AMODEL A- 1565 HS是65%玻纤和矿物纤维增强的聚邻苯二甲酰胺(PPA),主要针对要求高刚度、良好尺寸稳定性,以及在高温下也能保持良好刚度的高成本效益的产品。该牌号同时具有高变形温度和弯曲模量。 - 黑色:A-1565 HS BK 324 Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of stiffness at elevated temperatures. This grades also exhibits a high deflection temperature and flexural modulus. Black: A-1565 HS BK 324 |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.90 | g/cm³ | ISO 1183/A |
收缩率 Shrinkage rate |
|||
TD TD |
0.50 | % | ASTM D955 |
MD MD |
0.30 | % | ASTM D955 |
吸水率 Water absorption rate |
|||
24hr 24hr |
0.10 | % | ASTM D570 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
20700 | MPa | ASTM D638 |
拉伸模量 Tensile modulus |
ISO 527-2 | ||
23℃ 23℃ |
MPa | ISO 527-2 | |
100℃ 100℃ |
MPa | ISO 527-2 | |
150℃ 150℃ |
MPa | ISO 527-2 | |
175℃ 175℃ |
MPa | ISO 527-2 | |
拉伸强度 tensile strength |
MPa | ASTM D638 | |
拉伸强度 tensile strength |
ISO 527-2 | ||
断裂,23℃ Fracture, 23 ℃ |
MPa | ISO 527-2 | |
断裂,24℃ Fracture, 24 ℃ |
MPa | ISO 527-2 | |
断裂,150℃ Fracture, 150 ℃ |
MPa | ISO 527-2 | |
断裂,175℃ Fracture, 175 ℃ |
MPa | ISO 527-2 | |
拉伸应变 Tensile strain |
ISO 527-2 | ||
断裂 fracture |
% | ASTM D638 | |
断裂,23℃ Fracture, 23 ℃ |
% | ISO 527-2 | |
断裂,24℃ Fracture, 24 ℃ |
% | ISO 527-2 | |
断裂,150℃ Fracture, 150 ℃ |
% | ISO 527-2 | |
断裂,175℃ Fracture, 175 ℃ |
% | ISO 527-2 | |
弯曲模量 Bending modulus |
MPa | ASTM D790 | |
弯曲模量 Bending modulus |
ISO 178 | ||
23℃ 23℃ |
MPa | ISO 178 | |
100℃ 100℃ |
MPa | ISO 178 | |
150℃ 150℃ |
MPa | ISO 178 | |
175℃ 175℃ |
MPa | ISO 178 | |
弯曲强度 bending strength |
MPa | ASTM D790 | |
弯曲强度 bending strength |
ISO 178 | ||
23℃ 23℃ |
MPa | ISO 178 | |
100℃ 100℃ |
MPa | ISO 178 | |
150℃ 150℃ |
MPa | ISO 178 | |
175℃ 175℃ |
MPa | ISO 178 | |
压缩强度 compressive strength |
|||
13.0 mm 13.0 mm |
MPa | ASTM D695 | |
剪切强度 shear strength |
MPa | ASTM D732 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength |
|||
23℃ 23℃ |
kJ/m² | ISO 179/1eA | |
简支梁无缺口冲击强度 Charpy Unnotch Impact strength |
|||
23℃ 23℃ |
kJ/m² | ISO 179/1eU | |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
J/m | ASTM D256 | |
23℃ 23℃ |
kJ/m² | ISO 180-1A | |
悬臂梁缺口冲击强度 Impact strength of cantilever beam notch |
J/m | ASTM D256 | |
悬臂梁无缺口冲击强度 Notched impact strength of cantilever beam |
|||
23℃ 23℃ |
kJ/m² | ISO 180/1U | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 Hot deformation temperature |
|||
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ASTM D648 | |
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ISO 75-2/A | |
熔融峰值温度 Melting peak temperature |
℃ | ASTM D3418 | |
熔融温度 Melting temperature |
℃ | ISO 11357-3 | |
线性热膨胀系数 Linear coefficient of thermal expansion |
|||
TD TD |
ASTM E831 | ||
0 到 100℃ 0 to 100 ℃ |
cm/cm/℃ | ASTM E831 | |
100 到 200℃ 100 to 200 ℃ |
cm/cm/℃ | ASTM E831 | |
MD MD |
ASTM E831 | ||
0 到 100℃ 0 to 100 ℃ |
cm/cm/℃ | ASTM E831 | |
100 到 200℃ 100 to 200 ℃ |
cm/cm/℃ | ASTM E831 | |
电气性能 Electrical performance |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
体积电阻率 Volume resistivity |
ohms·cm | ASTM D257 | |
耐电弧性 Arc resistance |
sec | ASTM D495 | |
相比漏电起痕指数 Compared to the leakage tracing index |
V | UL 746 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
【新闻资讯】查看全部
美利肯赋予聚丙烯更美一面
2017-05-17 在今次展会,美利肯(Milliken)重点介绍其用于热成型和挤出聚丙烯应用的Millad NX 8000透明剂。使用Millad NX 8000增透后的聚丙烯能够实现卓越的透明度,从而替代在价格、功能性和环保等方面都略逊一筹的传统材料。 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |