牌号简介 About |
---|
LLDPE薄膜产品应用LL6910LA是硬质吹塑薄膜级产品,提供经认证的低水平凝胶,非常适合具有高度装饰性印刷的层压或薄膜应用。优点和特点LL6910LA是一种线型低密度聚乙烯共聚物,它含有己烯-1作为共聚单体,具有极低的凝胶级、良好的光学性能、耐高温、高抗蠕变性、优异的密封性和热粘着力,如果需要电晕处理,则水平应正常。l在38-48mn/m范围内。 LLDPE film products Applications LL6910LA is rigid blown film grade offering a certified low level of gels making it ideal for lamination or thin film applications with highly decorative printing. Benefits and Features LL6910LA is a linear low density polyethylene copolymer containing hexene-1 as the co-monomer which offers the following properties: Very low gel level Good optical properties High temperature resistance High creep resistance Excellent sealability and hot-tack strength If corona treatment is necessary, the level should normally be in the range 38-48 mN/m. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
0.936 | g/cm³ | ISO 1183/A |
熔体质量流动速率 Melt Flow Rate |
|||
190℃,2.16kg 190℃,2.16kg |
1.0 | g/10min | ISO 1133 |
薄膜 film |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
薄膜厚度 film thickness |
|||
测试 test |
38 | µm | |
拉伸模量 Tensile modulus |
|||
1% 正割,38 µm,吹塑薄膜 1% secant, 38 µ m, blow molded film |
450 | MPa | ISO 1184 |
拉伸强度 tensile strength |
ISO 527-3 | ||
MD,屈服,38 µm,吹塑薄膜 MD, yield, 38 µ m, blow molded film |
18.0 | MPa | ISO 527-3 |
TD,屈服,38 µm,吹塑薄膜 TD, yield, 38 µ m, blow molded film |
MPa | ISO 527-3 | |
拉伸强度 tensile strength |
ISO 527-3 | ||
MD,断裂,38 µm,吹塑薄膜 MD, fracture, 38 µ m, blow molded film |
MPa | ISO 527-3 | |
TD,断裂,38 µm,吹塑薄膜 TD, fracture, 38 µ m, blow molded film |
MPa | ISO 527-3 | |
拉伸应变 Tensile strain |
ISO 1184 | ||
MD,断裂,38 µm,吹塑薄膜 MD, fracture, 38 µ m, blow molded film |
% | ISO 1184 | |
TD,断裂,38 µm,吹塑薄膜 TD, fracture, 38 µ m, blow molded film |
% | ISO 1184 | |
落锤冲击 Drop hammer impact |
|||
38 µm,吹塑薄膜 38 µ m, blow molded film |
g | ASTM D1709-A | |
撕裂强度 tear strength |
|||
MD,38 µm,吹塑薄膜 MD, 38 µ m, blow molded film |
g | ASTM D1922 | |
埃尔曼多夫抗撕强度 Elmandorf tear strength |
|||
TD,38 µm,吹塑薄膜 TD, 38 µ m, blow molded film |
g | ASTM D1922 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
维卡软化温度 Vicat Softening Temp |
℃ | ISO 306/A | |
光学性能 optical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
光泽度 gloss |
|||
45°,38 µm,吹塑薄膜 45 °, 38 µ m, blow molded film |
ASTM D2457 | ||
雾度 Haze |
|||
38 µm,吹塑薄膜 38 µ m, blow molded film |
% | ASTM D1003 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
【新闻资讯】查看全部
煤电供应紧张化企面临限电限产
2021-08-16 搜料网资讯: 受夏季用电高峰期影响,近期多地用电负荷骤增、用煤紧张,部分省份采取限电措施,化工企业不得不错峰生产或是安排检修,生产运营受到极大影响。 国家电网数据显示 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |