公司信息及水印
牌号简介 About |
---|
PA 6,75%矿物质,注塑成型,热老化稳定,提高导热性 Durethan® BTC75H3.0EF 900117 (Dry) PA 6, 75% mineral, injection molding, heat-aging stabilized, improved heat conductivity Durethan® BTC75H3.0EF 900117 PA 6, 75% mineral, injection molding, heat-aging stabilized, improved heat conductivity Durethan® BTC75H3.0EF 900117 PA 6, 75% mineral, injection molding, heat-aging stabilized, improved heat conductivity |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
2.29 | g/cm³ | |
收缩率 Shrinkage rate |
|||
TD:120℃,2.0 mm TD:120℃,2.0 mm |
0.10 | % | |
TD:290℃,2.0 mm TD:290℃,2.0 mm |
0.70 | % | |
MD:120℃,2.0 mm MD:120℃,2.0 mm |
0.10 | % | |
MD:290℃,2.0 mm MD:290℃,2.0 mm |
0.60 | % | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
|||
23℃ 23℃ |
MPa | ||
拉伸强度 tensile strength |
|||
断裂,23℃ Fracture, 23 ℃ |
MPa | ||
拉伸应变 Tensile strain |
|||
断裂,23℃ Fracture, 23 ℃ |
% | ||
弯曲模量 Bending modulus |
|||
23℃ 23℃ |
MPa | ||
弯曲强度 bending strength |
|||
23℃ 23℃ |
MPa | ||
弯曲应变 Bending strain |
% | ||
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength |
|||
-30℃ -30℃ |
kJ/m² | ||
23℃ 23℃ |
kJ/m² | ||
简支梁无缺口冲击强度 Charpy Unnotch Impact strength |
|||
-30℃ -30℃ |
kJ/m² | ||
23℃ 23℃ |
kJ/m² | ||
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
|||
-30℃ -30℃ |
kJ/m² | ||
23℃ 23℃ |
kJ/m² | ||
悬臂梁无缺口冲击强度 Notched impact strength of cantilever beam |
|||
-30℃ -30℃ |
kJ/m² | ||
23℃ 23℃ |
kJ/m² | ||
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
0.45 MPa,未退火 0.45 MPa, unannealed |
℃ | ||
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ||
熔融温度 Melting temperature |
℃ | ||
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
MD:23~55℃ MD:23~55℃ |
1/℃ | ||
TD:23~55℃ TD:23~55℃ |
1/℃ | ||
导热系数 Thermal conductivity coefficient |
|||
-- -- |
W/m/K | ||
-- -- |
W/m/K | ||
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表面电阻率 Surface resistivity |
ohms | ||
体积电阻率 Volume resistivity |
|||
23℃ 23℃ |
ohms·cm | ||
相比漏电起痕指数 Compared to the leakage tracing index |
|||
解决方案 A Solution A |
V | ||
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
US FMVSS302 US FMVSS302 |
|||
灼热丝可燃性指数 Glowing wire flammability index |
|||
1.5 mm 1.5 mm |
℃ | ||
3.0 mm 3.0 mm |
℃ | ||
灼热丝起燃温度 Igniting temperature of the hot wire |
|||
1.5 mm 1.5 mm |
℃ | ||
3 mm 3 mm |
℃ | ||
补充信息 Supplementary information |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
ISO Shortname ISO Shortname |
备注 |
---|
2. 60x60x2mm, 4 hr |
3. 60x60x2mm, 80°C MT, 600 bar |
4. 2.0 mm/min |
5. 2 mm/min |
6. 10°C/min |
7. Through-plane |
8. with flow |
【新闻资讯】查看全部
埃万特在Medtec China2020展会展示医用聚合物解决方案
2020-09-14 搜料网资讯:2020年9月14日,埃万特公司,全球医疗保健行业中专业且可持续发展的材料解决方案和服务供应商,将于 Medtec China 2020展会期间展示聚合物配方,着色剂,功能性母粒和热塑 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |