公司信息及水印
牌号简介 About |
---|
Lupolen 4021 K RM Black Powder是新一代己烯线性中等密度聚乙烯LP 4021 K RM的黑色化合物版本,用于旋转成型。典型的客户应用包括大型储罐,包括地下和基础设施应用。该产品具有出色的ESCR性能,在低温下具有较高的抗冲击性和抗紫外线性能。Lupolen 4021 K RM Black Powder是一种完全紫外线稳定的聚合物。产品以粉末形式交付。试验表明,这种材料能够抵抗生物柴油的有害影响。**它不适用于医疗和制药应用。**电阻基于我们最新的专利技术 Lupolen 4021 K RM Black Powder is the black compound version of the new generation hexene linear medium-density polyethylene LP 4021 K RM for rotational molding. Typical customer applications include large tanks including underground and infrastructure applications. The product exhibits outstanding ESCR combined with high impact at low temperatures and improved UV resistance. Lupolen 4021 K RM Black Powder is a fully UV-stabilized polymer. The product is delivered as a powder. Tests have shown that this material is resisting against the harmful effect of biodiesel fuel.** It is not intended for use in medical and pharmaceutical applications. ** Resistance is based on our latest patented technology |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density 1 |
0.940 | g/cm³ | ISO 1183 |
熔体质量流动速率 Melt Flow Rate |
|||
190℃,2.16kg 190℃,2.16kg |
4.0 | g/10min | ISO 1133 |
抗环境应力开裂 ESCR(Environmental Stress Cracking Resistance) |
> 1000 | hr | ASTM D1693B |
全切口蠕变试验 Full incision creep test 2 |
|||
50℃ 50℃ 2 |
2.1 | day | ISO 16770 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
750 | MPa | ISO 527-2 |
拉伸强度 tensile strength |
|||
屈服 yield |
MPa | ISO 527-2 | |
拉伸应变 Tensile strain |
|||
断裂 fracture |
% | ISO 527-3 | |
屈服 yield |
% | ISO 527-2 | |
薄膜 film |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸冲击强度 Tensile impact strength |
ISO 8256/1A | ||
-30℃ -30℃ |
kJ/m² | ||
23℃ 23℃ |
kJ/m² | ||
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
维卡软化温度 Vicat Softening Temp |
|||
A50 A50 |
℃ | ISO 306/A50 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 Density value is given of the base polymer. Final density of the black product is higher due to pigmentation. |
3 6.0 MPa, 2% Arkopal N100 |
【新闻资讯】查看全部
埃克森美孚工厂爆炸 大火黑烟不时,37人受伤,公司再次面临巨额赔款
2019-08-05 7月31日周三下午, 埃克森美孚 位于德克萨斯州贝敦的烯烃工厂发生火灾,造成37人受伤,随后股票暴跌。 火灾发生在大约上午11点07分(当地时间)位于休斯敦以东约25英里(40公里)贝 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |