牌号简介 About |
---|
Starflex GM1210BA是一种颗粒状的MLLDPE树脂,用于需要最大强度和韧性的应用场合。GM1210BA包含一个处理辅助装置,但不包含滑动或防阻塞装置。 Starflex GM1210BA is a pelletized mLLDPE resin for use in applications that require maximum strength and toughness. GM1210BA contains a processing aid but does not contain slip or antiblock. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
0.912 | g/cm³ | ASTM D1505 |
熔体质量流动速率 Melt Flow Rate |
|||
190℃,2.16kg 190℃,2.16kg |
1.0 | g/10min | ASTM D1238 |
薄膜 film |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
薄膜厚度 film thickness |
|||
测试 test |
19 | µm | |
割线模量 Secant modulus |
ASTM D882 | ||
1% 正割,MD:19 µm 1% secant, MD: 19 µ m |
152 | MPa | ASTM D882 |
1% 正割,TD:19 µm 1% secant, TD: 19 µ m |
159 | MPa | ASTM D882 |
拉伸强度 tensile strength |
ASTM D882 | ||
MD,断裂,19 µm MD, fracture, 19 µ m |
MPa | ASTM D882 | |
TD,断裂,19 µm TD, fracture, 19 µ m |
MPa | ASTM D882 | |
拉伸应变 Tensile strain |
ASTM D882 | ||
MD,断裂,19 µm MD, fracture, 19 µ m |
% | ASTM D882 | |
TD,断裂,19 µm TD, fracture, 19 µ m |
% | ASTM D882 | |
落锤冲击 Drop hammer impact |
|||
19 µm 19 µm |
g | ASTM D1709-A | |
埃尔曼多夫抗撕强度 Elmandorf tear strength |
ASTM D1922 | ||
MD:19 µm MD:19 µm |
g | ASTM D1922 | |
TD:19 µm TD:19 µm |
g | ASTM D1922 | |
光学性能 optical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
光泽度 gloss |
|||
45°,19.1 µm 45°,19.1 µm |
ASTM D2457 | ||
雾度 Haze |
|||
19.1 µm 19.1 µm |
% | ASTM D1003 |
备注 | |||
---|---|---|---|
暂无数据 |
【新闻资讯】查看全部
美媒:特斯拉制造“鲶鱼效应”,助力中国电动汽车弯道超车
2021-12-02 搜料网资讯: 42年前,刘相尚造出帮助工厂生产廉价玩具和手表的机器。如今他帮特斯拉生产造车机械,用该公司创始人马斯克的话说,就是像造玩具汽车一样造出真正的汽车。 从某种 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |