HX-155DB是一种完全交联的热塑性弹性体(TPE)产品。热塑性弹性体可以很容易地用一般热塑性加工设备加工。压缩永久变形小,耐候性好,耐高温、耐化学药品和耐臭氧。柔性PVC、橡胶(CR、NBR、EPDM等)可替换为TPE。 HX-155DB is a fully-crosslinked thermoplastic elastomer(TPE) product. TPEs can be easily processed with general thermoplastic processing equipments. It has low compression set, good weatherability and excellent resistance to high temperature, chemicals, and ozone. Flexible PVC, rubbers (CR, NBR, EPDM etc.) can be replaced with TPE. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
0.940 | g/cm³ | ASTM D792 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
|||
邵氏 D Shaw's D |
55 | ASTM D2240 | |
弹性体 elastic body |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength |
|||
断裂 fracture |
15.7 | MPa | ASTM D412 |
100% 应变 100% strain |
9.81 | MPa | ASTM D412 |
拉伸应变 Tensile strain |
|||
断裂 fracture |
600 | % | ASTM D412 |
撕裂强度 tear strength |
kN/m | ASTM D624 | |
压缩形变 Compression deformation |
|||
70℃,72 hr 70℃,72 hr |
% | ASTM D395 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
|||
-40℃ -40℃ |
ASTM D256 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
【新闻资讯】查看全部
注塑模具毛病
2018-10-10 注塑模具的结构形式和模具加工质量直接影响着塑件制品质量和生产效率。注塑模具生产和塑料制品生产实践中最常见,最常出现的一些模具故障及其主要原因分析排除如下 1、浇口脱料困难。 在注塑过程中,浇口粘在浇口套内,不易脱出。开模时,制品出现裂纹损伤。此外,操作者必须用铜棒尖端从喷嘴处敲出,使之松动后方可脱模,严重影响生产效率。这种故障主要原因是浇口锥孔光洁度差,内 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |