牌号简介 About |
---|
Dryflex® PCW 92A331B:热塑性弹性体基材:TPO硬度:92邵尔A工作温度范围:-50至+75°C(无应力材料)。颜色:黑色表示:自由流动的颗粒,在正常条件下储存时无需预干燥。耐候性:优异的耐臭氧/紫外线性:优异的耐化学性:良好(不包括有机溶剂、芳香族和植物油)回收:100%可回收的模具收缩率(线性):约0.75-2%取决于例如,门式连接的形状和位置:PP、PE特殊特征:该等级包含约33%的消费后废物(按重量计)。 Dryflex PCW 92A331B: Thermoplastic Elastomer Base Material: TPO Hardness: 92 Shore A Service Temperature Range: -50 to +75°C (Unstressed Material). Colour: Black Presentation: Free flowing pellets that can be processed without predrying when stored under normal conditions Weather Resistance: Excellent Ozone / UV Resistance: Excellent Chemical Resistance: Good (excluding organic solvents, aromatic and vegetable oils) Recycling: 100% recyclable Mould Shrinkage (linear): Approx. 0.75 - 2% depending on e.g. shape of the detail and placement of gate Bonds to: PP, PE Special Features: This grade contains approximately 33% by weight of Post Consumer Waste |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.11 | g/cm³ | ISO 2781 |
收缩率 Shrinkage rate 2 |
0.75 to 2.0 | % | ISO 294-4 |
弹性体 elastic body |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength |
|||
屈服 yield |
7.50 | MPa | ISO 37 |
100% 应变 100% strain |
6.20 | MPa | ISO 37 |
拉伸应变 Tensile strain |
|||
断裂 fracture |
470 | % | ISO 37 |
撕裂强度 tear strength 3 |
kN/m | ISO 34-1 | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
|||
邵氏 A Shaw's A |
ISO 868 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 Depending on e.g. shape of the detail and placement of gate |
3 C 方法:新月形试样 |
【新闻资讯】查看全部
毛细管流变测量,热波动性ASTM D3835,
2017-07-03 毛细管流变剪切扫描,热稳定性ASTM D3835,ISO 11443 适用范围: 毛细管流变测量法在宽范围的剪切速率范围和不同温度下测量表观粘度(耐流动性),这与在模制,压延,挤出等方面遇到的 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |