牌号简介 About |
---|
TECNOBOND PP-TLA是一种由顺丁烯二酸酐通过新的连续工艺改性的无规嵌段聚丙烯共聚物,接枝率高,游离顺丁烯二酸酐含量低。用途:TECNOBOND PP-TLA在共挤工艺、熔相热成型、铸造或吹塑薄膜或片材中特别推荐用作粘结层粘合剂。TECNOBOND PP-TLA在作为PP的非极性层和作为EvoH或PA的极性势垒材料之间的刚性包装中提供了优异的粘合性。在势垒中,在与EvoH或PA的TECNOBOND PP-TLA界面处形成共挤出共价键,而纠缠处于PP和TECNOBOND PP-TLA的熔融相。 Description: TECNOBOND PP-TLA is a random-block polypropylene copolymer modified by maleic anhydride through a new continuous process with high grafting efficiency which guarantees a very low content of free maleic anhydride. Applications: TECNOBOND PP-TLA is particularly recommended as tie-layer adhesive in the co-extrusion processes, meltphase thermoforming, cast or blowing film or sheet. TECNOBOND PP-TLA provides outstanding adhesion in the rigid packaging between non—polar layers as PP and polar barrier materials as EVOH or PA. In barrier co-extrusion covalent bonds are formed at TECNOBOND PP-TLA interface with EVOH or PA while entanglements are in melt phase of PP and TECNOBOND PP-TLA. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
熔体质量流动速率 Melt Flow Rate |
|||
190℃,2.16kg 190℃,2.16kg |
3.0 到 5.0 | g/10min | ASTM D1238 |
马来酸酐含量 Maleic anhydride content |
0.2 到 0.4 | wt% | 内部方法 |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
熔融温度 Melting temperature |
145 | ℃ | DSC |
备注 | |||
---|---|---|---|
暂无数据 |
【新闻资讯】查看全部
陕京四线张家口支线开建
2021-08-21 搜料网资讯: 8月10日,国家管网集团陕京四线张家口市支线项目开工建设。 该支线项目是张家口市气代煤工程的保障措施之一,对进一步提升张家口地区清洁用能水平、推进京津冀协同 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |