牌号简介 About |
---|
充油丁苯合成橡胶SBR-1706基本上是一种苯乙烯(23.5%)和丁二烯(76.5%)的共聚物,通过乳化法和树脂/脂肪皂得到。共聚物中填充有油hi-ar或tdae。该聚合物不含亚硝胺和可能成为亚硝胺来源的物质。外观-深棕色捆;一捆重量(30±1)kg;包装-塑料容器;保质期-自制造之日起一(1)年 Oil-extended styrene butadiene synthetic rubber SBR-1706 is essentially a styrene (23.5%) and butadiene (76.5%) copolymer obtained by emulsification method with the use of resin/fatty soaps. The copolymer is filled with oil HI-AR or TDAE. The polymer contains no nitrosamines and substances that may become a source of nitrosamines. Appearance - bale of dark-brown color; weight of a bale - (30 ± 1) kg; packing -a plastic container; shelf life - one (1) year since the date of manufacture |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
门尼粘度 Mooney viscosity |
|||
ML 1+4,100℃ ML 1+4,100℃ |
36 到 44 | MU | ASTM D1646 |
结合苯乙烯 Combined with styrene |
22.0 到 25.0 | % | 内部方法 |
含油量 oil content |
|||
HIAR or TDAE HIAR or TDAE |
14 到 17 | % | 内部方法 |
Organic Acid Organic Acid |
5.0 到 6.4 | % | ASTM D5774 |
Soap(Organic Acid) Soap(Organic Acid) |
< 0.25 | % | ASTM D5774 |
Solvent Extract Content Solvent Extract Content |
% | 内部方法 | |
灰份含量 Ash Content |
% | ASTM D5667 | |
挥发物 Volatiles |
% | ASTM D5668 | |
弹性体 elastic body |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength |
|||
屈服 yield |
MPa | ASTM D3185 | |
300% 应变 300% strain |
MPa | ASTM D3185 | |
拉伸应变 Tensile strain |
|||
断裂 fracture |
% | ASTM D3185 |
备注 | |||
---|---|---|---|
暂无数据 |
【新闻资讯】查看全部
103.6亿元!河南心连心化学工业集团项目开工,涉及PA6、PA66等装置
2022-11-30 扫描上图二维码,可以免费下载 搜料 APP 11月27日,河南心连心化学工业集团股份有限公司化工新材料项目开工奠基仪式在新乡县化工园区举行。 心连心集团计划建设化工新材料项目, |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |
电邮一份说明书
PDF文档名:搜料网-SIBUR Synthetic Rubber SBR-1706 Grade D证书
发送至:(多个地址,中间以逗号隔开)
发送一份副本给我:您还没有填写邮箱!(点击完善资料)