牌号简介 About |
---|
Technyl A 222F天然FA是一种未填充的聚酰胺66,热稳定,中等粘度,用于注塑成型,快速结晶,用于短周期。该等级在无筋聚酰胺66的主要性能和加工性能之间提供了良好的结合,从而提高了生产率。这些性能与良好的尺寸稳定性和成型零件的刚性有关。它被设计用于食品接触应用。 TECHNYL® A 222F Natural FA is an unfilled polyamide 66, heat stabilized, medium viscosity, for injection moulding, fast crystallization, for short cycles. This grade offers a good combination between primary properties of the unreinforced polyamide 66 and processing properties leading to increased productivity. These performances are associated with excellent dimensional stability and good rigidity of moulded parts. It is designed to be used in food contact applications. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.14 | g/cm³ | ISO 1183/A |
吸水率 Water absorption rate |
|||
23℃,24hr 23℃,24hr |
1.2 | % | ISO 62 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
|||
23℃ 23℃ |
4000 | MPa | ISO 527-2/1A |
拉伸强度 tensile strength |
ISO 527-2/1A | ||
屈服,23℃ Yield, 23 ℃ |
95.0 | MPa | ISO 527-2/1A |
断裂,23℃ Fracture, 23 ℃ |
95.0 | MPa | ISO 527-2/1A |
拉伸应变 Tensile strain |
|||
断裂,23℃ Fracture, 23 ℃ |
% | ISO 527-2 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength |
|||
23℃ 23℃ |
kJ/m² | ISO 179/1eA | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
熔融温度 Melting temperature |
℃ | ISO 11357-3 |
备注 | |||
---|---|---|---|
暂无数据 |
【新闻资讯】查看全部
PPG收购Arsonsisi粉末涂料制造业务
2022-02-13 2月7日,PPG宣布已签署协议,收购位于意大利米兰的工业涂料公司Arsonsisi的粉末涂料业务。根据惯例成交条件,该交易预计将于2022年第一季度完成。财务条款尚未披露。该交易将扩大生 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |