Baytec 352是一种双组分、一次成型的系统,在邵尔75A至90A的硬度范围内产生具有良好机械性能的固体聚氨酯弹性体。与任何产品一样,在给定应用中使用Baytec 352必须事先由用户进行测试(包括现场测试等),以确定其适用性。 Baytec 352 is a two-component, one-shot system that yields a solid polyurethane elastomer with good mechanical properties in the hardness range of Shore 75A to 90A. As with any product, use of Baytec 352 in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability. |
技术参数 Technical Data | |||
---|---|---|---|
弹性体 elastic body |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength |
|||
断裂 fracture |
16.6 | MPa | ASTM D412 |
拉伸应变 Tensile strain |
|||
断裂 fracture |
410 | % | ASTM D412 |
撕裂强度 tear strength |
|||
-- -- 2 |
47.8 | kN/m | ASTM D624 |
开裂 cracking |
13 | kN/m | ASTM D1938 |
压缩形变 Compression deformation |
|||
70℃,22 hr 70℃,22 hr |
84 | % | ASTM D395B |
巴肖氏弹性 Basho's elasticity |
% | ASTM D2632 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热固组件 Thermosetting components |
|||
Part C Part C 3 |
|||
部件 A Component A 4 |
|||
部件 B Component B 5 |
|||
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
|||
邵氏 A Shaw's A |
ASTM D2240 | ||
泰伯耐磨性 Taber abraser |
|||
1000 周期 1000 cycles |
mg | ASTM D3489 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 C 模具 |
3 1,4 Butone Diol |
4 Isocyanate |
5 Polyol |
【新闻资讯】查看全部
工业互联网平台连接工业设备总数7300万台
2021-04-27 搜料网资讯: 记者23日从工信部获悉,截至3月底,企业关键工序数控化率、数字化研发设计工具普及率分别达52.1%和73%,工业互联网平台连接工业设备总数达到7300万台,工业App突破59万 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |