它是热塑性弹性体(TPE)系列中的一种软质、黑色、抗紫外辐射的热塑性硫化弹 性体(TPV)。这种材料同时具有良好的物理性质和耐化学性,适用于薄壁或复杂 型材的挤出成型领域。这一牌号的山都平 TPV 是剪切速率依赖型产品,可在常规 热塑性挤出成型、热成型或真空成型设备上加工。这是一种聚烯烃基材料,可在生 产过程中进行回收利用。 A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for thin wall or complex profile extrusion applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for extrusion, thermoforming or vacuum forming. It is polyolefin based and recyclable within the manufacturing stream. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
0.968 | g/cm³ | ASTM D792 |
密度 Density |
0.970 | g/cm³ | ISO 1183 |
弹性体 elastic body |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength |
|||
TD,断裂,23℃ TD, fracture, 23 ℃ |
7.40 | MPa | ASTM D412 |
TD,断裂,23℃ TD, fracture, 23 ℃ |
7.40 | MPa | ISO 37 |
TD,100% 应变,23℃ TD, 100% strain, 23 ℃ |
3.00 | MPa | ASTM D412 |
TD,100% 应变,23℃ TD, 100% strain, 23 ℃ |
MPa | ISO 37 | |
拉伸应变 Tensile strain |
|||
TD,断裂,23℃ TD, fracture, 23 ℃ |
% | ISO 37 | |
TD,断裂,23℃ TD, fracture, 23 ℃ |
% | ASTM D412 | |
撕裂强度 tear strength |
|||
TD,23℃ TD,23℃ |
kN/m | ISO 34-1 | |
TD,23℃ TD,23℃ |
kN/m | ASTM D624 | |
压缩形变 Compression deformation |
ASTM D395B | ||
70℃,22 hr 70℃,22 hr |
% | ASTM D395B | |
125℃,70 hr 125℃,70 hr |
% | ASTM D395B | |
压缩形变 Compression deformation |
ISO 815 | ||
70℃,22 hr 70℃,22 hr |
% | ISO 815 | |
125℃,70 hr 125℃,70 hr |
% | ISO 815 | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
|||
邵氏 A,15 秒,23℃ Shore A, 15 seconds, 23 ℃ |
ISO 868 | ||
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
脆化温度 Embrittlement temperature |
℃ | ASTM D746 | |
脆化温度 Embrittlement temperature |
℃ | ISO 812 | |
老化性能 Aging performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
空气中拉伸强度的变化率 The rate of change in tensile strength in air |
|||
150℃,168 hr 150℃,168 hr |
% | ISO 188 | |
150℃,168 hr 150℃,168 hr |
% | ASTM D573 | |
空气中极限伸长率的变化率 The rate of change in ultimate elongation in air |
|||
150℃,168 hr 150℃,168 hr |
% | ASTM D573 | |
Change in Tensile Strain at Break in Air(150℃,168 hr) Change in Tensile Strain at Break in Air(150℃,168 hr) |
% | ISO 188 | |
Change in Durometer Hardness in Air(邵氏 A,150℃,168 hr) Change in Durometer Hardness in Air (150 ℃, 168 hr) |
ASTM D573 | ||
空气中邵氏硬度的变化率 The rate of change of Shore hardness in air |
|||
邵氏 A,150℃,168 hr Shaw A, 150 ℃, 168 hr |
ISO 188 | ||
拉伸强度的变化率 The rate of change in tensile strength |
|||
125℃,70 hr,in IRM 903 Oil 125℃,70 hr,in IRM 903 Oil |
% | ASTM D471 | |
Change in Tensile Stress(125℃,70 hr,in IRM 903 Oil) Change in Tensile Stress(125℃,70 hr,in IRM 903 Oil) |
% | ISO 1817 | |
Change in Ultimate Elongation(125℃,70 hr,in IRM 903 Oil) Change in Ultimate Elongation(125℃,70 hr,in IRM 903 Oil) |
% | ASTM D471 | |
Change in Tensile Strain at Break(125℃,70 hr,in IRM 903 Oil) Change in Tensile Strain at Break(125℃,70 hr,in IRM 903 Oil) |
% | ISO 1817 | |
体积变化 Volume change |
|||
125℃,70 hr,在IRM 903油中 125 ℃, 70 hr, in IRM 903 oil |
% | ASTM D471 | |
125℃,70 hr,在IRM 903油中 125 ℃, 70 hr, in IRM 903 oil |
% | ISO 1817 | |
耐连续最高温度 Durable to continuous maximum temperature |
|||
1008 hr 1008 hr |
℃ | SAE J2236 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
介电强度 Dielectric strength |
|||
23 ℃,2 mm 23 ℃,2 mm |
kV/mm | ASTM D149 | |
介电常数 Dielectric constant |
|||
23 ℃,1.93 mm 23 ℃,1.93 mm |
IEC 60250 | ||
23 ℃,1.93 mm 23 ℃,1.93 mm |
ASTM D150 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 C 模具 |
3 B 方法,直角形试样(割口) |
4 类型 1 |
5 类型 A |
【新闻资讯】查看全部
利安德巴赛尔计划在德克萨斯州新建一家聚乙烯工厂
2022-06-27 根据《美国化学周刊》6月22日的报道,根据4月和5月提交给德克萨斯州审计署的文件,利安德巴赛尔公司正在考虑是否在德克萨斯州科珀斯克里斯蒂附近的生产基地建设一个新的聚乙烯 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |