公司信息及水印
牌号简介 About |
---|
Valox 420SE0树脂30%玻璃纤维增强,UL94 V-0/5V额定值。广泛应用:切边机、食品搅拌机电机定子和换向器、冷却风扇、连接器、线轴、开关等。 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.63 | g/cm³ | ASTM D792 |
特定体积 Specific volume |
0.610 | cm³/g | ASTM D792 |
密度 Density |
1.63 | g/cm³ | ISO 1183 |
熔体质量流动速率 Melt Flow Rate |
|||
250℃,5.0kg 250℃,5.0kg |
42 | g/10min | ASTM D1238 |
熔体体积流动速率 Melt Volume Rate |
|||
250℃,5 kg 250℃,5 kg |
29.0 | cm³/10min | ISO 1133 |
收缩率 Shrinkage rate |
Internal Method | ||
在拉伸杆上,MD On the stretching rod, MD |
% | 内部方法 | |
MD:3.2 mm MD:3.2 mm |
% | 内部方法 | |
在拉伸杆上,TD On the stretching rod, TD |
% | 内部方法 | |
TD:3.2 mm TD:3.2 mm |
% | 内部方法 | |
吸水率 Water absorption rate |
|||
饱和,23℃ Saturation, 23 ℃ |
% | ISO 62 | |
平衡,23℃,50% RH Equilibrium, 23 ℃, 50% RH |
% | ISO 62 | |
耐候性 Weathering resistance |
UL 746C | ||
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength |
ISO 179/1eA | ||
-30℃ -30℃ |
kJ/m² | ISO 179/1eA | |
23℃ 23℃ |
kJ/m² | ISO 179/1eA | |
简支梁无缺口冲击强度 Charpy Unnotch Impact strength |
ISO 179/1eU | ||
-30℃ -30℃ |
kJ/m² | ISO 179/1eU | |
23℃ 23℃ |
kJ/m² | ISO 179/1eU | |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
ASTM D256 | ||
-30℃ -30℃ |
J/m | ASTM D256 | |
23℃ 23℃ |
J/m | ASTM D256 | |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
ISO 180/1A | ||
23℃ 23℃ |
J/m | ASTM D4812 | |
-30℃ -30℃ |
kJ/m² | ISO 180-1A | |
23℃ 23℃ |
kJ/m² | ISO 180-1A | |
悬臂梁无缺口冲击强度 Notched impact strength of cantilever beam |
ISO 180/1U | ||
-30℃ -30℃ |
kJ/m² | ISO 180/1U | |
23℃ 23℃ |
kJ/m² | ISO 180/1U | |
装有测量仪表的落镖冲击 Dart impact equipped with measuring instruments |
|||
23℃,Total Energy 23℃,Total Energy |
J | ASTM D3763 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
1.8 MPa,未退火,3.2 mm 1.8 MPa, unannealed, 3.2 mm |
℃ | ASTM D648 | |
0.45 MPa,未退火,3.2 mm 0.45 MPa, unannealed, 3.2 mm |
℃ | ASTM D648 | |
0.45 MPa,未退火,100 mm跨距 0.45 MPa, unannealed, 100 mm span |
℃ | ISO 75-2/Be | |
1.8 MPa,未退火,100 mm跨距 1.8 MPa, unannealed, 100 mm span |
℃ | ISO 75-2/Ae | |
1.8 MPa,未退火,64 mm跨距 1.8 MPa, unannealed, 64 mm span |
℃ | ISO 75-2/Af | |
维卡软化温度 Vicat Softening Temp |
℃ | ASTM D1525 11 | |
维卡软化温度 Vicat Softening Temp |
|||
A50 A50 |
℃ | ISO 306/A50 | |
B50 B50 |
℃ | ISO 306 | |
B120 B120 |
℃ | ISO 306/B120 | |
球压测试 Ball pressure test |
|||
125℃ 125℃ |
IEC 60695-10-2 | ||
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
TD:-40~40℃ TD:-40~40℃ |
1/℃ | ASTM E831 | |
TD TD |
ISO 11359-2 | ||
-40 到 40℃ -40 to 40 ℃ |
cm/cm/℃ | ISO 11359-2 | |
23 到 80℃ 23 to 80 ℃ |
cm/cm/℃ | ISO 11359-2 | |
MD:-40~40℃ MD:-40~40℃ |
1/℃ | ASTM E831 | |
MD MD |
ISO 11359-2 | ||
-40 到 40℃ -40 to 40 ℃ |
cm/cm/℃ | ISO 11359-2 | |
23 到 80℃ 23 to 80 ℃ |
cm/cm/℃ | ISO 11359-2 | |
导热系数 Thermal conductivity coefficient |
W/m/K | ISO 8302 | |
相对温度指数 Relative temperature index |
|||
电气性能 Electrical performance |
℃ | UL 746 | |
强度机械性能 Strength mechanical performance |
℃ | UL 746 | |
冲击机械性能 Impact mechanical performance |
℃ | UL 746 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表面电阻率 Surface resistivity |
ohms | IEC 60093 | |
体积电阻率 Volume resistivity |
ohms·cm | ASTM D257 | |
体积电阻率 Volume resistivity |
ohms·cm | IEC 60093 | |
介电强度 Dielectric strength |
ASTM D149 | ||
1.6 mm,在油中 1.6 mm in oil |
kV/mm | ASTM D149 | |
3.2 mm,在空气中 3.2 mm in air |
kV/mm | ASTM D149 | |
介电强度 Dielectric strength |
IEC 60243-1 | ||
0.8 mm,在油中 0.8 mm in oil |
kV/mm | IEC 60243-1 | |
1.6 mm,在油中 1.6 mm in oil |
kV/mm | IEC 60243-1 | |
3.2 mm,在油中 3.2 mm in oil |
kV/mm | IEC 60243-1 | |
介电常数 Dielectric constant |
ASTM D150 | ||
100 Hz 100 Hz |
ASTM D150 | ||
1 MHz 1 MHz |
ASTM D150 | ||
相对电容率 Relative permittivity |
IEC 60250 | ||
50 Hz 50 Hz |
IEC 60250 | ||
60 Hz 60 Hz |
IEC 60250 | ||
100 Hz 100 Hz |
IEC 60250 | ||
1 MHz 1 MHz |
IEC 60250 | ||
耗散因数 Dissipation factor |
ASTM D150 | ||
100 Hz 100 Hz |
ASTM D150 | ||
1 MHz 1 MHz |
ASTM D150 | ||
耗散因数 Dissipation factor |
IEC 60250 | ||
50 Hz 50 Hz |
IEC 60250 | ||
60 Hz 60 Hz |
IEC 60250 | ||
100 Hz 100 Hz |
IEC 60250 | ||
1 MHz 1 MHz |
IEC 60250 | ||
耐电弧性 Arc resistance |
ASTM D495 | ||
相比漏电起痕指数 Compared to the leakage tracing index |
UL 746 | ||
相比漏电起痕指数 Compared to the leakage tracing index |
IEC 60112 | ||
CTI CTI |
V | IEC 60112 | |
解决方案 B Solution B |
V | IEC 60112 | |
高电弧燃烧指数(HAI) High Arc Burning Index (HAI) |
UL 746 | ||
高电压电弧起痕速率 High voltage arc marking rate |
|||
HVTR HVTR |
UL 746 | ||
热丝引燃 Hot wire ignition |
|||
HWI HWI |
UL 746 | ||
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame retardant level |
UL 94 | ||
0.40 mm 0.40 mm |
UL 94 | ||
0.71 mm 0.71 mm |
UL 94 | ||
2.00 mm 2.00 mm |
UL 94 | ||
灼热丝可燃性指数 Glowing wire flammability index |
|||
1.0 mm 1.0 mm |
℃ | IEC 60695-2-12 | |
极限氧指数 Extreme oxygen index |
% | ISO 4589-2 | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
MPa | ASTM D638 | |
拉伸模量 Tensile modulus |
MPa | ISO 527-1-2 | |
拉伸强度 tensile strength |
|||
断裂 fracture |
MPa | ISO 527-2/5 | |
断裂 fracture |
MPa | ASTM D638 | |
屈服 yield |
MPa | ISO 527-2/5 | |
屈服 yield |
MPa | ASTM D638 | |
拉伸应变 Tensile strain |
|||
断裂 fracture |
% | ISO 527-2/5 | |
断裂 fracture |
% | ASTM D638 | |
屈服 yield |
% | ISO 527-2/5 | |
屈服 yield |
% | ASTM D638 | |
弯曲模量 Bending modulus |
MPa | ISO 178 | |
50 mm跨距 50 mm span |
MPa | ASTM D790 | |
弯曲强度 bending strength |
MPa | ISO 178 | |
断裂,50 mm跨度 Fracture, 50 mm span |
MPa | ASTM D790 | |
泰伯耐磨性 Taber abraser |
|||
1000 周期,1000 g,CS-17 转轮 1000 cycles, 1000 g, CS-17 wheels |
mg | 内部方法 | |
洛氏硬度 Rockwell hardness |
|||
R 级 R-level |
ISO 2039-2 | ||
R 级 R-level |
ASTM D785 | ||
球压硬度 Ball hardness |
|||
H358/30 H358/30 |
MPa | ISO 2039-1 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 Tensile Bar |
3 0.20 in/min |
4 类型 1, 0.20 in/min |
5 0.051 in/min |
6 0.079 in/min |
7 80*10*4 sp=62mm |
8 80*10*4 |
9 120*10*4 mm |
10 80*10*4 mm |
11 标准 B (120°C/h), 载荷2 (50N) |
12 钨电极 |
【新闻资讯】查看全部
“世界药厂”近乎停摆,印度出口药物供应链几近崩溃!苹果产量腰斩
2021-05-31 搜料网资讯: 近两个月以来,印度第二波新冠疫情快速恶化成为全球抗疫最受瞩目的事件。疫情的肆虐,使得印度很多工厂关闭,众多本土企业和跨国公司陷入困境。 疫情持续恶化 印 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |