Hyflon PFA是一个独特的半结晶、可熔融处理的全氟聚合物家族,它结合了优异的机械特性和独特的性能,如化学惰性、耐热性、固有的阻燃性、低表面能和特殊的介电性能。Hyflon PFA树脂的设计目的是在从低温到300°C(572°F)*的各种温度范围内保持其性能,并且是化学工艺工业、特种电缆、半导体工业、航空航天和其他具有挑战性的行业中衬里等应用的首选材料。Hyflon® PFA P120X是一种低熔融流动速率树脂,专为吹塑应用而设计,需要极高的粘度和熔融强度。与标准PFA相比,它对气体的渗透性也显著降低。Hyflon pfa p12ox是一种ASTM D3307-XVI型树脂。*对于300°C(572°F)下的额定值,请联系您的Solvay代表。 Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance, inherent flame resistance, low surface energy, and exceptional dielectric properties. Hyflon® PFA resins have been designed to retain their properties over a wide range of temperatures from cryogenic up to 300°C (572°F)* and are the material of choice in applications such as linings in the Chemical Process Industry, specialty cables, semiconductor industry, aerospace, and other challenging industries. Hyflon® PFA P120X is a low melt flow rate resin designed for blow molding applications, where very high viscosity and melt strength are needed. It also has significantly lower permeability to gasses than standard PFAs. Hyflon® PFA P12OX is an ASTM D3307 - Type XVI resin. * For rating at 300°C (572°F) contact your Solvay Representative. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
熔体质量流动速率 Melt Flow Rate |
|||
372℃,5.0kg 372℃,5.0kg |
2.5 到 5.0 | g/10min | ASTM D1238 |
密度 Density |
2.120 到 2.170 | g/cm³ | ASTM D792 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus 2 |
|||
280℃ 280℃ 3 |
49.0 | MPa | ASTM D1708 |
23℃ 23℃ 2 |
500 到 600 | MPa | ASTM D1708 |
拉伸强度 tensile strength |
|||
断裂,280℃ Fracture, 280 ℃ |
4.60 | MPa | ASTM D1708 |
断裂,23℃ Fracture, 23 ℃ |
MPa | ASTM D1708 | |
拉伸应变 Tensile strain |
|||
断裂,280℃ Fracture, 280 ℃ |
% | ASTM D1708 | |
断裂,23℃ Fracture, 23 ℃ |
% | ASTM D1708 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
熔融温度 Melting temperature |
℃ | ASTM D3307 | |
结晶峰温度 Crystallization peak temperature |
|||
DSC DSC |
℃ | DSC | |
比热 specific heat |
|||
23℃ 23℃ |
J/kg/℃ | DSC | |
导热系数 Thermal conductivity coefficient |
|||
40℃ 40℃ |
W/m/K | ASTM C177 | |
结晶热 Crystallization heat |
J/g | DSC | |
融合热量 Fusion heat |
J/g | DSC | |
线性热膨胀系数 Linear coefficient of thermal expansion |
cm/cm/℃ | ASTM D696 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 0.039 in/min |
3 1mm/min |
【新闻资讯】查看全部
震雄集团中期溢利暴增210%
2017-12-08 据震雄集团发布的最新公告显示,截至2017年9月30日止6个月,震雄集团收益8.7亿港元,同比增长22%;公司拥有人应占溢利为6596.2万港元,同比增长210%。 震雄集团表示,本财年上半年,集团无论在营业额、利润或产品销量方面都平稳向上,主要原因是该集团的新产品广受市场欢迎(如新的第六代MK6注塑机系列,以及两板式大型注塑机等)。而中国经济增长稳中向好,世界主体经济陆续改善(尤其是一些发展中国家),这些都是推动震雄集团业绩上升的重要因素。 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |