Sarlink® TPE EE-2235N是一种热塑性弹性体(TPE)材料,。 该产品在亚太地区、北美洲、拉丁美洲、欧洲或非洲和中东有供货,加工方式为:挤出。 Sarlink® TPE EE-2235N的主要特性为:通过 ROHS 认证。 Sarlink® TPE EE-2235N的典型应用领域为:汽车行业 Sarlink EE-2235N is a general purpose thermoplastic elastomer designed for automotive applications, including exterior extruded components. Sarlink EE-2235N is a low hardness, high density, filled grade with good UV resistance and and has excellent extrudability. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.17 | g/cm³ | ASTM D792 |
熔体质量流动速率 Melt Flow Rate |
|||
230℃,2.16kg 230℃,2.16kg |
0.60 | g/10min | ASTM D1238 |
弹性体 elastic body |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength |
ASTM D412 | ||
TD,100% 应变 TD, 100% strain |
0.552 | MPa | ASTM D412 |
MD,100% 应变 MD, 100% strain |
0.896 | MPa | ASTM D412 |
拉伸强度 tensile strength |
ASTM D412 | ||
断裂 fracture |
5.24 | MPa | ASTM D412 |
MD,断裂 MD, fracture |
MPa | ASTM D412 | |
拉伸应变 Tensile strain |
ASTM D412 | ||
断裂 fracture |
% | ASTM D412 | |
流量,断裂 Flow rate, fracture |
% | ASTM D412 | |
撕裂强度 tear strength |
|||
TD TD |
kN/m | ASTM D624 | |
压缩形变 Compression deformation |
ASTM D395 | ||
23℃,22 hr 23℃,22 hr |
% | ASTM D395 | |
70℃,22 hr 70℃,22 hr |
% | ASTM D395 | |
125℃,70 hr 125℃,70 hr |
% | ASTM D395 | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
ASTM D2240 | ||
邵氏 A Shaw's A |
ASTM D2240 | ||
邵氏 A,15 秒 Shore A, 15 seconds |
ASTM D2240 |
备注 |
---|
1 (formerly approved under Tekron 4000-35UV) |
2 一般属性:这些不能被视为规格。 |
【新闻资讯】查看全部
大亚湾经开区:加快建成世界级产业基地
2022-02-22 2022年是党的二十大隆重召开、实施十四五规划承上启下的重要一年,也是大亚湾区加快建成世界级绿色石化产业基地的重要一年。大亚湾区的三大项目在今年的广东省政府工作中被提及 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |