Noryl V02570是一种25%研磨纤维增强,注塑成型等级。该树脂具有良好的尺寸稳定性和低翘曲性,还使用了无氯化、无溴的FR添加剂,以达到1.0 mm时的V0 UL94额定值。Noryl V02570是一种很好的材料,适用于需要电绝缘性能、低翘曲和薄壁阻燃性的应用。 NORYL V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating at 1.0 mm. NORYL V02570 is may be an excellent material candidate for application requiring electrically insulating properties, low warpage and thin wall flame resistance. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.35 | g/cm³ | ASTM D792 |
熔体质量流动速率 Melt Flow Rate |
|||
300℃,5.0kg 300℃,5.0kg |
12 | g/10min | ASTM D1238 |
熔体体积流动速率 Melt Volume Rate |
|||
300℃,5 kg 300℃,5 kg |
8.00 | cm³/10min | ISO 1133 |
收缩率 Shrinkage rate |
|||
MD MD 3 |
0.30 到 0.50 | % | |
MD:3.2 mm MD:3.2 mm |
0.30 到 0.50 | % | |
吸水率 Water absorption rate |
|||
饱和,23℃ Saturation, 23 ℃ |
% | ||
平衡,23℃,50% RH Equilibrium, 23 ℃, 50% RH |
% | ||
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁无缺口冲击强度 Charpy Unnotch Impact strength 10 |
|||
-30℃ -30℃ |
kJ/m² | ||
23℃ 23℃ |
kJ/m² | ||
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
|||
-30℃ -30℃ |
J/m | ||
23℃ 23℃ |
J/m | ||
悬臂梁无缺口冲击强度 Notched impact strength of cantilever beam 11 |
|||
-30℃ -30℃ |
kJ/m² | ||
23℃ 23℃ |
kJ/m² | ||
装有测量仪表的落镖冲击 Dart impact equipped with measuring instruments |
|||
23℃,Total Energy 23℃,Total Energy |
J | ASTM D3763 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
0.45 MPa,未退火,100 mm跨距 0.45 MPa, unannealed, 100 mm span 12 |
℃ | ISO 75-2/Be | |
1.8 MPa,未退火,3.2 mm 1.8 MPa, unannealed, 3.2 mm |
℃ | ASTM D648 | |
1.8 MPa,未退火,100 mm跨距 1.8 MPa, unannealed, 100 mm span 12 |
℃ | ISO 75-2/Ae | |
维卡软化温度 Vicat Softening Temp |
|||
-- -- |
℃ | ASTM D1525 13 | |
B50 B50 |
℃ | ISO 306 | |
B120 B120 |
℃ | ISO 306/B120 | |
球压测试 Ball pressure test |
|||
123~127℃ 123~127℃ |
|||
155℃ 155℃ 14 |
|||
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
MD:-40~40℃ MD:-40~40℃ |
1/℃ | ASTM E831 | |
MD:23~80℃ MD:23~80℃ |
1/℃ | ISO 11359-2 | |
TD:-40~40℃ TD:-40~40℃ |
1/℃ | ASTM E831 | |
TD:23~80℃ TD:23~80℃ |
1/℃ | ISO 11359-2 | |
导热系数 Thermal conductivity coefficient |
W/m/K | ISO 8302 | |
相对温度指数 Relative temperature index |
℃ | UL 746 | |
电气性能 Electrical performance |
℃ | UL 746 | |
冲击机械性能 Impact mechanical performance |
℃ | UL 746 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表面电阻率 Surface resistivity |
ohms | IEC 60093 | |
体积电阻率 Volume resistivity |
ohms·cm | IEC 60093 | |
介电强度 Dielectric strength |
|||
0.8 mm,在油中 0.8 mm in oil |
kV/mm | ||
1.6 mm,在油中 1.6 mm in oil |
kV/mm | ||
3.2 mm,在油中 3.2 mm in oil |
kV/mm | ||
相对电容率 Relative permittivity |
|||
50 Hz 50 Hz |
|||
60 Hz 60 Hz |
|||
1 MHz 1 MHz |
|||
耗散因数 Dissipation factor |
|||
50 Hz 50 Hz |
|||
60 Hz 60 Hz |
|||
1 MHz 1 MHz |
|||
相比漏电起痕指数 Compared to the leakage tracing index |
V | IEC 60112 | |
高电弧燃烧指数(HAI) High Arc Burning Index (HAI) 15 |
UL 746 | ||
高压电弧抗点燃指数(HVAR)(PLC) High voltage arc ignition resistance index (HVAR) (PLC) |
UL 746 | ||
高电压电弧起痕速率 High voltage arc marking rate |
|||
HVTR HVTR |
UL 746 | ||
热丝引燃 Hot wire ignition |
|||
HWI HWI |
UL 746 | ||
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
1.00 mm 1.00 mm |
UL 94 | ||
灼热丝可燃性指数 Glowing wire flammability index |
|||
1.0 mm 1.0 mm |
℃ | IEC 60695-2-12 | |
灼热丝起燃温度 Igniting temperature of the hot wire |
|||
1 mm 1 mm |
℃ | ||
2 mm 2 mm |
℃ | ||
3 mm 3 mm |
℃ | ||
极限氧指数 Extreme oxygen index |
% | ISO 4589-2 | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
球压硬度 Ball hardness |
|||
H358/30 H358/30 |
MPa | ISO 2039-1 | |
拉伸模量 Tensile modulus |
|||
-- -- 4 |
MPa | ASTM D638 | |
-- -- |
MPa | ISO 527-1-2 | |
拉伸强度 tensile strength |
|||
屈服 yield 5 |
MPa | ASTM D638 | |
屈服 yield |
MPa | ISO 527-2/5 | |
断裂 fracture 5 |
MPa | ASTM D638 | |
断裂 fracture |
MPa | ISO 527-2/5 | |
拉伸应变 Tensile strain |
|||
屈服 yield 5 |
% | ASTM D638 | |
屈服 yield |
% | ISO 527-2/5 | |
断裂 fracture 5 |
% | ASTM D638 | |
断裂 fracture |
% | ISO 527-2/5 | |
弯曲模量 Bending modulus |
|||
50 mm跨距 50 mm span 6 |
MPa | ASTM D790 | |
-- -- 7 |
MPa | ISO 178 | |
弯曲强度 bending strength |
|||
-- -- 7 , 8 |
MPa | ISO 178 | |
-- -- 7 , 9 |
MPa | ISO 178 | |
屈服,50 mm跨度 Yield, 50 mm span 6 |
MPa | ASTM D790 |
备注 |
---|
3. Tensile Bar |
4. 5.0 mm/min |
5. 类型 1, 5.0 mm/min |
6. 1.3 mm/min |
7. 2.0 mm/min |
8. at Yield |
9. at Break |
10. 80*10*4 sp=62mm |
11. 80*10*4 mm |
12. 120*10*4 mm |
13. 速率 A (50°C/h), 载荷2 (50N) |
14. Approximate Maximum |
15. Surface |
【新闻资讯】查看全部
美国Aurora PVC AP3000 Series 中文物性表/价格走势
2019-07-12 美国Aurora PVC AP3000 一种用于挤出中等密度泡沫的硬质PVC粉末混合物。 产地:北美洲 完整 PDF物性表下载 及 查看价格走势 可点击 物性表下载 ;如果你 有采购需求或者技术服务需求( |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |