牌号简介 About |
---|
KetaSpire® KT-820P是一种低流量等级的无增强聚醚醚酮(PEEK),以天然色粗粉形式提供。KetaSpire Peek是按照最高的行业标准生产的,具有独特的性能组合,包括优异的耐磨性、一流的抗疲劳性、易熔加工性、高纯度和对有机物、酸和碱具有优异的耐化学性。这些特性使其非常适合用于医疗、运输、电子、化学加工和其他工业用途。KetaSpire® KT-820P用于挤压复合。这种粉末也可作为KT-820NT在自然色颗粒形式注射成型。 KetaSpire® KT-820P is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industry standards and is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, ease of melt processing, high purity and excellent chemical resistance to organics, acids, and bases. These properties make it well-suited for applications in healthcare, transportation, electronics, chemical processing, and other industrial uses. KetaSpire® KT-820P is intended for extrusion compounding. This powder is also available as KT-820NT in a natural-color pellet form for injection molding. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.30 | g/cm³ | ASTM D792 |
吸水率 Water absorption rate |
|||
24hr 24hr |
0.10 | % | ASTM D570 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
3600 | MPa | ASTM D638 |
拉伸强度 tensile strength |
96.0 | MPa | ASTM D638 |
拉伸应变 Tensile strain |
ASTM D638 | ||
屈服 yield |
5.2 | % | ASTM D638 |
断裂 fracture 3 |
% | ASTM D638 | |
断裂 fracture 4 |
% | ASTM D638 | |
弯曲模量 Bending modulus |
MPa | ASTM D790 | |
弯曲强度 bending strength |
MPa | ASTM D790 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
J/m | ASTM D256 | |
悬臂梁无缺口冲击强度 Notched impact strength of cantilever beam |
ASTM D4812 | ||
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ASTM D648 | |
玻璃化转变温度 Glass transition temperature |
℃ | ASTM D3417 | |
熔融温度 Melting temperature |
℃ | ASTM D3417 | |
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
MD:-50~50℃ MD:-50~50℃ |
1/℃ | ASTM E831 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 结晶 |
3 淬火 |
【新闻资讯】查看全部
台湾科技大学《ACS Omega》:热塑性聚氨酯混合物中氮化硼/石墨烯的聚合
2021-10-15 搜料网资讯: 在全球变暖和气候变化的背景下,避免和减少能源浪费引起了越来越多的关注。随着材料科学的进步,各种具有高导热性的多功能材料显示出优异的节能潜力。台湾科技大 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |