牌号简介 About |
---|
拜内尔2200系列树脂是改性乙烯丙烯酸酯树脂。它们含有一种温度稳定的酯,使它们在高温共挤出中发挥作用。它们以颗粒形式提供,用于传统的挤出和共挤设备,设计用于加工聚乙烯(PE)树脂。拜内尔2200系列树脂适用于各种材料。它们最常用于粘合PE、PP、PET和纸张。 BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. BYNEL 2200 series resins adhere to a wide variety of materials. They are most often used to adhere to PE, PP, PET and paper. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
0.940 | g/cm³ | ASTM D792 |
密度 Density |
0.940 | g/cm³ | ISO 1183 |
熔体质量流动速率 Melt Flow Rate |
|||
190℃,2.16kg 190℃,2.16kg |
2.0 | g/10min | ASTM D1238 |
190℃,2.16kg 190℃,2.16kg |
2.0 | g/10min | ISO 1133 |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
维卡软化温度 Vicat Softening Temp |
48.0 | ℃ | ASTM D1525 |
维卡软化温度 Vicat Softening Temp |
℃ | ISO 306 | |
熔融峰值温度 Melting peak temperature |
℃ | ASTM D3418 | |
熔融温度 Melting temperature |
|||
DSC DSC |
℃ | ISO 3146 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
【新闻资讯】查看全部
注塑产品开裂或易断裂原因及处理方法
2017-06-27 制品开裂,包括表面丝状裂纹、微裂、顶白、开裂及因制件粘膜、流道粘膜儿造成或创伤危机,开裂按时间分脱模开裂和应用开裂。裂纹是指开模或顶出时成型制品破裂。制品偏脆或者脱模不良时有时会产生裂纹。顶出针的速度也会导致裂纹的产生,速度越快,则越容易发生破裂。 制品开裂的原因大致分析如下: 1、加工方面 ①加工压力过大、速度过快、充料越多、注射、保压时间过长,都会造成内应力过大而开裂。 ②快速强拉制品易造成脱模开裂,应适当调整开模速度与压 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |