |
kV/mm | IEC 60243-1 | |
3.2 mm,在油中 3.2 mm in oil |
kV/mm | IEC 60243-1 | |
相对电容率 Relative permittivity |
IEC 60250 | ||
50 Hz 50 Hz |
IEC 60250 | ||
60 Hz 60 Hz |
IEC 60250 | ||
100 Hz 100 Hz |
IEC 60250 | ||
1 MHz 1 MHz |
IEC 60250 | ||
耗散因数 Dissipation factor |
IEC 60250 | ||
50 Hz 50 Hz |
IEC 60250 | ||
60 Hz 60 Hz |
IEC 60250 | ||
100 Hz 100 Hz |
IEC 60250 | ||
1 MHz 1 MHz |
IEC 60250 | ||
耐电弧性 Arc resistance 16 |
ASTM D495 | ||
相比漏电起痕指数 Compared to the leakage tracing index |
UL 746 | ||
相比漏电起痕指数 Compared to the leakage tracing index |
IEC 60112 | ||
CTI CTI |
V | IEC 60112 | |
解决方案 B Solution B |
V | IEC 60112 | |
高电弧燃烧指数(HAI) High Arc Burning Index (HAI) |
UL 746 | ||
高压电弧抗点燃指数(HVAR)(PLC) High voltage arc ignition resistance index (HVAR) (PLC) |
UL 746 | ||
高电压电弧起痕速率 High voltage arc marking rate |
|||
HVTR HVTR |
UL 746 | ||
热丝引燃 Hot wire ignition |
|||
HWI HWI |
UL 746 | ||
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame retardant level |
UL 94 | ||
0.71 mm 0.71 mm |
UL 94 | ||
3.00 mm 3.00 mm |
UL 94 | ||
灼热丝可燃性指数 Glowing wire flammability index |
|||
1.0 mm 1.0 mm |
℃ | IEC 60695-2-12 | |
极限氧指数 Extreme oxygen index |
% | ISO 4589-2 | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus 5 |
MPa | ASTM D638 | |
拉伸模量 Tensile modulus |
MPa | ISO 527-1-2 | |
拉伸强度 tensile strength |
|||
断裂 fracture |
MPa | ISO 527-2/50 | |
断裂 fracture 6 |
MPa | ASTM D638 | |
屈服 yield 6 |
MPa | ASTM D638 | |
屈服 yield |
MPa | ISO 527-2/50 | |
拉伸应变 Tensile strain |
|||
断裂 fracture 6 |
% | ASTM D638 | |
断裂 fracture |
% | ISO 527-2/50 | |
屈服 yield 6 |
% | ASTM D638 | |
屈服 yield |
% | ISO 527-2/50 | |
弯曲模量 Bending modulus 8 |
MPa | ISO 178 | |
50 mm跨距 50 mm span 7 |
MPa | ASTM D790 | |
弯曲强度 bending strength 8 , 9 |
MPa | ISO 178 | |
弯曲强度 bending strength 7 |
|||
屈服,50 mm跨度 Yield, 50 mm span 7 |
MPa | ASTM D790 | |
泰伯耐磨性 Taber abraser |
|||
1000 周期,1000 g,CS-17 转轮 1000 cycles, 1000 g, CS-17 wheels |
mg | 内部方法 | |
洛氏硬度 Rockwell hardness |
|||
R 级 R-level |
ISO 2039-2 | ||
球压硬度 Ball hardness |
|||
H358/30 H358/30 |
MPa | ISO 2039-1 | |
特殊值 Special value |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
TD TD 2 |
% | 内部方法 | |
TD TD 4 |
% | 内部方法 | |
TD TD 3 |
% | 内部方法 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 Tensile Bar |
3 0.75 to 2.3 mm |
4 2.3 to 4.6 mm |
5 0.20 in/min |
6 类型 1, 2.0 in/min |
7 0.051 in/min |
8 0.079 in/min |
9 Yield |
10 80*10*4 sp=62mm |
11 80*10*4 |
12 120*10*4 mm |
13 80*10*4 mm |
14 标准 B (120°C/h), 载荷2 (50N) |
15 速率 A (50°C/h), 载荷2 (50N) |
16 Short-Time |
17 钨电极 |
【新闻资讯】查看全部
注塑模具检修时最容易无视的中央有哪些?
2018-04-13 每个注塑成型位置所需的维修程序取决于不同的模具循环周期。下面是一些通用原则可以让每个模具使用者用来保证热流道、加热器、导柱和顶针等模具组件的有效运行,以防意外情况的出现。 |
注塑模具检修时最容易无视的中央有哪些? 每一个注塑工艺部位需要的检修程序流程在于不一样的模具循环系统周期时间。下边是一些通用性标准能够让每一个模具使用人用于确保热流道系统、加热器、定位销和顶针等模具部件的合理运作,防止出现意外状况的出現。
1、您在查询散出气孔处是不是有预警信息性的锈蚀或湿冷现象�C假如您在热流道系统排出气孔周边发觉有锈蚀或湿冷现象,那么就代表着內部冷疑或者有可能自来水管裂开了。湿冷现象会引起对加热器致命性的短路故障。假如设备并不是全年度难休地运作,只是在晚上或者礼拜天会待机得话,产生这类凝固现象的概率便会提升。 2、还记得提示操作工不必把进胶口处的热嘴头“清除”掉�C如果操作工恰巧见到模具水部位上有一小片不锈钢板,那有可能实际上是个点水部位部件。“清除”掉这看起来是阻拦的物品经常会摧毁热嘴头。为了更好地不会毁坏热嘴,请在付诸行动前确定下热流道系统的嘴头种类,保证全部操作工都经过训练而且能鉴别自身所触碰全部不一样种类的嘴头。 3、滑跑止扣�C针对全年度难休运作的设备,此项工作中理应每星期开展一次。 4、互动校检加热器的电阻值�C您应当在一开始应用加热器的情况下就早已精确测量过它的电阻值,如今便是情况下再度精确测量并开展比照了。假如电阻值有左右10%的波动,就该考虑到更换加热器以确保它不容易在加工过程中的紧要关头出情况。要是以沒有精确测量过最开始的电阻值,那如今就精确测量一次并将个人所得的标值用作将来查验该加热器时的参照数据信息。
5、查询定位销和导套间是不是有损坏的征兆 �C 寻找是不是有刮�p或擦�p等印痕,这类损坏是因为欠缺润化的关联。假如印痕仅仅刚出現,那麼您还能够根据给定位销和导柱加多润化来增加其使用寿命。倘若损坏已很严重,那便是情况下拆换新零件了。不然得话,凹模和型芯一部分很有可能没法非常好地紧密结合,造成 零部件壁内厚薄不一。 6、查验流水状况�C在水道出入口联接一条塑料软管,让水根据自来水管留在桶里。假如排出的水不清亮或者颜色就很有可能有锈蚀现象产生,而流水不顺畅就代表着某点阻塞。假如发觉这种难题就将全部自来水管再度钻穿,确保通畅 (或者采用您最常见的一切方式开展清除)。改善加工厂的水处理装置可以避免 将来再出現由锈蚀和堵塞而引起的各种各样难题。 7、清理顶针�C历经一年的時间,顶针会因为汽体推积和薄膜状残渣而越来越好脏。振业注塑加工强烈推荐每过六到十二个月用模具清洁剂好好清理一番。清理整洁之后,在顶针上涂上一层润滑液避免 擦破或破裂。 8、查询热灌嘴的半经地区是不是有断裂面 �C 断裂面是由残余在设备热口中的疏松的发硬的塑料残片在往前注塑加工时从注塑料筒部件产生的夹紧力所导致的。难题的诱因也是有可能是轴线沒有指向。在发觉断裂面时要考虑到这二种概率。假如受到的毁坏已比较严重到不可以避免出现花朵状泄露(模具使用人过去应用的一个专业术语:指在导柱和设备的热嘴头间出現的塑料泄露),就应更换进胶口套。 来源于:振业注塑加工汇 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |