LNP*Thermocomp*ZKC06是一种基于PPO树脂的化合物,含有矿物填料、冲击改性剂。这种材料的附加特性包括:高介电常数(dk)、极低的耗散系数(df)、良好的延展性和良好的热性能。 LNP* Thermocomp* ZKC06 is a compound based on PPO resin containing Mineral Filler, Impact Modifier. Added features of this material include: high dielectric constant (Dk), extremely low dissipation factor (Df), good ductility, and good thermal performance. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.35 | g/cm³ | ASTM D792,ISO 1183 |
熔体质量流动速率 Melt Flow Rate |
ASTM D1238 | ||
300℃,10.0kg 300℃,10.0kg |
36 | g/10min | ASTM D1238 |
300℃,5.0kg 300℃,5.0kg |
11 | g/10min | ASTM D1238 |
熔体体积流动速率 Melt Volume Rate |
ISO 1133 | ||
300℃,10 kg 300℃,10 kg |
30.0 | cm³/10min | ISO 1133 |
300℃,5 kg 300℃,5 kg |
9.00 | cm³/10min | ISO 1133 |
收缩率 Shrinkage rate |
ISO 294-4 | ||
TD:24 hrs TD:24 hrs |
% | ISO 294-4 | |
MD:24 hrs MD:24 hrs |
% | ISO 294-4 | |
吸水率 Water absorption rate |
|||
23℃,24hr 23℃,24hr |
% | ISO 62 | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
|||
-- -- 2 |
MPa | ASTM D638 | |
-- -- |
MPa | ISO 527-1-2 | |
拉伸强度 tensile strength |
|||
屈服 yield 3 |
MPa | ASTM D638 | |
屈服 yield |
MPa | ISO 527-2/50 | |
断裂 fracture 3 |
MPa | ASTM D638 | |
断裂 fracture |
MPa | ISO 527-2/50 | |
拉伸应变 Tensile strain |
|||
屈服 yield 3 |
% | ASTM D638 | |
屈服 yield |
% | ISO 527-2/50 | |
断裂 fracture 3 |
% | ASTM D638 | |
断裂 fracture |
% | ISO 527-2/50 | |
弯曲模量 Bending modulus |
|||
50 mm跨距 50 mm span 4 |
MPa | ASTM D790 | |
-- -- 5 |
MPa | ISO 178 | |
弯曲强度 bending strength |
|||
-- -- 5 , 6 |
MPa | ISO 178 | |
-- -- 5 , 7 |
MPa | ISO 178 | |
屈服,50 mm跨度 Yield, 50 mm span 4 |
MPa | ASTM D790 | |
断裂,50 mm跨度 Fracture, 50 mm span 4 |
MPa | ASTM D790 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
|||
-20℃ -20℃ |
J/m | ASTM D256 | |
23℃ 23℃ |
J/m | ASTM D256 | |
-20℃ -20℃ 8 |
kJ/m² | ISO 180-1A | |
23℃ 23℃ 8 |
kJ/m² | ISO 180-1A | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
0.45 MPa,未退火,3.2 mm 0.45 MPa, unannealed, 3.2 mm |
℃ | ASTM D648 | |
0.45 MPa,未退火,64 mm跨距 0.45 MPa, unannealed, 64 mm span 9 |
℃ | ISO 75-2/Bf | |
1.8 MPa,未退火,3.2 mm 1.8 MPa, unannealed, 3.2 mm |
℃ | ASTM D648 | |
1.8 MPa,未退火,64 mm跨距 1.8 MPa, unannealed, 64 mm span 9 |
℃ | ISO 75-2/Af | |
线性热膨胀系数 Linear coefficient of thermal expansion |
ASTM E831 | ||
MD:-40~150℃ MD:-40~150℃ |
1/℃ | ASTM E831 | |
TD:-40~150℃ TD:-40~150℃ |
1/℃ | ASTM E831 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
介电常数 Dielectric constant |
内部方法 | ||
1.10 GHz 1.10 GHz |
内部方法 | ||
1.9 GHz 1.9 GHz |
内部方法 | ||
5.00 GHz 5.00 GHz |
内部方法 | ||
10.0 GHz 10.0 GHz |
内部方法 | ||
耗散因数 Dissipation factor |
内部方法 | ||
1.1 GHz 1.1 GHz |
内部方法 | ||
1.9 GHz 1.9 GHz |
内部方法 | ||
5 GHz 5 GHz |
内部方法 | ||
10 GHz 10 GHz |
内部方法 | ||
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
1.0 到 3.0 mm 1.0 to 3.0 mm |
UL 94 |
备注 |
---|
2 50 mm/min |
3 类型 1, 50 mm/min |
4 1.3 mm/min |
5 2.0 mm/min |
6 Yield |
7 Break |
8 80*10*4 |
9 80*10*4 mm |