MVR(330°C/2.16kg)17 cm³/10分钟;紫外线稳定;软化温度(vst/b 120)=171°C;注塑-熔融温度320-340°C;制动灯和指示灯盖;家用/工业灯盖;车内灯盖;前照灯透镜 MVR (330°C/2.16kg) 17 cm³/10 min; UV stabilized; 'softening temperature (VST/B 120)=171 °C; injection molding - melt temperature 320 - 340°C; Covers for brake lights and indicator lights; Covers for domestic / industrial lamps; car interior light covers; Headlamp lenses |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.17 | g/cm³ | ISO 1183 |
熔体质量流动速率 Melt Flow Rate |
|||
330℃,2.16kg 330℃,2.16kg |
17 | g/10min | ISO 1133 |
熔体体积流动速率 Melt Volume Rate |
|||
330℃,2.16 kg 330℃,2.16 kg |
17.0 | cm³/10min | ISO 1133 |
收缩率 Shrinkage rate 2 |
ISO 294-4 | ||
TD:2.0 mm TD:2.0 mm |
0.80 | % | ISO 294-4 |
MD:2.0 mm MD:2.0 mm |
0.80 | % | ISO 294-4 |
吸水率 Water absorption rate |
|||
饱和,23℃ Saturation, 23 ℃ |
% | ISO 62 | |
平衡,23℃,50% RH Equilibrium, 23 ℃, 50% RH |
% | ISO 62 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁无缺口冲击强度 Charpy Unnotch Impact strength |
ISO 179/1eU | ||
-30℃ -30℃ |
ISO 179/1eU | ||
23℃ 23℃ |
ISO 179/1eU | ||
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ISO 75-2/A | |
0.45 MPa,未退火 0.45 MPa, unannealed |
℃ | ISO 75-2/B | |
维卡软化温度 Vicat Softening Temp |
|||
B120 B120 |
℃ | ISO 306/B120 | |
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
TD:23~55℃ TD:23~55℃ |
1/℃ | ISO 11359-2 | |
MD:23~55℃ MD:23~55℃ |
1/℃ | ISO 11359-2 | |
相对温度指数 Relative temperature index |
|||
电气性能 Electrical performance |
℃ | UL 746 | |
强度机械性能 Strength mechanical performance |
℃ | UL 746 | |
冲击机械性能 Impact mechanical performance |
℃ | UL 746 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表面电阻率 Surface resistivity |
ohms | IEC 60093 | |
体积电阻率 Volume resistivity |
|||
23℃ 23℃ |
ohms·cm | IEC 60093 | |
介电强度 Dielectric strength |
|||
23 ℃,1 mm 23 ℃,1 mm |
kV/mm | IEC 60243-1 | |
相对电容率 Relative permittivity |
IEC 60250 | ||
23℃,100 Hz 23℃,100 Hz |
IEC 60250 | ||
23℃,1 MHz 23℃,1 MHz |
IEC 60250 | ||
耗散因数 Dissipation factor |
IEC 60250 | ||
23℃,100 Hz 23℃,100 Hz |
IEC 60250 | ||
23℃,1 MHz 23℃,1 MHz |
IEC 60250 | ||
相比漏电起痕指数 Compared to the leakage tracing index |
IEC 60112 | ||
解决方案 A Solution A |
V | IEC 60112 | |
解决方案 B Solution B |
V | IEC 60112 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame retardant level |
UL 94 | ||
1.50 mm 1.50 mm |
UL 94 | ||
3.00 mm 3.00 mm |
UL 94 | ||
灼热丝可燃性指数 Glowing wire flammability index |
℃ | IEC 60695-2-12 | |
极限氧指数 Extreme oxygen index 4 |
% | ISO 4589-2 | |
光学性能 optical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
折射率 Refractive index 5 |
ISO 489 | ||
透光率 Transmittance |
|||
1000 µm 1000 µm |
% | ISO 13468-2 | |
补充信息 Supplementary information |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
电解腐蚀 Electrolytic corrosion |
|||
23℃ 23℃ |
IEC 60426 | ||
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
|||
23℃ 23℃ |
MPa | ISO 527-1-2 | |
拉伸强度 tensile strength |
|||
屈服,23℃ Yield, 23 ℃ |
MPa | ISO 527-2/50 | |
拉伸应变 Tensile strain |
|||
屈服,23℃ Yield, 23 ℃ |
% | ISO 527-2/50 | |
标称拉伸断裂应变 Nominal tensile fracture strain |
|||
23℃ 23℃ |
% | ISO 527-2/50 | |
弯曲强度 bending strength 3 |
|||
23℃ 23℃ |
MPa | ISO 178 | |
球压硬度 Ball hardness |
MPa | ISO 2039-1 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 60x60x2 mm |
3 0.079 in/min |
4 程序 A |
5 方法 A |
【新闻资讯】查看全部
全球海运费大跌,新冠疫情和乌克兰危机导致商品供应制约情况缓解
2022-09-26 扫描上图二维码,可以免费下载 搜料 APP 新冠肺炎疫情和乌克兰危机造成的商品供应限制正在不断缓解。截至8月,显示全球供应链混乱程度的指数已连续四个月有所改善,集装箱船运费 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |