公司信息及水印
牌号简介 About |
---|
BorSafe™ HE3498-LS是采用先进的Borstar技术生产的双峰聚乙烯化合物。它能完全稳定地抵抗热降解,并且挤出过程中形成的模具最小化。此外,它有一个高度覆盖的颜料,即使挤压成一层薄薄的黑色管道,也能产生明亮的条纹。它还含有紫外线稳定剂。BorSafe™ HE3498-LS建议用于生产由Borsafe HE3490-LS生产的黑色管道的识别条纹。 BorSafe HE3498-LS is a bimodal polyethylene compound produced by the advanced Borstar technology. It's fully stabilized against thermal degradation and the die buid-up during extrusion is minimized. Furthermore, it has a highly covered pigment that gives a bright colored stripe even when extruded as a thin layer on a black pipe. It also contains UV-stabilizer. BorSafe HE3498-LS recommended for the production of identifying stripes of black pipes produced from BorSafe HE3490-LS |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
0.953 | g/cm³ | ISO 1183 |
熔体质量流动速率 Melt Flow Rate |
|||
190℃,5.0kg 190℃,5.0kg |
0.30 | g/10min | ISO 1133 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
【新闻资讯】查看全部
热熟化模塑工艺影响制品紧缩变定功能
2015-11-30 在热熟化模塑工艺中,能否得到满意的模塑制品很大程度上取决于有效的熟化条件。一般在发泡完毕后,模具必须在1min内迅速加热,以补充在模具表面的热量损失。但如果加热太快,易使泡沫带来不稳定因素,造成部分塌泡;同时,过多的热量易使脱模剂液化为泡沫体所吸收,造成在模具中表面粘模。如加热太慢,则影响熟化,造成脱模困难和影响制品的压缩变定性能。 加热热源可采用气体燃料或其它辐射加热等方式,加热后还需在洞道中进行保温。 由于上述装置占地面积大,能量损耗亦很可观,目前热熟化 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |