牌号简介 About |
---|
建议使用抗真菌的PVC化合物注射浴室地毯。 |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density 2 |
1.30 到 1.36 | g/cm³ | ASTM D792 |
Cadmium Content Cadmium Content |
< 50 | ppm | IEC 62321 |
Chromium Content Chromium Content |
< 100 | ppm | IEC 62321 |
Color a Color a |
-2.04 到 0.960 | ME 12 | |
Color b Color b |
0.480 到 3.48 | ME 12 | |
Color L Color L |
ME 12 | ||
Mercury Content Mercury Content |
ppm | IEC 62321 | |
颜色 Color |
ME 12 | ||
补充信息 Supplementary information |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
Bromine Content Bromine Content |
ppm | IEC 62321 | |
铅含量 Lead content |
ppm | IEC 62321 | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
|||
邵氏 A,15 秒 Shore A, 15 seconds |
NBR 7456 | ||
拉伸强度 tensile strength |
MPa | ASTM D638 | |
拉伸应变 Tensile strain |
|||
屈服 yield |
% | ASTM D638 |
备注 |
---|
2 24 hr |
【新闻资讯】查看全部 ![]()
研发人员将使用过的食用油作为聚氨酯泡沫的原料
2022-05-26 波兰克拉科夫理工大学的一个小组开发了一种开孔聚氨酯泡沫,其中所有的多元醇成分都来自使用过的食用油。 由Krzysztof Polaczek领导的小组表示,虽然从植物油中提取的生物基多元醇比 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |
电邮一份说明书
PDF文档名:搜料网-Karina IVORY PVC COMPOUND 651D35/1-D-IS证书
发送至:(多个地址,中间以逗号隔开)
发送一份副本给我:您还没有填写邮箱!(点击完善资料)