牌号简介 About |
---|
Ultem 2312EPR树脂,30%磨碎玻璃填充,高流动性聚醚酰亚胺(TG 217C),具有内部脱模和增强的电稳定性。符合ECO标准,UL94 v0清单。 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.48 | g/cm³ | ASTM D792 |
密度 Density |
1.48 | g/cm³ | ISO 1183 |
熔体质量流动速率 Melt Flow Rate |
|||
337℃,6.60kg 337℃,6.60kg |
14 | g/10min | ASTM D1238 |
熔体体积流动速率 Melt Volume Rate |
|||
360℃,5 kg 360℃,5 kg |
14.0 | cm³/10min | ISO 1133 |
收缩率 Shrinkage rate |
Internal Method | ||
MD MD 2 |
0.40 to 0.60 | % | 内部方法 |
MD:3.2 mm MD:3.2 mm |
% | 内部方法 | |
收缩率 Shrinkage rate |
|||
TD:3.2 mm TD:3.2 mm |
% | 内部方法 | |
吸水率 Water absorption rate |
|||
饱和,23℃ Saturation, 23 ℃ |
% | ISO 62 | |
平衡,23℃,50% RH Equilibrium, 23 ℃, 50% RH |
% | ISO 62 | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus 3 |
MPa | ASTM D638 | |
拉伸模量 Tensile modulus |
MPa | ISO 527-1-2 | |
拉伸强度 tensile strength 4 |
|||
断裂 fracture 4 |
MPa | ASTM D638 | |
断裂 fracture |
MPa | ISO 527-2/5 | |
屈服 yield |
MPa | ISO 527-2/5 | |
屈服 yield 4 |
MPa | ASTM D638 | |
拉伸应变 Tensile strain 4 |
|||
断裂 fracture |
% | ISO 527-2/5 | |
断裂 fracture 4 |
% | ASTM D638 | |
屈服 yield |
% | ISO 527-2/5 | |
屈服 yield 4 |
% | ASTM D638 | |
弯曲模量 Bending modulus 6 |
MPa | ISO 178 | |
50 mm跨距 50 mm span 5 |
MPa | ASTM D790 | |
弯曲强度 bending strength 6 , 7 |
MPa | ISO 178 | |
弯曲强度 bending strength 5 |
|||
屈服,50 mm跨度 Yield, 50 mm span 5 |
MPa | ASTM D790 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength 8 |
ISO 179/1eA | ||
-30℃ -30℃ |
kJ/m² | ISO 179/1eA | |
23℃ 23℃ |
kJ/m² | ISO 179/1eA | |
简支梁无缺口冲击强度 Charpy Unnotch Impact strength 8 |
ISO 179/1eU | ||
-30℃ -30℃ |
kJ/m² | ISO 179/1eU | |
23℃ 23℃ |
kJ/m² | ISO 179/1eU | |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch 9 |
ISO 180/1A | ||
23℃ 23℃ |
J/m | ASTM D4812 | |
23℃ 23℃ |
J/m | ASTM D256 | |
-30℃ -30℃ |
kJ/m² | ISO 180-1A | |
23℃ 23℃ |
kJ/m² | ISO 180-1A | |
悬臂梁无缺口冲击强度 Notched impact strength of cantilever beam 9 |
ISO 180/1U | ||
-30℃ -30℃ |
kJ/m² | ISO 180/1U | |
23℃ 23℃ |
kJ/m² | ISO 180/1U | |
装有测量仪表的落镖冲击 Dart impact equipped with measuring instruments |
|||
23℃,Total Energy 23℃,Total Energy |
J | ASTM D3763 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
ASTM D648 | ||
1.8 MPa,未退火,64 mm跨距 1.8 MPa, unannealed, 64 mm span 10 |
℃ | ISO 75-2/Af | |
0.45 MPa,未退火,64 mm跨距 0.45 MPa, unannealed, 64 mm span 10 |
℃ | ISO 75-2/Bf | |
0.45 MPa,未退火,3.2 mm 0.45 MPa, unannealed, 3.2 mm |
℃ | ASTM D648 | |
0.45 MPa,未退火,6.4 mm 0.45 MPa, unannealed, 6.4 mm |
℃ | ASTM D648 | |
热变形温度 Hot deformation temperature |
ASTM D648 | ||
1.8 MPa,未退火,3.2 mm 1.8 MPa, unannealed, 3.2 mm |
℃ | ASTM D648 | |
1.8 MPa,未退火,6.4 mm 1.8 MPa, unannealed, 6.4 mm |
℃ | ASTM D648 | |
维卡软化温度 Vicat Softening Temp |
℃ | ASTM D1525 11 | |
维卡软化温度 Vicat Softening Temp |
|||
B50 B50 |
℃ | ISO 306 | |
B120 B120 |
℃ | ISO 306/B120 | |
球压测试 Ball pressure test |
|||
125℃ 125℃ |
IEC 60695-10-2 | ||
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
TD:23~150℃ TD:23~150℃ |
1/℃ | ISO 11359-2 | |
TD:-40~150℃ TD:-40~150℃ |
1/℃ | ASTM E831 | |
MD:23~150℃ MD:23~150℃ |
1/℃ | ISO 11359-2 | |
MD:-40~150℃ MD:-40~150℃ |
1/℃ | ASTM E831 | |
导热系数 Thermal conductivity coefficient |
W/m/K | ISO 8302 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
耐电弧性 Arc resistance 12 |
ASTM D495 | ||
相比漏电起痕指数 Compared to the leakage tracing index |
UL 746 | ||
高电弧燃烧指数(HAI) High Arc Burning Index (HAI) |
UL 746 | ||
高电压电弧起痕速率 High voltage arc marking rate |
|||
HVTR HVTR |
UL 746 | ||
热丝引燃 Hot wire ignition |
|||
HWI HWI |
UL 746 | ||
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
0.40 mm 0.40 mm |
UL 94 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 Tensile Bar |
3 0.20 in/min |
4 类型 1, 0.20 in/min |
5 0.051 in/min |
6 0.079 in/min |
7 Yield |
8 80*10*4 sp=62mm |
9 80*10*4 |
10 80*10*4 mm |
11 标准 B (120°C/h), 载荷2 (50N) |
12 钨电极 |
【新闻资讯】查看全部
齐鲁石化塑料厂孵化27项创新效果
2018-02-06 1月3日,齐鲁石化塑料厂高密度聚乙烯装置排放气回收系统稳定运行105天,运行周期创出新高,系统回收效率与回收总量实现同步提升,标志着该厂在此项技术创新领域实现突破。 成绩来自于不懈的努力。2017年,该厂党委及各基层党支部坚持“融入中心、服务大局、务实有效”,通过党员攻关创效、党员先锋机组等做法,以及厂党委组织的“党员之星”评选等,推动基层党组织、党员融入企业创新创效工作,并以党组织、党员创新创效推动全员创新创效,成功“孵化”QHM32F茂金属产品系列化生产开发等27项创新 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |