牌号简介 About |
---|
纤维素增强苯酚改性三聚氰胺模塑料具有很好的电气性能、优异的表面硬度、良好的机械性能、良好的紫外线稳定性和良好的耐热性。主要用途:家用电器配件。本产品符合重金属和PCA的允许上限,也符合根据ISO 14528-1:MP(LD30+MD15)、X、E-(LD40+MD05)、X、E DIN7708:MP 181.5,欧盟指令2002/95(RoHS)、2002/96(WEEE)和2006/122(PFOS)标识的要求 Cellulose reinforced phenol modified Melamine moulding compound Very good electrical properties, excellent surface hardness, good mechanical properties, good UV stability and good heat resistance Primary application(s): Mountings for household appliances This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (WEEE) and 2006/122 (PFOS) Identification according to ISO 14528-1: MP (LD30+MD15), X, E - (LD40+MD05), X, E DIN 7708: MP 181.5 |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.60 到 1.70 | g/cm³ | ISO 1183 |
表观密度 Apparent density |
0.55 到 0.75 | g/cm³ | ISO 60 |
收缩率 Shrinkage rate |
ISO 2577 | ||
MD MD 3 |
0.80 到 1.2 | % | ISO 2577 |
MD MD 4 |
0.50 到 0.90 | % | ISO 2577 |
吸水率 Water absorption rate |
|||
23℃,24hr 23℃,24hr |
< 2.0 | % | ISO 62 |
后收缩 Post contraction 5 |
% | ISO 2577 | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
ISO 527-2 | ||
模压成型 Compression Molding |
MPa | ISO 527-2 | |
注塑成型 injection molding |
MPa | ISO 527-2 | |
拉伸强度 tensile strength |
ISO 527-2 | ||
模压成型 Compression Molding |
MPa | ISO 527-2 | |
注塑成型 injection molding |
MPa | ISO 527-2 | |
弯曲模量 Bending modulus |
ISO 178 | ||
模压成型 Compression Molding |
MPa | ISO 178 | |
注塑成型 injection molding |
MPa | ISO 178 | |
弯曲强度 bending strength |
ISO 178 | ||
模压成型 Compression Molding |
MPa | ISO 178 | |
注塑成型 injection molding |
MPa | ISO 178 | |
压缩强度 compressive strength |
MPa | ISO 604 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength |
ISO 179/1eA | ||
模压成型 Compression Molding |
kJ/m² | ISO 179/1eA | |
注塑成型 injection molding |
kJ/m² | ISO 179/1eA | |
简支梁无缺口冲击强度 Charpy Unnotch Impact strength |
ISO 179/1eU | ||
模压成型 Compression Molding |
kJ/m² | ISO 179/1eU | |
注塑成型 injection molding |
kJ/m² | ISO 179/1eU | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ISO 75-2/A | |
8.0 MPa,未退火 8.0 MPa, unannealed |
℃ | ISO 75-2/C | |
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
MD:50~100℃ MD:50~100℃ |
1/℃ | ISO 11359-2 | |
导热系数 Thermal conductivity coefficient |
W/m/K | ASTM E1461 | |
最高使用温度 Maximum operating temperature |
IEC 60216 | ||
<50 h <50 h |
℃ | IEC 60216 | |
20,000 h 20,000 h |
℃ | IEC 60216 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表面电阻率 Surface resistivity |
ohms | IEC 60093 | |
体积电阻率 Volume resistivity |
ohms·cm | IEC 60093 | |
介电强度 Dielectric strength |
kV/mm | IEC 60243-1 | |
相对电容率 Relative permittivity |
IEC 60250 | ||
100 Hz 100 Hz |
IEC 60250 | ||
1 MHz 1 MHz |
IEC 60250 | ||
耗散因数 Dissipation factor |
IEC 60250 | ||
100 Hz 100 Hz |
IEC 60250 | ||
1 MHz 1 MHz |
IEC 60250 | ||
耐电弧性 Arc resistance |
ASTM D495 | ||
相比漏电起痕指数 Compared to the leakage tracing index |
V | IEC 60112 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame retardant level |
|||
1.50 mm 1.50 mm |
UL 94 | ||
灼热丝可燃性指数 Glowing wire flammability index |
℃ | IEC 60695-2-12 | |
灼热丝起燃温度 Igniting temperature of the hot wire |
℃ | IEC 60695-2-13 | |
补充信息 Supplementary information |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
压缩成型压力 Compression molding pressure |
MPa | ||
压缩成型温度 Compression molding temperature |
℃ |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 Compression Molded |
3 Injection Molded |
4 168 h / 110°C |
【新闻资讯】查看全部
飓风哈维强袭美国 国际聚烯烃市场将遭遇重创
2017-08-31 前情提要: 上周末飓风哈维周末登陆美国,为50多年来侵袭得克萨斯州的最强飓风,造成多人丧生,最大威胁由强风变成洪水。 哈维已经导致占美国化工产品三分之一以上的产能下线,后期必然导致价格上升,聚乙烯,聚氯乙烯等化学品短缺进而会影响工业和建筑行业。 飓风哈维造成损失将高达1000亿美元 作为美国的 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |