柔性,紫外线稳定,无卤挤压等级,适用于电线绝缘和电缆护套。根据ASTM D4459,紫外线老化后具有良好的颜色稳定性。浅色可选。阻燃性能满足UL VW-1要求。根据UL 1581的规定,80C应用温度等级和良好的热变形性能。82肖氏A硬度。通常在标准挤压设备上进行的加工。使用0.12 mm x 20绞合铜导线在2.0 mm电线上进行的UL 1581试验。 Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame retardant performance capable of meeting UL VW-1 requirement. 80C application temperature rating and good heat deformation performance as defined by UL 1581. 82 Shore A hardness. Processing typically conducted on standard extrusion equipment. UL 1581 tests conducted on 2.0 mm wire with 0.12 mm x 20 stranded copper conductor. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.09 到 1.17 | g/cm³ | ASTM D792 |
熔体质量流动速率 Melt Flow Rate |
|||
250℃,5.0kg 250℃,5.0kg |
20 | g/10min | ASTM D1238 |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
脆化温度 Embrittlement temperature |
< -40.0 | ℃ | ASTM D746 |
UL温度额定值 UL temperature rating |
80 | ℃ | UL 1581 |
Heat Deformation(100℃) Heat Deformation(100℃) 6 |
15 | % | UL 1581 |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
体积电阻率 Volume resistivity |
ohms·cm | ASTM D257 | |
介电强度 Dielectric strength |
|||
2 mm,在油中 2 mm in oil |
kV/mm | IEC 60243-1 | |
介电常数 Dielectric constant |
|||
1 MHz 1 MHz |
ASTM D150 | ||
耗散因数 Dissipation factor |
|||
1 MHz 1 MHz |
ASTM D150 | ||
相比漏电起痕指数 Compared to the leakage tracing index |
V | IEC 60112 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
灼热丝可燃性指数 Glowing wire flammability index |
|||
3.0 mm 3.0 mm |
℃ | IEC 60695-2-12 | |
灼热丝起燃温度 Igniting temperature of the hot wire |
|||
3 mm 3 mm |
℃ | IEC 60695-2-13 | |
极限氧指数 Extreme oxygen index |
% | ISO 4589-2 | |
VW-1 VW-1 |
UL 1581 | ||
烟雾密度 Smoke density |
ASTM E662 | ||
Flame,0.5 mm plaque,Ds,max Flame,0.5 mm plaque,Ds,max |
|||
Non-Flame,0.5 mm plaque,Ds,max Non-Flame,0.5 mm plaque,Ds,max |
|||
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
|||
邵氏 A,30 秒 Shore A, 30 seconds |
ASTM D2240 | ||
拉伸强度 tensile strength |
|||
断裂 fracture |
MPa | UL 1581 | |
断裂 fracture 1 |
MPa | ASTM D638 | |
断裂,113℃ Fracture, 113 ℃ 2 |
MPa | UL 1581 | |
断裂 fracture |
MPa | ISO 527-2/50 | |
拉伸应变 Tensile strain |
|||
断裂 fracture |
% | UL 1581 | |
断裂 fracture 3 |
% | ASTM D638 | |
断裂,113℃ Fracture, 113 ℃ 4 |
% | UL 1581 | |
断裂 fracture |
% | ISO 527-2/50 | |
弯曲模量 Bending modulus 5 |
|||
100 mm跨距 100 mm span |
MPa | ASTM D790 | |
-- -- |
MPa | ISO 178 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 类型 1, 2.0 in/min |
3 After 7 days |
4 0.49 in/min |
5 250 g |
【新闻资讯】查看全部
“启新程,创未来”,诺力昂天津南港机过氧化物生产基地全面建成
2022-11-30 扫描上图二维码,可以免费下载 搜料 APP 11月23日,随着诺力昂天津南港的世界级创新型有机过氧化物生产基地的全面建成,天津诺力昂过氧化物有限公司南港新工厂正式开业。 据搜料 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |