牌号简介 About |
---|
Keliren氯化聚乙烯(CPE)热塑性树脂广泛应用于PVC挤出和注塑应用中的冲击改性剂,尤其是在壁板、外窗型材和管道等产品中。低剂量的Kelliren树脂与硬质聚氯乙烯树脂可以显著提高抗冲击强度,并作为加工助剂。除了具有良好的耐化学性、优异的低温性能、较高的填料接受度和与多种配方成分的良好相容性等特性外,Kelliren树脂在适当配方的化合物中还具有优异的耐候性。用途:FR-ABS,柔性PVC,PE薄膜性能:加工流动性好,残余结晶少。 Keliren® Chlorinated Polyethylene(CPE) thermoplastic resins are widely used as impact modifiers in PVC extrusion and injection molding applications, especially in products such as siding, widow profiles and pipe. The low dosage levels of Keliren® resins with rigid PVC resins can significantly improve impact strength and also act as a processing aid. In addition to offering attributes such as good chemical resistance, excellent low temperature properties, high filler level acceptance and excellent compatibility with a broad range of formulation ingredients, Keliren® resins offer excellent resistance to weathering in a properly formulated compound. Application: FR-ABS, Flexible PVC, PE Film Performance: Excellent processing flowability and minimal residual crystal. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
含氯量 Chlorine content |
34.0 到 36.0 | wt% | ISO 7725 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
|||
邵氏 A Shaw's A |
< 57 | ISO 7619 | |
弹性体 elastic body |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength |
|||
断裂 fracture |
> 8.50 | MPa | ISO 37 |
拉伸应变 Tensile strain |
|||
断裂 fracture |
> 800 | % | ISO 37 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
【新闻资讯】查看全部
院士谈石墨烯开展思路:好材料决议产业未来
2017-04-14 4月10日,在清华大学深圳研究生院召开的2017深圳国际石墨烯高峰论坛上,中国科学院院士、北京大学化学与分子工程学院教授刘忠范表达了为推动石墨烯产业发展,加速我国研发核心技术整体布局的思路及其行动力。 制备决定未来 装备决定制备 “制备决定未来,装备决定制备。石墨烯产业有没有未来,到底有多大,取决于我们能否提供真正好的石墨烯材料。”刘忠范强调。 目前,中国在石墨烯产业化方面走在世界前列。从专利申请情况来看,近 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |