Lexan Lux7432c树脂Lexan Lux7432c聚碳酸酯(PC)树脂是一种非填充、注射成型级树脂。这种非氯化、非溴化阻燃PC的UL-94V0额定值为1.2 mm/5VA额定值为3.0 mm,并且紫外线稳定(F1额定值)提供了额外的耐候性。Lexan Lux7432C提供扩散色。 LEXAN LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm and is UV stabilized(F1 rating) providing additional weathering capability. LEXAN LUX7432C is available in diffusion colors. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.19 | g/cm³ | ASTM D792 |
密度 Density |
1.20 | g/cm³ | ISO 1183 |
熔体质量流动速率 Melt Flow Rate |
|||
300℃,1.20kg 300℃,1.20kg |
10 | g/10min | ASTM D1238 |
熔体体积流动速率 Melt Volume Rate |
|||
300℃,1.2 kg 300℃,1.2 kg |
9.00 | cm³/10min | ISO 1133 |
收缩率 Shrinkage rate |
|||
TD:3.2 mm TD:3.2 mm |
0.60 to 0.80 | % | 内部方法 |
MD:3.2 mm MD:3.2 mm |
% | 内部方法 | |
吸水率 Water absorption rate |
|||
饱和,23℃ Saturation, 23 ℃ |
% | ISO 62 | |
平衡,23℃,50% RH Equilibrium, 23 ℃, 50% RH |
% | ISO 62 | |
耐候性 Weathering resistance |
UL 746C | ||
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus 2 |
MPa | ASTM D638 | |
拉伸模量 Tensile modulus |
MPa | ISO 527-1-2 | |
拉伸强度 tensile strength 3 |
|||
断裂 fracture |
MPa | ISO 527-2/50 | |
断裂 fracture 3 |
MPa | ASTM D638 | |
屈服 yield |
MPa | ISO 527-2/50 | |
屈服 yield 3 |
MPa | ASTM D638 | |
拉伸应变 Tensile strain |
|||
断裂 fracture 4 |
% | ASTM D638 | |
断裂 fracture |
% | ISO 527-2/50 | |
屈服 yield 3 |
% | ASTM D638 | |
屈服 yield |
% | ISO 527-2/50 | |
弯曲模量 Bending modulus 5 |
MPa | ISO 178 | |
50 mm跨距 50 mm span 4 |
MPa | ASTM D790 | |
弯曲强度 bending strength 5 , 6 |
MPa | ISO 178 | |
弯曲强度 bending strength 4 |
|||
屈服,50 mm跨度 Yield, 50 mm span 4 |
MPa | ASTM D790 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength 7 |
ISO 179/1eA | ||
-30℃ -30℃ |
kJ/m² | ISO 179/1eA | |
23℃ 23℃ |
kJ/m² | ISO 179/1eA | |
简支梁无缺口冲击强度 Charpy Unnotch Impact strength 7 |
ISO 179/1eU | ||
-30℃ -30℃ |
ISO 179/1eU | ||
23℃ 23℃ |
ISO 179/1eU | ||
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
ASTM D256 | ||
-30℃ -30℃ |
J/m | ASTM D256 | |
23℃ 23℃ |
J/m | ASTM D256 | |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch 8 |
ISO 180/1A | ||
-30℃ -30℃ |
kJ/m² | ISO 180-1A | |
23℃ 23℃ |
kJ/m² | ISO 180-1A | |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
ASTM D4812 | ||
-30℃ -30℃ |
ASTM D4812 | ||
23℃ 23℃ |
ASTM D4812 | ||
悬臂梁无缺口冲击强度 Notched impact strength of cantilever beam 8 |
ISO 180/1U | ||
-30℃ -30℃ |
ISO 180/1U | ||
23℃ 23℃ |
ISO 180/1U | ||
装有测量仪表的落镖冲击 Dart impact equipped with measuring instruments |
|||
23℃,Total Energy 23℃,Total Energy |
J | ASTM D3763 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature 9 |
|||
1.8 MPa,未退火,3.2 mm 1.8 MPa, unannealed, 3.2 mm |
℃ | ASTM D648 | |
1.8 MPa,未退火,100 mm跨距 1.8 MPa, unannealed, 100 mm span 9 |
℃ | ISO 75-2/Ae | |
0.45 MPa,未退火,3.2 mm 0.45 MPa, unannealed, 3.2 mm |
℃ | ASTM D648 | |
0.45 MPa,未退火,100 mm跨距 0.45 MPa, unannealed, 100 mm span 9 |
℃ | ISO 75-2/Be | |
维卡软化温度 Vicat Softening Temp |
℃ | ASTM D1525 10 | |
维卡软化温度 Vicat Softening Temp |
|||
B50 B50 |
℃ | ISO 306 | |
B120 B120 |
℃ | ISO 306/B120 | |
球压测试 Ball pressure test |
|||
125℃ 125℃ |
IEC 60695-10-2 | ||
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
TD:23~80℃ TD:23~80℃ |
1/℃ | ISO 11359-2 | |
TD:-40~40℃ TD:-40~40℃ |
1/℃ | ASTM E831 | |
MD:23~80℃ MD:23~80℃ |
1/℃ | ISO 11359-2 | |
MD:-40~40℃ MD:-40~40℃ |
1/℃ | ASTM E831 | |
相对温度指数 Relative temperature index |
|||
电气性能 Electrical performance |
℃ | UL 746 | |
强度机械性能 Strength mechanical performance |
℃ | UL 746 | |
冲击机械性能 Impact mechanical performance |
℃ | UL 746 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
介电常数 Dielectric constant |
|||
1.10 GHz 1.10 GHz |
ASTM ES7-83 | ||
耗散因数 Dissipation factor |
|||
1.1 GHz 1.1 GHz |
ASTM ES7-83 | ||
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame retardant level |
UL 94 | ||
0.40 mm 0.40 mm |
UL 94 | ||
1.00 mm 1.00 mm |
UL 94 | ||
1.20 mm 1.20 mm |
UL 94 | ||
3.00 mm 3.00 mm |
UL 94 | ||
灼热丝可燃性指数 Glowing wire flammability index |
|||
1.2 mm 1.2 mm |
℃ | IEC 60695-2-12 | |
灼热丝起燃温度 Igniting temperature of the hot wire |
|||
1.2 mm 1.2 mm |
℃ | IEC 60695-2-13 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 2.0 in/min |
3 类型 1, 2.0 in/min |
4 0.051 in/min |
5 0.079 in/min |
6 Yield |
7 80*10*3 sp=62mm |
8 80*10*3 |
9 120*10*4 mm |
10 标准 B (120°C/h), 载荷2 (50N) |
【新闻资讯】查看全部
朗盛扩大阻燃塑料的范围,用于家用电器设计
2021-09-23 搜料网资讯: ●朗盛扩大了其阻燃塑料的范围 ● 通过VDE认证的材料在终端产品上进行灼热丝测试 ● 高阻燃性能为部件设计提供更大的自由度 ● 有可能适用于电动汽车 根据纽伦堡消费 |
朗盛扩大阻燃塑料的范围,用于家用电器设计 搜料网资讯:● 朗盛扩大了其阻燃塑料的范围 ● 通过VDE认证的材料在终端产品上进行灼热丝测试 ● 高阻燃性能为部件设计提供更大的自由度 ● 有可能适用于电动汽车
根据纽伦堡消费者研究协会(GfK)进行的一项研究,尽管发生了冠状病毒大流行,但2020年技术性消费品的销售额仍有所增长。对家用电器的需求也仍然强劲,因为许多消费者越来越多地投资于自己的家。其结果是对符合国际防火标准IEC/EN 60335-1的阻燃塑料的需求不断增加,用作洗碗机等无人看管的家用电器部件。作为回应,朗盛正在扩大其阻燃化合物的范围,包括在根据该标准进行的灼热丝测试中提供高度阻燃的改性材料。 该系列的最新产品是无卤素阻燃剂Durethan BKV30FN34,主要针对那些出于安全考虑,倾向于按照家用电器标准的严格条件和要求对终端产品进行灼热丝测试的用户(灼热丝终端产品测试,IEC 60695-2-1)。高性能材料(HPM)业务部门的阻燃塑料专家Alexander Radeck说:“这种聚酰胺6化合物由于其高度的阻燃性,提供了巨大的安全储备。这为部件的几何设计提供了更大的自由。” 高抗爬电能力和断裂伸长率 这种新型聚酰胺6的耐灼热丝性已经得到VDE Pruef- und Zertifizierungsinstitut GmbH(德国电气工程、电子和信息技术协会)的认证,壁厚在0.4至3.0毫米之间的GWIT值为775℃(灼热丝点燃温度,IEC 60695-2-13)。这种材料的另一个优点是其600V的高漏电起痕指数(CTI A,相对漏电起痕指数,IEC 60112),这减少了由爬电电流引起的短路和缺陷的风险。这使设计者能够使电气和电子模块更加紧凑,进而减少最终产品的尺寸。这种塑料由30%的短玻璃纤维加固,还具有很高的断裂伸长率。Radeck说:“这意味着,例如,出于视觉原因而稍厚的扣合件不会在啮合前变形和断裂。” 另一种PBT化合物具有出色的抗灼热丝能力 另一种为最终产品的灼热丝测试而设计的化合物是Pocan TFN4230。这种PBT+PET(聚丁烯/聚对苯二甲酸乙二醇酯)混合物已经被用于一系列的系列应用中,并通过了VDE认证,其GWIT值为775℃(0.4至3.0毫米)。该材料不仅具有较高的抗跟踪能力,而且具有出色的尺寸稳定性。 在汽车电池充电系统中的应用潜力 Radeck说:“我们希望看到这两种化合物被用于洗衣机、滚筒式烘干机和洗碗机等电器的外壳、微动开关和连接器。但是,我们也看到了电动汽车的一系列电气和电子元件中令人兴奋的潜力--特别是在电池充电系统中。” |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |
抱歉!该牌号暂无认证数据。
价格走势图
抱歉!该牌号暂无认证数据。
抱歉!暂无数据。
抱歉!暂无数据。