公司信息及水印
牌号简介 About |
---|
灵活,迁移改进,无卤挤压等级,用于评估电线绝缘和电缆护套等应用。火焰性能满足UL VW1要求。80C最终使用温度额定值和良好的热变形性能,如UL 1581所定义。肖氏硬度为80。通常在标准挤压设备上进行的加工。使用0.12 mm x 20绞合铜导线在2.0 mm电线上进行的UL 1581试验。 Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements. 80C end use temperature rating and good heat deformation performance as defined by UL 1581. 80 Shore A hardness. Processing typically conducted on standard extrusion equipment. UL 1581 tests conducted on 2.0 mm wire with 0.12 mm x 20 stranded copper conductor. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.10 | g/cm³ | ASTM D792 |
熔体质量流动速率 Melt Flow Rate |
|||
250℃,5.0kg 250℃,5.0kg |
11 | g/10min | ASTM D1238 |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
脆化温度 Embrittlement temperature |
< -40.0 | ℃ | ASTM D746 |
UL温度额定值 UL temperature rating 8 |
80 | ℃ | UL 1581 |
Heat Deformation(100℃) Heat Deformation(100℃) 9 |
16 | % | UL 1581 |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
体积电阻率 Volume resistivity |
ohms·cm | IEC 60093 | |
介电强度 Dielectric strength |
|||
2 mm,在油中 2 mm in oil |
kV/mm | IEC 60243-1 | |
相对电容率 Relative permittivity |
|||
50 Hz 50 Hz |
|||
60 Hz 60 Hz |
|||
1 MHz 1 MHz |
|||
耗散因数 Dissipation factor |
|||
50 Hz 50 Hz |
|||
60 Hz 60 Hz |
|||
1 MHz 1 MHz |
|||
相比漏电起痕指数 Compared to the leakage tracing index |
V | IEC 60112 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
4.00 mm 4.00 mm |
UL 94 | ||
灼热丝可燃性指数 Glowing wire flammability index |
|||
3.0 mm 3.0 mm |
℃ | IEC 60695-2-12 | |
灼热丝起燃温度 Igniting temperature of the hot wire |
|||
3 mm 3 mm |
℃ | IEC 60695-2-13 | |
极限氧指数 Extreme oxygen index |
% | ISO 4589-2 | |
VW-1 VW-1 2 |
UL 1581 | ||
烟雾密度 Smoke density 10 |
|||
Flaming,Ds max:500.0 µm Flaming,Ds max:500.0 µm |
|||
Non-Flaming,Ds max:500.0 µm Non-Flaming,Ds max:500.0 µm |
|||
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
|||
邵氏 A,30 秒 Shore A, 30 seconds |
ASTM D2240 | ||
拉伸强度 tensile strength |
|||
断裂 fracture 2 |
MPa | UL 1581 | |
断裂 fracture 3 |
MPa | ASTM D638 | |
断裂,113℃ Fracture, 113 ℃ 4 |
MPa | UL 1581 | |
断裂 fracture |
MPa | ISO 527-2/50 | |
拉伸应变 Tensile strain |
|||
断裂 fracture 2 |
% | UL 1581 | |
断裂 fracture 5 |
% | ASTM D638 | |
断裂,113℃ Fracture, 113 ℃ 6 |
% | UL 1581 | |
断裂 fracture |
% | ISO 527-2/50 | |
弯曲模量 Bending modulus 7 |
|||
100 mm跨距 100 mm span |
MPa | ASTM D790 | |
-- -- |
MPa | ISO 178 |
备注 |
---|
2. 2.0 mm wire with 0.12 mm x 20 stranded copper |
3. 类型 1, 50 mm/min |
4. After 7 days. Tested on 2.0 mm wire with 0.12 mm x 20 stranded copper |
5. 类型 1, 5.0 mm/min |
6. 6 days, 2.0 mm wire with 0.12 mm x 20 stranded copper |
7. 13 mm/min |
8. 2.0mm wire with 0.12 mm x 20 stranded copper |
9. 250g, 2.0 mm wire with 0.12 mm x 20 stranded copper |
10. Plaque |
【新闻资讯】查看全部
通用汽车GE退出塑料工业协会!塑料备受争议,外部环境逐步好转
2019-11-08 汽车制造商通用汽车将不再是美国塑料工业协会(PLASTICS)的成员。 根据绿色和平组织11月5日的新闻稿,通用汽车曾向该组织表示已允许其成员资格失效,理由是该公司对塑料的看法有 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |