公司信息及水印
牌号简介 About |
---|
Keliren氯化聚乙烯(CPE)热塑性树脂广泛应用于PVC挤出和注塑应用中的冲击改性剂,尤其是在壁板、外窗型材和管道等产品中。低剂量的Kelliren树脂与硬质聚氯乙烯树脂可以显著提高抗冲击强度,并作为加工助剂。除了具有良好的耐化学性、优异的低温性能、较高的填料接受度和与多种配方成分的良好相容性等特性外,Kelliren树脂在适当配方的化合物中还具有优异的耐候性。用途:FR-ABS,柔性PVC,PE薄膜性能:加工流动性好,残余结晶少。 Keliren® Chlorinated Polyethylene(CPE) thermoplastic resins are widely used as impact modifiers in PVC extrusion and injection molding applications, especially in products such as siding, widow profiles and pipe. The low dosage levels of Keliren® resins with rigid PVC resins can significantly improve impact strength and also act as a processing aid. In addition to offering attributes such as good chemical resistance, excellent low temperature properties, high filler level acceptance and excellent compatibility with a broad range of formulation ingredients, Keliren® resins offer excellent resistance to weathering in a properly formulated compound. Application: FR-ABS, Flexible PVC, PE Film Performance: Excellent processing flowability and minimal residual crystal. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
含氯量 Chlorine content |
34.0 到 36.0 | wt% | ISO 7725 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
|||
邵氏 A Shaw's A |
< 57 | ISO 7619 | |
弹性体 elastic body |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength |
|||
断裂 fracture |
> 8.50 | MPa | ISO 37 |
拉伸应变 Tensile strain |
|||
断裂 fracture |
> 800 | % | ISO 37 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
【新闻资讯】查看全部
2000万吨陆地塑料危害超乎想象
2017-11-02 当前,塑料污染已经成为地球上直逼气候变化的另一重大威胁,因为它正在急剧而不可逆地污染每一种自然系统,并危及越来越多的生物。 长期以来,人们一直聚焦于陆地上土壤环境中的塑料污染,而对地球的另一组成部分――海洋中的塑料污染问题却很少关注。事实上,海洋塑料垃圾污染以及它们对于海洋生态环境造成的危害已经远远超出了我们的想象。 海洋塑料垃圾污染有多严重? 全球每年塑料废弃物超过3000万吨,其中有超过2000万吨的塑料垃圾被直接丢弃或从陆地通过河道、风 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |